Cách đọc các tài liệu TDS, SDS và COA về chất làm đặc dùng trong in ấn dệt may
Technical Guide Supplier Document Review Updated July 2026 Direct Answer
A TDS explains the product’s technical characteristics, intended use and typical or reference specification. An SDS communicates hazard, handling, storage, exposure-control and emergency information. A COA reports the test results or conformity status for a specific production batch. Textile printing buyers should use the TDS to select a possible grade, the SDS to review safety and handling, and the batch COA to confirm that the supplied material meets the agreed quality requirements. None of these documents should be used as a substitute for sample testing and production validation.
Three Documents
Three Different Jobs
TDS, SDS and COA are related but not interchangeable. A TDS is not proof of an individual batch result. An SDS is not a product-performance specification. A COA does not explain the complete application or safety requirements. Buyers should read the three documents together and check that the product name, grade, manufacturer or issuer, test method and batch information remain consistent.
Quick Comparison
TDS vs SDS vs COA
This table explains what each document is designed to answer during supplier evaluation and bulk purchasing.
| Document | Main Purpose | Typical Information | Usually Batch-Specific? | Main Buyer Question |
|---|---|---|---|---|
| TDS | Product selection and technical reference | Product description, appearance, typical values, test methods, applications, preparation and storage guidance | Usually no | Does this grade appear suitable for my process? |
| SDS | Hazard communication and safe handling | Identification, hazards, composition, first aid, handling, storage, PPE, transport and emergency information | Usually no | How should this material be handled, stored and transported? |
| COA | Batch-quality verification | Product and grade, batch number, test items, specification limits, actual results, release date and authorization | Yes | Does this supplied batch meet the agreed specification? |
Document layouts vary between suppliers and markets. The function and traceability of the information are more important than decorative formatting.
Document Roles
What Each Document Can and Cannot Confirm
TDS
Bảng dữ liệu kỹ thuật
Used to understand the product grade, reference specification and intended application direction.
- Supports initial grade selection
- Explains reference test conditions
- May include typical rather than batch results
- Does not prove the quality of one shipment
SDS
Bảng dữ liệu an toàn
Used to communicate hazards, protective measures, safe handling and emergency information.
- Supports safety and compliance review
- Uses a structured 16-section format
- May be called MSDS in older communication
- Does not confirm printing performance
COA
Giấy chứng nhận phân tích
Used to connect a specific batch with applicable tests, specification limits and results.
- Should identify the batch
- Should identify the tested product or grade
- Should list relevant results or conformity
- Does not replace an application trial
Bảng dữ liệu kỹ thuật
How to Read a TDS
Begin by confirming the product identity and application scope before comparing any technical number.
| TDS Field | What to Verify | Tại sao điều này lại quan trọng |
|---|---|---|
| Product name and grade | Confirm the exact CMC, CMS, sodium alginate or digital paste model. | Similar product-family names may contain different grades and application routes. |
| Product description | Check whether it is powder, flake or liquid and whether it is a thickener, paste or pretreatment product. | Product form affects preparation, dosage and test method. |
| Intended application | Confirm reactive, disperse, pigment, screen, digital or industrial use. | A product proven in one process should not automatically be transferred to another. |
| Hình thức | Review the stated colour, form and visual condition. | Appearance may be a basic receiving and batch-check indicator. |
| Độ nhớt | Confirm concentration, temperature, instrument, spindle or rotor and RPM. | A viscosity number without its test method is incomplete. |
| pH | Confirm whether pH is measured as supplied or at a stated solution concentration. | Test basis and product form affect interpretation. |
| Moisture or solids | Confirm whether the value applies to powder, flake or liquid material. | Moisture affects delivered dry matter. A liquid nonvolatile-content result does not by itself identify active-polymer content; confirm the grade-specific basis before comparing dosage. |
| Preparation and dosage | Review mixing order, hydration time, dilution and application conditions. | Incorrect preparation may create misleading trial results. |
| Storage guidance | Check temperature, moisture protection, container closure and storage period. | Storage conditions can affect product stability and usability. |
| Revision date | Confirm that the TDS is the current applicable version. | Specifications, grades or test methods may change between versions. |
Typical value is not always a guaranteed batch limit.
A TDS may show a typical, reference or target value rather than the acceptance range applied to every production batch. Ask the supplier which values are guaranteed specifications and which are provided only as general technical guidance.
Bảng dữ liệu an toàn

How to Read an SDS
SDS information is primarily used for hazard communication, handling, storage, exposure control, first aid and emergency planning.
The current GHS-aligned format uses sixteen sections. OSHA requires the specified information for Sections 1–11 and 16, while the complete GHS-aligned layout also includes ecological, disposal, transport and regulatory sections.
| Section | Heading | Buyer Review Focus |
|---|---|---|
| 1 | Identification | Product identifier, recommended use, supplier or responsible party and emergency contact. |
| 2 | Hazard identification | Classification, signal word, hazard statements, pictograms and precautionary statements. |
| 3 | Composition / ingredients | Substance, mixture and applicable component or concentration information. |
| 4–6 | First aid, firefighting and accidental release | Immediate response measures for exposure, fire, spill or release. |
| 7 | Handling and storage | Safe handling precautions, storage conditions and incompatibilities. |
| 8 | Exposure controls / PPE | Exposure limits, ventilation, gloves, eye protection and other protective measures. |
| 9–10 | Properties, stability and reactivity | Relevant physical properties, stability, incompatibilities and hazardous decomposition. |
| 11 | Toxicological information | Routes of exposure, symptoms and available health-effect information. |
| 12–15 | Ecology, disposal, transport and regulations | Environmental, waste, shipping and applicable regulatory information. |
| 16 | Other information | Preparation date, revision date and other document information. |
SDS and MSDS usually refer to the same document family.
“MSDS” is the older term still used by some buyers and suppliers. “SDS” is the current GHS-aligned term. A change from MSDS to SDS does not turn the document into a product specification or batch COA.
Giấy chứng nhận phân tích
How to Read a Batch COA
The COA should connect the supplied material to a specific product, batch and set of applicable test results.
- Product name and exact grade
- Batch or lot number
- Manufacturing or release date where applicable
- Expiry or retest information where applicable
- Each applicable test item
- Specification or acceptance range
- Actual numerical result where available
- Test method or method reference
- Release or conformity status
- Authorized approval or signature
- Document issuer or responsible laboratory
- Revision or document-control information
The batch number is the traceability link.
The batch number on the COA should match the supplied packaging, invoice, packing list or other applicable shipment record. A COA with no clear batch connection provides limited evidence for the material actually delivered.
Specification vs Result
How TDS and COA Values Should Relate
| Test Item | TDS Reference or Specification | COA Batch Result | Buyer Check |
|---|---|---|---|
| Hình thức | White to off-white powder | Conforms | Confirm that the result uses an agreed visual criterion. |
| Độ nhớt | 45,000–55,000 mPa·s under a defined method | 50,200 mPa·s | Confirm that TDS and COA use the same concentration, temperature, spindle and RPM. |
| pH | 6.5–8.0 at a defined concentration | 7.2 | Confirm the solution concentration and test basis. |
| Độ ẩm | Maximum 10.0% | 7.4% | Confirm units and whether the limit applies to the supplied product form. |
The figures above are illustrative examples only and are not FSX Chemical product specifications.
For a detailed explanation of viscosity test conditions, review how to compare textile printing thickener viscosity test methods .
Product Identity
Match the Product Across All Documents
Match the exact product identity across the quotation, sample, TDS, SDS, COA and shipment records. A documented name change, such as DG-20 formerly DP-R, should be supported by the supplier’s grade cross-reference and applicable document revision. Retain the original issuer, batch and source document; do not edit an old COA merely to replace its model name.
Information That Should Match
- Product family
- Exact product or model code
- Product form
- Applicable use or grade
- Batch number where relevant
- Supplier or manufacturer relationship
Information That May Differ
- TDS revision date
- SDS revision date
- Document language
- Responsible party required by the destination market
- Batch-specific COA results
- Certification or laboratory issuer
Different issuer names do not automatically mean the document is invalid.
A brand, legal company, original manufacturer, testing laboratory, distributor or certification body may appear on different documents for different reasons. The important question is whether the issuer’s role, product scope and batch relationship are clear and verifiable.
Document Issuer
Why the Original Issuer Should Be Preserved
A technical or compliance document should continue to identify the entity responsible for issuing the information. Removing or replacing the original company, laboratory or certification-body name can make the document difficult to verify and may misrepresent who performed the testing or issued the certification.
Brand Presentation
The website, quotation or document cover may identify the international business brand used for customer communication.
Original Document Issuer
The original SDS, COA, test report or certificate should retain the responsible manufacturer, laboratory, certification body or other issuing entity shown on the source document.
Verify the role instead of forcing every document to use one name.
Buyers should be able to identify who supplies the product, who manufactures or tests it, who issued the document and which batch, product or certification scope the document covers.
Product-Specific Review
What to Check for Four FSX Product Routes
| Quy trình sản phẩm | Important TDS Fields | Important COA Fields | Main Review Risk |
|---|---|---|---|
| CMC | Viscosity method, concentration, DS, pH, moisture, purity and recommended application | Batch viscosity, pH, moisture and other agreed control items | Comparing grades only by viscosity while ignoring DS and purity |
| FSX CMS | Commercial synthetic-thickener family; exact grade, product form, printing route, viscosity, pH and preparation method | Batch appearance, viscosity, pH and applicable quality items | Treating reactive, disperse and specialty CMS as one universal product |
| Alginat natri | HV, MV or LV route, concentration, viscosity method, pH, moisture and reactive-printing use | Batch viscosity, pH, moisture, appearance and agreed indicators | Treating HV, MV and LV as quality rankings instead of grade routes |
| Hỗn hợp in kỹ thuật số | DG-20 (formerly DP-R) for reactive fabric pretreatment; DP-P for pigment fabric pretreatment; confirm the exact current disperse grade rather than infer a DP-D mapping. Check form, dosage, pH, application and fixation route | Batch appearance, pH, solids or other product-form-specific indicators | Comparing screen-printing and digital-pretreatment data directly |
For product-route selection, review the CMC, CMS, sodium alginate and digital printing paste comparison guide .
For process-based selection, review the reactive, disperse, pigment and digital printing thickener guide .
Common Document Problems

Eight Warning Signs Buyers Should Review
Missing product grade
A general family name may not identify which grade, viscosity route or application the document actually covers.
Viscosity without method
A value without concentration, temperature, instrument, spindle and RPM cannot be compared reliably.
COA without batch number
The document cannot be clearly connected to the supplied production batch.
TDS used as batch proof
A general specification sheet does not prove that one shipment was tested and released.
SDS used as performance proof
Safety and handling information does not confirm colour yield, viscosity stability, wash-off or application suitability.
Outdated revision
An older document may use a previous product description, specification, address or regulatory format.
Altered issuer details
Removing the original issuer may prevent verification of the laboratory, manufacturer or certification source.
Certificate without scope
A certificate should not be assumed to cover every product, factory, site or batch unless its stated scope confirms this.
Buyer Workflow
Six Steps for Reviewing Supplier Documents
STEP 01
Confirm the Product
Match the product family, grade, form and intended application with the quotation and requested sample. STEP 02
Review the TDS
Check technical parameters, test methods, application route, preparation instructions and revision date. STEP 03
Review the SDS
Check product identity, hazard classification, handling, storage, PPE, transport and emergency information. STEP 04
Test the Sample
Compare the candidate product using a defined laboratory method and the intended printing process. STEP 05
Review the Batch COA
Confirm the batch number, applicable specification, actual results and authorized release information. STEP 06
Match the Shipment
Confirm that packaging labels, batch numbers, COA and commercial documents refer to the supplied material.
FSX Chemical Support
Documents Available During Product Evaluation
Depending on the product, grade, project and document availability, FSX Chemical can provide or coordinate applicable technical and batch information for B2B evaluation.
- Applicable product TDS
- Applicable product SDS
- Sample or trial information
- Reference viscosity test conditions
- Batch COA for applicable commercial supply
- Packaging and batch-identification information
- Available certificates or records
- Grade-matching review
Document availability and issuer may vary.
The original issuing entity, product scope, batch information, revision date and validity shown on each document should be retained. Buyers should confirm document requirements before quotation or order approval.
Câu hỏi thường gặp dành cho người mua
Các câu hỏi thường gặp
What is the main difference between a TDS and COA?
A TDS normally describes the product grade, intended use and reference or typical specification. A COA relates to a specific batch and reports the applicable test results or conformity status for that batch. Is an SDS the same as an MSDS?
MSDS is the older term still used in some markets. SDS is the current GHS-aligned term and normally follows a structured sixteen-section format. Can an SDS prove that a textile thickener is high quality?
No. An SDS communicates safety, handling and hazard information. Product quality should be evaluated using the TDS, batch COA, sample testing and actual printing performance. Should every COA contain actual numerical results?
Numerical tests should normally show numerical results where applicable. Some visual or qualitative tests may be reported as conforming to an agreed requirement. The reporting format should still be clear and traceable to the batch. Can two suppliers’ TDS viscosity values be compared directly?
Only when the concentration, temperature, instrument, spindle or rotor, RPM, preparation method and units are consistent. Otherwise, the values may not be comparable. Why might the company name differ between documents?
Different documents may identify a brand, legal entity, original manufacturer, testing laboratory, distributor or certification body. The relationship and issuing role should be clear, and the original issuer should remain identifiable. Does a COA guarantee printing performance?
No. A COA confirms applicable batch-test results, but final printing performance also depends on fabric, dye or ink, recipe, equipment, fixation and production conditions.
About This Technical Guide
This guide is intended for textile printing mills, chemical distributors, importers and procurement teams reviewing technical, safety and batch documents before sample approval or bulk purchase.
FSX Hóa chất
Công ty TNHH Sợi Polymer Foshan Fushixin.
Updated July 2026
Technical References
Document and Hazard-Communication References
These sources provide general document-structure and batch-quality context. Buyers must also follow applicable destination-country requirements and the terms agreed for the specific product and order.
- U.S. Occupational Safety and Health Administration. Appendix D to 29 CFR 1910.1200 — Safety Data Sheets. View official OSHA guidance
- United Nations Economic Commission for Europe. Globally Harmonized System of Classification and Labelling of Chemicals. View current GHS publication page
- International Council for Harmonisation. ICH Q7 Good Manufacturing Practice Guide, Section 11.4, Certificates of Analysis. Used here as a reference framework for clear batch identification, test limits, results and issuing responsibility. View official guideline
Review the Product, Method and Batch Before Bulk Purchase
Send your current TDS, SDS, COA, product sample or document requirements together with the printing process and target specification. FSX Chemical can review an appropriate product and document route before controlled testing or commercial supply.
Yêu cầu mẫu đối chiếu View Documents📧 Email: Service@fsxchemical.com
Các bài viết liên quan
Cách so sánh các phương pháp thử nghiệm độ nhớt của chất làm đặc trong in vải
Chất làm đặc trong in vải theo loại thuốc nhuộm và quy trình in
Cách đánh giá nhà sản xuất chất làm đặc trong in ấn dệt may trước khi mua số lượng lớn
CMC so với CMS so với natri alginat so với bột in kỹ thuật số: Hướng dẫn lựa chọn thực tiễn
CMC trong in ấn dệt may: Hướng dẫn lựa chọn loại và mua sắm
So sánh giữa natri alginat và CMC trong in ấn dệt may: So sánh hiệu suất và chi phí
Cách đọc Bảng dữ liệu kỹ thuật (TDS) của natri alginat
Bán buôn natri alginat: Danh sách kiểm tra khi đặt hàng số lượng lớn dành cho người mua trong lĩnh vực in ấn dệt may
Nhà cung cấp hóa chất in vải: Những điều người mua cần kiểm tra trước khi hợp tác
Cách đánh giá nhà sản xuất alginat natri tại Trung Quốc: Bảng điểm dành cho người mua trong lĩnh vực in ấn dệt may
Nhà cung cấp hóa chất công nghiệp cho ngành in vải: Các tài liệu về chất lượng mà người mua cần kiểm tra
Alginat natri chuyên dụng cho in ấn dệt may: Xu hướng ứng dụng và Hướng dẫn lựa chọn loại sản phẩm
Liên kết nhanh
Gửi yêu cầu của bạn
Mẫu thử miễn phí · Trả lời trong vòng 24 giờ
Gửi yêu cầu về sản phẩm của bạn
Vui lòng cung cấp tên sản phẩm, ứng dụng, số lượng, điểm đến và bất kỳ tài liệu kỹ thuật (TDS), hình ảnh mẫu hoặc tài liệu nào mà quý khách đã có. FSX Chemical sẽ xem xét thông tin này và đề xuất bước tiếp theo liên quan đến báo giá, đối chiếu mẫu hoặc lựa chọn sản phẩm.