FSX केमिकल मुख्यतः प्रतिक्रियाशील वस्त्र मुद्रण के लिए उच्च, मध्यम और निम्न विस्कोसिटी वाले सोडियम अल्गीनेट थिकनर प्रदान करता है। ग्रेडों को विस्कोसिटी, घुलनशीलता और प्रक्रिया संबंधी आवश्यकताओं के अनुसार अनुकूलित किया जा सकता है, जिससे स्थिर पेस्ट तैयारी, स्वच्छ मुद्रण प्रदर्शन और चयनित फॉर्मूलेशन उपयोग में सहायता मिलती है।.
Synthetic Thickeners · Application Overview
How Synthetic Thickeners Support Textile Printing
Acrylic-based liquid thickeners control printing-paste viscosity and flow. Select the grade for pigment, reactive or disperse printing, then assess performance with your fabric and formulation.
Viscosity Build
Develops paste body and allows viscosity adjustment during preparation.
Paste Flow
Controls paste rheology for transfer through flat-screen and rotary-screen equipment.
परिभाषा प्रिंट करें
Supports sharp outlines and controlled spreading in a matched printing formulation.
स्क्रीन चलना
Supports smooth paste transfer with reduced mesh-clogging tendency under suitable conditions.
Electrolyte Tolerance
YS-3169 offers strong electrolyte tolerance for reactive dye printing pastes.
Wash-Off & Handle
YS-3169 and YS-816 support desizing and soft handle under suitable process conditions.
Three Grades · Three Printing Systems
वर्णक मुद्रण
For pigment and binder pastes; stock-paste preparation or direct viscosity adjustment.
प्रतिक्रियाशील मुद्रण
For cotton and viscose; used as the main thickener or with sodium alginate.
विखुरित मुद्रण
For polyester with flat-screen and rotary-screen printing processes.
Application Guide · Printing Workflow
Synthetic Thickeners in the Printing Process
Follow the paste from preparation to the finished fabric. Mixing, fixation and washing requirements depend on the selected printing system.
-
01
Prepare the Paste
Stir the liquid thickener before use. Incorporate it under effective mixing, following the selected grade’s preparation sequence.
-
02
Adjust the Formulation
Mix the colorants and required auxiliaries. Adjust dosage to target paste viscosity and check uniformity before printing.
-
03
Screen Printing
Check paste transfer, screen running and pattern edges on the actual fabric at the intended machine speed.
-
04
Dry & Fix
Follow the binder’s curing conditions for pigment printing, or the dye system’s fixation conditions for reactive and disperse printing.
-
05
Wash Where Required
For reactive and disperse printing, follow the specified wash-off process. Conventional pigment printing generally does not require post-print washing.
-
06
Review the Finished Print
Check color yield, print definition and fabric handle after the required treatments. Record results for production approval.
Application Trials · Print Performance
Evaluate Synthetic Thickener Printing Performance
Compare paste behavior and finished fabric when evaluating synthetic thickeners for pigment, reactive or disperse printing. Record the formulation, working dosage and process conditions for each trial.
Six Checks for Your Printing Trial
Use your current thickener as the reference and compare the following results under matched conditions.
Paste Stability & Compatibility
Measure viscosity at consistent intervals. Check for separation, particles or viscosity changes after adding colorants and auxiliaries.
Screen Transfer & Flow
Observe paste transfer, screen release and mesh build-up during flat-screen or rotary-screen printing at the trial speed.
परिभाषा प्रिंट करें
Compare fine lines, sharp edges and solid areas. Check bleeding, uneven coverage and penetration on the selected fabric.
Color Yield & Uniformity
Compare shade depth and evenness at the same colorant level, fabric and fixation conditions, including any required washing.
After-Treatment & Handle
For reactive and disperse prints, assess wash-off and background clarity. For pigment prints, assess handle after binder curing.
Repeatability & Cost-in-Use
Repeat the trial to check consistency. Compare thickener cost at the dosage needed to achieve an acceptable print result.
Synthetic Thickeners · Paste Preparation
Preparing Synthetic Thickener Printing Paste
Preparation Checks from Product to Printing Paste
Bars indicate checklist order, not mixing time or performance scores.
-
उत्पाद
preparationConfirm the grade and batch. Stir the liquid thickener before weighing and use.
Step 01 / 06 -
Water &
auxiliariesPrepare the water and required auxiliaries in the order specified for the selected grade.
Step 02 / 06 -
Thickener
additionIncorporate the weighed thickener under effective mixing, following its TDS addition method.
Step 03 / 06 -
Mixing &
standingComplete the grade-specific mixing stage and any prescribed standing time before evaluation.
Step 04 / 06 -
संधानशीलता
adjustmentCheck the complete paste under consistent test conditions and evaluate any dosage adjustment.
Step 05 / 06 -
Final paste
checkReview uniformity, stability and screen behavior. Record the formulation and preparation conditions.
Step 06 / 06
Match the Preparation Method to the Grade
FSX synthetic thickeners are acrylic-based liquid grades for textile printing paste. Use the preparation method for the selected product; one mixing sequence does not cover every pigment, reactive and disperse formulation.
FSX 5112 · Pigment printing. For stock-paste preparation, add gradually to water under high-speed stirring. Direct viscosity adjustment is another TDS-listed route, with the addition level evaluated in the pigment and binder formulation.
FSX YS-3169 · Reactive printing. Follow the specified sequence for water and auxiliaries. Where sodium alginate is included, complete its prescribed mixing stage before adding YS-3169, then follow the TDS mixing and aging guidance.
FSX YS-816 · Disperse printing. Stir before use and follow its TDS for incorporation. Evaluate working dosage and paste viscosity for the intended flat-screen or rotary-screen polyester printing process.
Choose a Starting Synthetic Thickener for Your Printing Trial
Select your printing system to review the corresponding FSX grade. Confirm formulation compatibility and working dosage through sample trials. Reference dosages below are starting points; check the calculation basis against the current TDS.
FSX 5112
FSX Chemical Acrylic-Based Liquid Printing Thickener
FSX YS-3169
FSX Chemical Acrylic-Based Liquid Printing Thickener
FSX YS-816
FSX Chemical Acrylic-Based Liquid Printing Thickener
अपनी उत्पाद आवश्यकता भेजें
उत्पाद का नाम, उपयोग, मात्रा, गंतव्य और आपके पास पहले से मौजूद कोई भी टीडीएस, नमूना फोटो या दस्तावेज़ साझा करें। FSX केमिकल इस जानकारी की समीक्षा करेगा और कोटेशन, नमूना मिलान या उत्पाद चयन के लिए अगले कदम की सिफारिश करेगा।.