Digital Textile Pretreatment Rheology: Why Standing Viscosity Does Not Predict Coating Uniformity

Standing viscosity is useful for routine digital textile pretreatment QC, but it does not predict...

Standing viscosity is useful for digital textile pretreatment QC, but a reference apparent-viscosity reading cannot predict coating uniformity by itself. A coating line imposes changing shear, pressure and deformation before the liquor wets a porous textile. Compare the actual flow response, application add-on, widthwise distribution and final print result. Test time-dependent recovery or elasticity where relevant; do not assume every pretreatment has the same structural-rebuilding mechanism.

Why Does Standing Viscosity Fail to Predict Coating Uniformity?

Because a coating line does not apply pretreatment under one static test condition.

The formulation experiences a sequence such as:

Storage → Pumping → Pipe / Filter Flow → Coating-Head Shear → Gap / Blade Deformation → Fabric Wetting → Penetration → Leveling → Structural Recovery → Drying

A standing viscosity measurement captures only one point in that sequence.

Two products can therefore show the same reference viscosity yet differ in how quickly viscosity drops under shear, how much elastic resistance they develop, how fast they recover after shear, how far they penetrate into fabric, how well the wet film levels and how uniformly coating weight remains across width.

Standing Viscosity Is a QC Parameter; Coating Uniformity Is a Rheology + Machine + Fabric Result.

What Is Standing Viscosity?

In mill practice, “standing viscosity” usually means a routine apparent-viscosity reading measured after the pretreatment has been prepared and allowed to hydrate or equilibrate.

A valid result requires a defined concentration, temperature, instrument, spindle or rotor, rotational speed, reading time and hydration or conditioning period.

This value is useful for batch-to-batch QC, concentration control and detecting gross viscosity drift.

But it does not describe the full stress history experienced in a coating head.

Viscosity vs. Rheology

Viscosity describes resistance to flow under a defined condition.

Rheology describes how a material responds to different shear rates, stress levels, time under shear, deformation and recovery.

Digital textile pretreatment is usually a polymeric, non-Newtonian fluid. That means apparent viscosity can change when the coating process changes.

For coating, rheology is therefore more informative than one viscosity number alone.

What Happens to Pretreatment During Coating?

At rest in the tank, the formulation may show relatively high structure. When pumped and forced beneath a coating blade, the local shear rate increases. After leaving the coating head, shear drops rapidly.

After the coating head, flow must allow sufficient leveling while limiting unwanted spreading or penetration until the layer is stabilised. Time-dependent structural rebuilding, where demonstrated, is one contribution; wetting, fabric structure and drying also matter.

This creates three different rheological needs:

At Rest → Stability

Under Coating Shear → Flow / Metering

After Coating → Controlled Recovery / Leveling

One standing viscosity cannot represent all three.

1. Shear Thinning

Many polymeric pretreatments become less viscous as shear rate increases.

This can be useful in coating because the formulation can remain structured before application, flow more easily beneath the blade and reduce excessive coating-head pressure.

But stronger shear thinning is not automatically better.

Research on blade coating of fabrics has shown that shear-thinning behavior can promote fluid penetration into the textile structure.

If the pretreatment loses too much structure under coating shear, it may penetrate more deeply before recovery occurs.

Therefore, evaluate Shear Thinning + Recovery + Fabric Penetration as one group.

2. Yield Stress / Structure at Rest

Some pretreatments behave as if a minimum stress is required before substantial flow begins.

A useful yield-like structure can help hold polymer near the fabric surface, reduce drainage and improve storage stability.

But excessive structure can create poor pumping, high coating-head pressure, ridges and uneven metering.

A formulation can therefore have a desirable standing viscosity but too much low-shear structure for a particular coating line.

3. Thixotropy and Structural Recovery

A thixotropic response includes a time-dependent decrease in apparent viscosity during sustained controlled shear, with rebuilding assessed after that shearing condition is reduced. It is different from a shear-rate-dependent viscosity change alone. Establish whether the actual formulation shows this response before using recovery speed to explain coating behaviour.

The recovery speed matters.

Recovery Too Slow: the wet film continues to flow, pretreatment penetrates further and local redistribution can occur.

Recovery Too Fast: blade marks may remain, leveling can be incomplete and ridges may be frozen into the wet film.

Where time-dependent rebuilding is demonstrated, its useful rate is process-specific. Compare the measured response with actual leveling and penetration; a higher recovery ratio is not a universal coating-performance score.

4. Viscoelasticity

Polymer solutions can store part of the deformation energy elastically rather than behaving as purely viscous liquids.

Textile-coating studies have shown that viscoelasticity can affect coating penetration and defect formation.

In blade coating, elastic response can resist penetration into yarns, create ribbing or bounce-back behavior and change the pressure response beneath the blade.

This explains why two formulations with similar shear viscosity can produce different coating depth.

5. Leveling After the Coating Head

Immediately after coating, the wet layer may contain blade lines, local thickness differences and surface disturbances.

The formulation must level enough to create a uniform surface.

Too little leveling can leave streaks, ridges and uneven digital-print color later. Too much leveling can create excess penetration, edge flow and loss of surface-localized polymer.

Leveling is controlled by more than standing viscosity. Surface tension, shear history, recovery and fabric absorbency all contribute.

6. Penetration into Fabric

Fabric coating is different from coating a nonporous film because the substrate itself can absorb liquid.

Penetration depends on shear rheology, elasticity, fabric pore structure, capillary pressure, surface tension and contact time.

Published fabric-coating research specifically found competing effects: shear thinning can promote penetration while elasticity can reduce it.

This is a strong example of why one standing-viscosity number does not predict coating behavior.

7. Wetting and Surface Tension

Even an ideal rheology cannot coat uniformly if the pretreatment does not wet the textile consistently.

Poor wetting can cause beading, local dewetting, patchy coating and uneven film continuity.

Excessive wetting can increase penetration and loss of surface localization.

Therefore, coating uniformity is a combined result of Rheology + Wetting + Fabric Structure + Coating Geometry.

Why Two Products with the Same Viscosity Coat Differently

Suppose two pretreatments both measure 2,500 mPa·s under the same routine QC method.

Product A may be strongly shear-thinning with slow recovery. Product B may be less shear-thinning but more elastic with faster recovery.

Under a blade, Product A may penetrate further and level more, while Product B may remain closer to the surface but show stronger ribbing sensitivity.

Both can pass the standing-viscosity specification.

This is why coating approval must include an actual application test.

Knife-over-Roll Coating

In knife-over-roll coating, the fabric is supported by a roll and passes beneath a blade.

Coating thickness depends on the gap between blade and substrate, blade geometry, fabric thickness, line speed and pretreatment rheology.

Technical references note that variations in substrate thickness can create nonuniform coating thickness even when the nominal machine gap is constant.

Therefore, a rheology trial should be performed on the actual production fabric, not only on a smooth laboratory film.

Knife-over-Air Coating

In knife-over-air systems, fabric is not supported by a roll directly beneath the blade.

Fabric tension therefore becomes part of the metering mechanism.

If tension changes, fabric deflection changes, effective coating pressure changes and add-on can change.

A formulation that coats uniformly at one tension may behave differently after speed or fabric-width changes.

Rheology should therefore be qualified together with web tension.

Roll / Metering Coating

Roll-coating systems can impose their own combinations of shear, pressure, film splitting and transfer.

The pretreatment must transfer from one surface to another and then wet the textile uniformly.

Standing viscosity can indicate batch consistency, but transfer efficiency, film splitting, roll-speed ratio and recovery also influence coating uniformity.

Line Speed Changes the Effective Rheology Requirement

Changing production speed changes shear rate, contact time, pressure history, time available for penetration and time available for leveling before drying.

This means a formulation that coats well at laboratory speed may not behave identically at full production speed.

When scaling up, test at realistic line speed whenever possible.

Do not approve the product only from a low-speed hand-coating result.

Coating Gap and Fabric Thickness

Machine gap and fabric thickness must be considered together.

If fabric thickness increases locally, effective gap decreases, pressure under the blade can increase and coating weight can change.

If the textile has edge-center thickness variation, the same pretreatment may show a widthwise coating profile.

Before blaming rheology, map fabric thickness, GSM and coating add-on across the width.

Fabric Tension and Deflection

Textile coating is mechanically coupled to the substrate.

Changes in tension can change fabric thickness, open area, blade contact and penetration.

Knits and stretch fabrics are especially sensitive.

A stable coating specification should therefore include fabric tension or another practical machine-control reference when tension materially affects application.

Temperature and Viscosity Drift

Polymer viscosity is temperature-sensitive.

If pretreatment is measured at one laboratory temperature but coated at a warmer production temperature, apparent viscosity can differ substantially.

This can change flow under the blade, penetration, leveling and coating weight.

Always record temperature with viscosity.

For production troubleshooting, compare the product at the actual process temperature where practical.

Holding Time and Shear History

A pretreatment can change during mixing, circulation, pumping and tank holding.

Time-dependent rheology can cause one sample to have the same initial standing viscosity but different coating behavior later in the run.

Evaluate fresh viscosity, held viscosity, multi-speed response and coating result after realistic circulation when production drift is reported.

pH, Electrolytes and Water Quality

Digital pretreatment can contain alkali, urea, salts, hard-water ions and other auxiliaries.

These can change polymer hydration and rheology.

A coating product tested in deionized water can behave differently in hard plant water, high-conductivity process water or a different alkali system.

Record pH, conductivity and water hardness when comparing unexplained viscosity or coating drift.

Filtration, Gel and Micro-Defects

Micro-gels or incompletely hydrated particles can create blade streaks, drag lines, local high spots and coating-head contamination.

A pretreatment can pass standing-viscosity QC while still containing unacceptable residue.

Use standardized filtration testing and inspect the retained material.

Coating uniformity requires both correct rheology and clean formulation.

Fabric Structure Changes the Coating Window

The same pretreatment can coat differently on dense woven cotton, open knit, high-GSM fabric, viscose and lyocell.

The reason is that the textile changes capillary suction, pore size, surface roughness, thickness and mechanical response.

Therefore, rheology should be matched to the fabric rather than approved generically.

Woven Fabrics

Stable woven fabrics often provide predictable support under knife-over-roll coating.

However, weave density and yarn structure still affect penetration.

A dense woven may require good leveling and controlled wetting, while an open woven may need more structure to prevent excessive strike-through.

Check both face and reverse sides during the coating trial.

Knitted Fabrics

Knitted fabrics can deform under tension and pressure.

This changes thickness, porosity and effective blade gap.

A rheology window that works on woven cotton may therefore not transfer to a stretch knit.

For knits, monitor fabric width, tension, coating add-on and penetration together.

Viscose / High-Absorbency Fabrics

Viscose and similar high-absorbency fabrics can pull liquid rapidly into the textile structure.

This can make low-structure coatings penetrate too deeply even when standing viscosity appears adequate.

Useful trials should compare surface coating weight, reverse-side show-through, dry add-on and post-wash K/S rather than relying on standing viscosity alone.

Lyocell

Lyocell should be qualified independently because its surface behavior, fibrillation control and finishing history can change liquid uptake.

A coating grade that works on viscose may require different structure, wetting or application add-on on lyocell.

Coating Weight vs. Standing Viscosity

Coating weight is the more direct application output.

Standing viscosity should be connected to:

Viscosity / Rheology → Coating Weight → Widthwise Uniformity → Penetration → Final Print Result

If standing viscosity changes but coating weight and print quality remain stable, the process may still be acceptable.

If standing viscosity is stable but coating weight drifts, investigate rheology under shear, machine gap, tension, temperature and fabric variation.

Widthwise Coating Uniformity

Use fixed cross-width positions such as Left → Left-Middle → Center → Right-Middle → Right.

At each position, measure what is practical: wet coating add-on, dry coating add-on, residual moisture, post-wash K/S and line-width or bleeding score.

Repeat at the beginning, middle and end of the roll.

This separates rheology problems from gap variation, blade contamination, fabric-thickness variation and time-dependent bath drift.

Drying and Chemical Migration

Coating does not end when the fabric leaves the blade.

During drying, water movement can redistribute polymer, alkali, urea and other soluble auxiliaries.

A low-structure film that continues penetrating before drying can produce a different final surface from a faster-recovering film.

Therefore, evaluate the fabric immediately after coating, after drying and after printing/fixation before deciding which rheology is better.

Effect on Ink Spreading and Edge Definition

Digital pretreatment coating prepares the textile surface that receives the inkjet droplet.

If coating is uneven, one zone can bleed more, fine lines can widen differently and color boundaries can lose definition.

A uniform surface polymer layer can help control migration, but excessive surface film can create other issues such as harsh hand or difficult wash-off.

The target is controlled, uniform add-on—not maximum coating thickness.

Effect on Color Yield

Surface-localized pretreatment can help maintain more dye near the visible face of the fabric.

This can increase apparent post-wash color if fixation remains effective.

But rheology can also change penetration.

A more shear-thinning coating may penetrate further under application stress, reducing surface polymer concentration. A more elastic coating may resist penetration but require better leveling control.

Measure face-side K/S, back-side show-through and post-wash color when comparing products.

Effect on Reactive Fixation

Reactive pretreatment coating carries more than polymer. It can also carry alkali, moisture-management chemistry and other auxiliaries.

Therefore, coating-weight variation also becomes fixation-chemistry variation.

A width zone with low coating add-on may receive less alkali. A zone with deeper penetration may distribute alkali differently through the fabric.

Always evaluate the final steamed and washed result.

Build a Better QC Test Method

A practical coating-pretreatment QC method should record sample concentration, water source, preparation/hydration time, temperature, viscometer, spindle/rotor, reference speed, reading time and appearance/gel observation.

The standing-viscosity method should remain simple enough for routine production.

More detailed rheology tests can then be used during product development, supplier matching and troubleshooting.

إنشاء ملف تعريف لزوجة متعدد السرعات

When two products have similar standing viscosity but different coating performance, measure apparent viscosity at multiple speeds.

Test Pointالغرض
Low rotational speedLow-shear structure / standing behavior
Reference speedRoutine QC comparison
Higher rotational speedShear sensitivity / thinning tendency

The exact speeds should match the instrument and product range.

Do not define one universal shear ratio for all digital pretreatments.

Use the profile to explain differences, not as a stand-alone winner score.

Add a Structural-Recovery Check

A simple development test can compare viscosity or rheological response:

Before High Shear → During / Immediately After High Shear → After Defined Recovery Time

This comparison can reveal a change during shear and a return, or lack of return, within the observation window. A persistent difference alone does not identify permanent polymer damage; check temperature, concentration, preparation, sample age and measurement conditions before further material investigation.

The result should be connected to leveling, penetration and coating streaks on actual fabric.

Record the Shear-and-Time Sequence Before Interpreting Recovery

Keep a clock-matched reference aliquot with the same preparation and holding conditions, but without the additional high-shear conditioning step, where practical. This helps separate that shear-history effect from changes during the same holding time.

  1. Fix the measurement conditions. Record sample age, preparation, concentration, water, temperature, geometry, container, fill and the valid measuring range. The same RPM on different geometries is not the same shear condition.
  2. Define the sequence before testing. Record the baseline setting and dwell, the higher-shear conditioning step and duration, and the return to the original setting. Retain the elapsed time of each later reading instead of writing only “recovered”.
  3. Retain controls on composition and temperature. Limit evaporation, entrained air and unintended dilution. A viscosity difference after vigorous mixing can include heating or a measurement artefact as well as a material response.
  4. State the observation limit. Report the response at the recorded times. Failure to return within that window is not proof of irreversible molecular degradation, and a speed sweep is not a measurement of elastic modulus or a universal coating-head shear rate.

Use the results to design a fabric-coating comparison, not as a standalone approval. Brookfield’s measurement guidance distinguishes shear-rate and time-dependent responses and explains why controlled instrument conditions matter. For a wetting or application uncertainty, compare the actual padding, coating or spray route before attributing the result to polymer recovery.

Build a Coating Rheology Matrix

CandidateStanding StructureShear ResponseالتعافيFabric Result
Current productمرجعمرجعمرجعالتحكم
Lower-structure candidateMeasureMeasureMeasurePenetration / leveling
Higher-structure candidateMeasureMeasureMeasureSurface hold / streaks
Alternate polymer routeMeasureMeasureMeasureFull print trial

For each candidate, record coating weight, widthwise uniformity, penetration, drying and post-wash print quality.

The best candidate is the one with the widest stable application window, not the highest standing viscosity.

الموافقة على التجربة الإنتاجية

Record fabric fiber/construction/GSM/thickness, pretreatment product/batch, concentration, standing-viscosity method, multi-speed profile where relevant, holding time, process temperature, coating geometry/gap, fabric tension, line speed, wet/dry coating add-on, widthwise add-on profile, drying conditions, residual moisture, ink/print mode, steaming/washing and post-wash K/S/definition/penetration.

Approve a rheology–coating–fabric working window rather than one standing-viscosity number.

Common Coating-Rheology Mistakes

1. Selecting a Product by Standing Viscosity Alone

Standing viscosity does not describe shear thinning, elasticity or recovery.

2. Assuming Higher Viscosity Means More Uniform Coating

Excess structure can produce ridges, poor leveling or high gap sensitivity.

3. Assuming Lower Viscosity Means Better Leveling

Low structure can increase penetration and surface-film loss.

4. Ignoring Fabric Thickness Variation

Knife-over-roll gap is affected by substrate thickness.

5. Ignoring Fabric Tension

Knife-over-air and stretch fabrics can be strongly tension-sensitive.

6. Measuring at the Wrong Temperature

Production viscosity can differ materially from room-temperature QC.

7. Ignoring Gel / Filtration

Micro-gels can create streaks even when average viscosity passes.

8. Judging Coating Before Printing

Final approval requires drying, digital printing, fixation and wash-off.

جدول استكشاف الأعطال وإصلاحها

المشكلة الملاحظةالمتغيرات الأولى التي يجب التحقق منهالا تفترض
Standing viscosity passes but coating streaksRecovery, viscoelasticity, blade condition, gapViscosity QC proves coating suitability
Coating penetrates too deeplyShear thinning, recovery, wetting, fabric absorbencyOnly standing viscosity is too low
Blade pressure becomes highHigh-shear viscosity, yield structure, temperatureMore dilution is automatically correct
Edge-center coating weight differsGap, fabric thickness, tension, widthwise rheology/temperatureThe polymer concentration is globally wrong
Good leveling but weak surface colorPenetration, recovery, coating add-onMore ink is the first solution
High surface color but harsh handSurface polymer add-on, wash-off, film concentrationHigher K/S means better overall performance
Production differs from labLine speed, shear history, temperature, full-width mechanicsLab standing viscosity transfers directly
Coating changes later in the runHolding, circulation shear, temperature, water lossThe fabric lot is the only cause

التكلفة الإجمالية أثناء الاستخدام

Coating-rheology optimization affects more than pretreatment price.

Cost per accepted m² = total non-overlapping in-scope coating-and-printing cost ÷ accepted finished-fabric area. Define the material, mixing, pumping, coating, drying, printing, fixation and additional quality or disposal expenses included. Count chemicals and fabric lost during rejects or rework once; compare equivalent fabric and finished-quality requirements.

A formulation with a slightly higher unit price can be economically better if it maintains coating weight more uniformly, reduces blade streaks, allows stable line speed, reduces rework and improves first-pass digital-print quality.

Compare cost per acceptable printed meter—not cost per kilogram or standing viscosity alone.

What Information Should You Send to a Supplier?

For useful coating-rheology matching, provide:

  • Ink system
  • Fabric fiber / construction / GSM / thickness
  • Current pretreatment product / TDS
  • التركيز
  • Standing viscosity and complete test method
  • Coating method: knife-over-roll, knife-over-air, roll or other
  • Gap / blade information
  • Fabric tension
  • Line speed
  • Wet / dry coating add-on
  • Widthwise uniformity
  • Water hardness / pH / conductivity where relevant
  • Drying conditions
  • Main issue: penetration, streaking, leveling, width variation, bleeding or weak color

يمكن لشركة FSX Chemical الاستفادة من هذه المعلومات من خلال العينات والمطابقة to compare actual coating behavior rather than matching one standing-viscosity number.

مراجعة Digital Textile Printing Pretreatment و تطبيقات الطباعة الرقمية for related process selection.

How Should a Mill Evaluate Digital Pretreatment Rheology for Coating?

Standardize Standing Viscosity → Add Multi-Speed / Recovery Testing When Needed → Coat Actual Fabric → Measure Add-On / Width Uniformity / Penetration → Dry → Print → Fix → Wash → Compare Final Performance

  1. Standing viscosity is useful for routine QC but cannot represent the full stress history of a coating process.
  2. Shear thinning, viscoelasticity and recovery determine how the pretreatment behaves under and after the coating head.
  3. Fabric coating is a porous-substrate problem, so penetration depends on rheology and fabric structure together.
  4. Knife gap, tension, line speed and temperature can change coating uniformity even when the product viscosity is unchanged.
  5. Coating add-on and final digital-print performance are more important than one standing-viscosity target.
  6. The best pretreatment is the formulation that maintains a stable coating window and delivers uniform post-wash color, definition and fixation at the lowest practical Total Cost in Use.

الأسئلة الشائعة

1. What is standing viscosity in digital textile pretreatment?

It is a routine apparent-viscosity reading measured under a defined test method after the formulation has been prepared and conditioned. It is useful for QC but does not describe complete coating rheology.

2. Why can two products with the same standing viscosity coat differently?

They can differ in shear thinning, elasticity, yield structure, thixotropic recovery, wetting and penetration.

3. Does higher standing viscosity give more uniform coating?

Not necessarily. Excess structure can cause poor leveling, ridges and strong gap sensitivity.

4. Does lower viscosity always improve leveling?

No. Lower structure can increase penetration and reduce surface localization even when the wet film looks smooth.

5. Why is shear thinning important in knife coating?

Shear thinning can allow easier flow under blade shear. Its effect on penetration depends on the complete flow response, wetting, fabric structure and how quickly flow becomes limited after application; it does not prove thixotropic recovery.

6. Why is viscoelasticity important?

Elastic response can resist fabric penetration and influence ribbing or bounce-back under rapid deformation at the coating head.

7. What is thixotropic recovery?

It is time-dependent rebuilding after a shearing condition is reduced in a formulation that exhibits thixotropy. Establish it using a controlled shear-and-time history, then assess its relation to leveling and penetration on the actual coating route.

8. Why does knife-over-roll coating depend on fabric thickness?

The effective gap is defined by blade position relative to the supported substrate, so local fabric-thickness variation can change coating thickness.

9. Why does production coating behave differently from the laboratory?

Production changes line speed, shear history, full-width gap, fabric tension, temperature and holding time.

10. Should I use a multi-speed viscosity test?

For routine QC, one standardized speed may be sufficient. Multi-speed testing becomes useful when products with similar reference viscosity show different coating behavior.

11. What is more important: standing viscosity or coating add-on?

Standing viscosity helps control the product, but coating add-on and its widthwise uniformity are more direct indicators of what actually reaches the fabric.

12. What should I send FSX Chemical for coating-rheology matching?

Send the fabric, current pretreatment/TDS, concentration, complete viscosity method, coating type, gap/tension/speed, add-on, drying conditions and the exact penetration, streaking or print-quality issue.

Match Coating Rheology to the Fabric and Coating Head

If two digital pretreatments show similar standing viscosity but produce different coating weights, penetration, streaks or print color, FSX Chemical can help compare the formulations by multi-speed response, recovery, filtration, fabric add-on and final printing performance.

ابدأ بـ العينات والمطابقة and provide your current fabric, viscosity method, coating equipment and production settings.

مراجعة Digital Textile Printing Pretreatment for the current FSX pretreatment routes📧 البريد الإلكتروني: Service@fsxchemical.com

Select a coating pretreatment whose measured flow response fits the coating head, actual fabric, wetting and drying conditions. Confirm uniform add-on, the intended penetration and the final print result over a stable operating window rather than choosing the highest or most familiar standing-viscosity value.

روابط سريعة

الاتصال السريع

أرسل طلبك

أو

عينات مجانية · الرد خلال 24 ساعة

الاستفسارات والدعم الفني بشأن المنتجات

أرسل متطلبات منتجك

يرجى إرسال اسم المنتج، والتطبيق، والكمية، والوجهة، وأي بيانات تقنية (TDS)، أو صورة عينة أو مستند متوفر لديكم بالفعل. وستقوم شركة FSX Chemical بمراجعة هذه المعلومات وتقديم توصية بشأن الخطوة التالية سواء كانت تقديم عرض أسعار، أو مطابقة العينة، أو اختيار المنتج.

معلومات عن المنتج اسم المنتج، الدرجة، الطراز، صورة الملصق أو مرجع المورد.
الوثائق المتاحة TDS، SDS، COA، صورة العينة، قائمة المنتجات أو بيانات الاختبار.
تفاصيل الطلب الكمية التقديرية، والتعبئة، وبلد المقصد، والميناء، أو الشروط التجارية.
الطلب أو المشكلة عملية طباعة المنسوجات، متطلبات التركيبة، المشكلات الحالية أو الأداء المستهدف.