Chất làm đặc trong in vải theo loại thuốc nhuộm và quy trình in

Learn how to choose thickener and pretreatment routes for reactive, disperse, pigment and digital textile...

Technical Guide Printing Process & Thickener Selection Updated July 2026 Direct Answer

Choose a textile printing thickener or pretreatment route by identifying the fabric, colourant system, printing method and fixation process before comparing viscosity or price. Sodium alginate is commonly used as a benchmark for reactive screen printing on cellulosic fabrics. Disperse printing on polyester requires a route compatible with disperse dyes and heat fixation. Conventional pigment printing normally depends on a synthetic thickener and binder system. Digital textile printing requires a process-specific pretreatment selected for reactive, disperse or pigment inkjet printing.

Colourant System
vs Printing Method

Reactive, disperse and pigment describe different colourant and fixation systems. Digital describes the method used to place ink droplets on the textile. Digital textile printing can therefore use reactive ink, disperse ink or pigment ink. A “digital printing paste” must be selected according to the specific digital ink and fabric route rather than treated as one universal fourth dye system.

Selection Hierarchy

Six Questions to Answer Before Selecting a Thickener

Product selection should follow the production route. Starting with a viscosity number or product price can lead to an unsuitable comparison. QUESTION 01

What Is the Fabric?

Confirm cotton, viscose, lyocell, polyester, silk, wool or a blended fabric before selecting the colourant and paste route. QUESTION 02

Which Colourant?

Identify reactive dye, disperse dye, pigment ink or another dye class. Different colourants require different fixation chemistry. QUESTION 03

Screen or Digital?

Conventional screen paste and digital fabric pretreatment have different preparation, rheology and application requirements. QUESTION 04

How Is It Fixed?

Confirm steaming, thermofixation, sublimation or binder curing, together with the intended temperature and time. QUESTION 05

What Is the Main Problem?

Identify low colour yield, bleeding, poor sharpness, difficult wash-off, unstable paste or unacceptable fabric handle. QUESTION 06

How Will It Be Tested?

Define the laboratory method, application trial and acceptance criteria before comparing candidate products.

Quick Process Matrix

Printing Process and Starting Thickener Route

The table provides an initial selection framework. Final suitability must be confirmed using the intended recipe, fabric and machinery.

Lộ trình in ấnTypical FabricStarting Thickener or Paste RouteFixation / Post-TreatmentMain Evaluation Points
In lụa phản ứngCotton, viscose, lyocell and suitable cellulosic fabricsSodium alginate benchmark; selected reactive CMS route may be evaluatedSteaming followed by washing and removal of unfixed dye and thickenerColour yield, definition, penetration, wash-off and handle
Disperse screen printingPolyester and suitable polyester blendsProcess-specific disperse printing thickener, including selected CMS or synthetic routesHeat or steam fixation according to the dye and production routeDispersion, screen running, fixation, sharpness and residue
Pigment screen printingCotton, polyester and many blended or mixed-fibre fabricsSynthetic thickener combined with a compatible pigment binder and auxiliary systemDrying and binder curingRubbing fastness, colour strength, sharpness, curing and handle
In kỹ thuật số phản ứngCotton, viscose and lyocell; silk only with a validated silk-specific reactive processReactive digital fabric pretreatment such as DG-20 (formerly DP-R), subject to grade and process validationSteaming and wash-offInk bleeding, edge definition, colour development and wash-off
In kỹ thuật số phân tánPolyester and suitable polyester blendsProcess-specific direct-disperse fabric pretreatment where required; transfer-paper coating is a separate selectionHeat fixation or sublimationPenetration, sharpness, ink spreading, fixation and fastness
In kỹ thuật số bằng mực màuCotton, polyester and suitable blendsPigment digital fabric pretreatment such as DP-P, coordinated with the actual pigment ink and binder systemDrying and curingRubbing fastness, definition, colour strength and hand feel

Product names and internal model codes are not universal industry standards. Confirm the applicable TDS and trial procedure before use.

Reactive Screen Printing

Choosing a Thickener for Reactive Printing

Reactive dyes form chemical bonds with suitable fibres such as cotton and viscose during fixation. The thickener must control the printing paste without consuming a significant part of the reactive dye or preventing its transfer to the fibre.

Sodium alginate is widely used as the reference thickener for conventional reactive printing because its structure generally has limited reaction with reactive dyes and it can provide useful screenability, colour yield and wash-off performance when the complete process is controlled.[1] 01

Phương pháp sử dụng natri alginat

Mẫu chất làm đặc in vải từ natri alginat kèm dung dịch và đánh giá trên vải

Use sodium alginate as the initial benchmark when evaluating reactive screen printing on cotton, viscose or other suitable cellulosic fibres.

  • Compare HV, MV and LV under the same test method
  • Confirm stock-paste concentration
  • Evaluate screen release and edge definition
  • Review colour yield, wash-off and fabric handle

Review sodium alginate grades 02

Reactive CMS Route

FSX CMS printing-thickener route for disperse textile application evaluation

FSX CMS denotes a commercial synthetic printing-thickener family. Evaluate an exact grade or controlled blend only for its documented printing route; do not infer carboxymethyl-starch chemistry or a degree of substitution from the family name.

  • Confirm grade suitability for reactive printing
  • Compare colour yield and outline sharpness
  • Check background cleanliness and wash-off
  • Do not assume universal one-to-one replacement

Review CMS printing grades

CMC is not automatically a direct alginate replacement.

Selected CMC grades may be useful in specialty printing and other industrial systems, but conventional reactive printing suitability depends on degree of substitution, purity, dye interaction and the complete recipe. It must be proven through controlled trials.

Disperse Screen Printing

Choosing a Thickener for Polyester Disperse Printing

Disperse dyes are designed for hydrophobic fibres, particularly polyester. The printing paste must maintain a stable dye dispersion, transfer cleanly through the screen and release the dye during the selected heat-fixation process.

A reactive printing thickener should not be transferred directly to disperse printing simply because it gives a similar laboratory viscosity. The dye, auxiliary, acidity, heat treatment and residue requirements are different.

FS-05 CMS Route

FSX Chemical positions FS-05 as a starting CMS route for selected disperse screen-printing trials.

  • Confirm powder dispersion and hydration
  • Review screen running and paste stability
  • Evaluate definition after fixation
  • Check residue, washing and fabric handle

Synthetic Thickener Route

A process-specific synthetic thickener may also be used when the formulation requires low dosage, salt tolerance or a particular rheological profile.

  • Confirm compatibility with dispersing agents
  • Check the valid pH and electrolyte range
  • Evaluate heat stability
  • Review removal or residual-film behaviour

Direct printing and transfer printing are different routes.

Direct disperse printing places the colourant on the fabric before fixation. Sublimation transfer printing first prints transfer paper and then transfers the dye to polyester under heat. Their paste, coating and ink requirements should not be treated as identical.

Pigment Screen Printing

Why Pigment Printing Requires a Binder System

Pigments do not have the same fibre affinity or chemical fixation route as reactive and disperse dyes. In conventional pigment printing, the pigment is normally fixed to the fabric through a polymeric binder film.

The printing paste therefore commonly includes a pigment dispersion, synthetic thickener, binder and other auxiliaries. Research on textile pigment printing evaluates both colour properties and dry or wet rubbing fastness because binder formation and curing affect the final result.[2]

Thickener Responsibilities

  • Control screen-printing rheology
  • Limit unwanted spreading
  • Support even pigment distribution
  • Remain compatible with the binder and auxiliaries

Binder Responsibilities

  • Attach pigment particles to the fabric
  • Develop rubbing and washing resistance
  • Form correctly during curing
  • Balance fastness with fabric softness

Do not select pigment paste by viscosity alone.

Binder compatibility, curing temperature, curing time, pigment loading, rubbing fastness and fabric handle may be more important than matching one initial viscosity value.

In kỹ thuật số trên vải

Why Digital Printing Uses a Separate Pretreatment Decision

In conventional screen printing, the dye, thickener and most auxiliaries are combined in the colour paste before application. In textile inkjet printing, many functional chemicals are instead applied to the fabric through pretreatment, while the printer jets a low-viscosity ink through fine nozzles.[3]

The pretreatment helps control droplet spreading, penetration, edge definition, colour development and fixation. Select it for the ink chemistry and textile substrate. DG-20 is the current reactive pretreatment code formerly called DP-R. It is applied to the fabric; this does not qualify the product as an ink ingredient.

Digital fabric pretreatment route comparison for reactive, disperse and pigment textile printing

In kỹ thuật số phản ứng

DG-20 (formerly DP-R) is an FSX candidate for reactive inkjet fabric pretreatment on suitable cellulosic fabrics. Confirm the exact TDS, application method and complete-process trial; any silk use needs its own validated dye and fixation conditions.

  • Confirm fabric absorbency and preparation
  • Review thickener, alkali and humectant requirements
  • Evaluate bleeding, definition and colour development
  • Confirm steaming and wash-off conditions

Confirm the Exact Disperse Grade

In kỹ thuật số phân tán

For direct-disperse inkjet printing on polyester, confirm whether fabric pretreatment is required and select an exact grade for the ink, substrate and heat-fixation route. If a legacy record says DP-D, request the current grade identity and applicable TDS before specifying it. Do not transfer a fabric-pretreatment recipe to sublimation transfer paper or printer ink.

  • Confirm direct or transfer printing
  • Review coating or pretreatment dosage
  • Evaluate droplet spreading and penetration
  • Confirm heat fixation or sublimation

DP-P

In kỹ thuật số bằng mực màu

DP-P remains a pigment digital fabric-pretreatment candidate. Confirm the applicable grade documents, fabric, pigment ink, binder location and curing process through a complete trial; do not treat the route label as approval for every natural or synthetic fabric.

  • Confirm pigment ink and binder system
  • Evaluate surface ink control and edge sharpness
  • Review curing and rubbing fastness
  • Balance colour strength with fabric handle

TEST

Digital Trial Boundary

Evaluate fabric pretreatment with the actual ink, fabric, application method, dried or wet pretreatment state, print settings, drying and fixation process. Retain a previously qualified reference and assess final fabric quality; a successful coating trial does not establish printhead-ink compatibility.

  • Do not rely only on laboratory viscosity
  • Check filtration and coating uniformity
  • Confirm pretreatment-application equipment compatibility and monitor printing on the treated fabric; do not add ordinary pretreatment to printhead ink
  • Confirm production-side repeatability

Review digital printing paste routes

Fixation and Post-Treatment

Why Fixation Determines Product Selection

Tuyến đườngTypical Fixation DirectionPost-Treatment FocusSelection Risk
Reactive dyeSteaming or another validated reactive fixation processRemoval of unfixed dye, alkali, auxiliaries and thickenerPoor wash-off may reduce cleanliness and handle
Disperse dyeHeat fixation, high-temperature steaming or sublimation, depending on the routeRemoval of surface dye or residual paste where requiredIncorrect heat response may reduce colour or definition
Chất màuBinder drying and curingUsually no dye wash-off route equivalent to reactive printingUnder-curing can reduce fastness; over-curing may affect handle
Digital inkjetDepends on reactive, disperse or pigment ink chemistryMust follow the corresponding ink and fibre route“Digital” alone does not define the required fixation process

Performance Evaluation

What to Check During a Printing Trial

The same acceptance criteria should not be applied blindly to every process, but the following indicators provide a useful evaluation framework.

  • Paste preparation and hydration
  • Viscosity stability during use
  • Screen release or pretreatment uniformity
  • Edge definition and fine-line sharpness
  • Colour yield or colour strength
  • Ink or paste penetration
  • Mức độ sạch của nền
  • Bleeding or uncontrolled spreading
  • Fixation efficiency
  • Wash-off or residue removal
  • Dry and wet rubbing fastness
  • Tay cầm bằng vải hoàn thiện

Rheology affects print application and definition.

Thickeners are used to control paste movement and reduce unwanted dye migration. The useful rheological profile depends on the application method rather than one universally ideal viscosity. [5]

Common Selection Errors

Six Mistakes to Avoid

Choosing by viscosity alone

Similar viscosity values do not prove equivalent dye compatibility, rheology, wash-off, fixation or fabric handle.

Ignoring fabric composition

Cotton, viscose and polyester require different colourant and fixation routes. A product proven on one fibre may fail on another.

Mixing screen and digital logic

Screen-printing colour paste and digital pretreatment perform different functions and should not be compared only by dosage or viscosity.

Ignoring fixation

A thickener or pretreatment must remain compatible with steaming, heat fixation, sublimation or binder curing.

Comparing price per kilogram only

Dosage, dye or ink consumption, washing, rejected fabric and batch adjustment may change the real production cost.

Skipping the production trial

Laboratory testing is useful for screening, but final approval requires the buyer’s actual machinery, recipe and process.

Buyer Information

What to Send for Process-Based Grade Matching

  • Fabric composition and construction
  • Reactive, disperse or pigment colourant
  • Screen or digital printing method
  • Direct or transfer digital route
  • Current product name and specification
  • Current recipe and dosage
  • Target viscosity and test method
  • Steaming, heating or curing conditions
  • Current production problem
  • Required fastness and fabric handle
  • Monthly consumption
  • Required TDS, SDS and batch COA

For viscosity comparisons, review how to compare textile printing thickener viscosity test methods .

For a material-route comparison, review the CMC, CMS, sodium alginate and digital printing paste selection guide .

FSX Chemical Routes

Product Routes Available for Initial Evaluation

Dòng sản phẩmFSX RoutesInitial Application DirectionRequired Confirmation
Alginat natriHV / MV / LVReactive textile printingStock-paste concentration, print method, colour and wash-off
CMSCN-R / FS-05 / H5Reactive, disperse and selected specialty routesDye system, fabric, preparation, fixation and trial result
CMCHD / MD / LDSelected printing, specialty and industrial formulationsDS, viscosity method, purity and full recipe compatibility
Hỗn hợp in kỹ thuật sốDG-20 (formerly DP-R) / grade-confirmed disperse candidate / DP-PReactive, disperse and pigment inkjet printingInk, fabric, product form, dosage, printer and fixation route

Câu hỏi thường gặp dành cho người mua

Các câu hỏi thường gặp

Which thickener is normally considered first for reactive printing?

Sodium alginate is commonly used as the initial benchmark for conventional reactive printing on cotton, viscose and suitable cellulosic fabrics. Selected CMS alternatives may also be tested, but they require controlled recipe and printing trials. Can the same thickener be used for reactive and disperse printing?

It should not be assumed. Reactive and disperse dye systems use different fabrics, auxiliaries, fixation conditions and post-treatment. A grade must be validated for the intended printing process. Is sodium alginate the default thickener for pigment printing?

No. Conventional pigment printing normally relies on a compatible synthetic thickener and binder system. Pigment fixation, curing, rubbing fastness and fabric handle must be evaluated together. Is digital printing paste mixed directly into the printer ink?

Do not add an ordinary digital fabric pretreatment to printer ink. The printer requires a separately formulated and qualified ink. Any proposed ink ingredient needs independent formulation, filtration, stability and printhead-compatibility qualification; fabric-pretreatment trials do not provide that approval. Can one digital pretreatment be used for reactive, disperse and pigment inks?

It should not be assumed. Reactive, disperse and pigment inks have different fibre interactions, fixation processes and auxiliary requirements. Use a route developed and tested for the specific ink system. Is the lowest-priced thickener the lowest-cost option?

Not necessarily. Buyers should also consider dosage, colour yield, ink or dye consumption, washing, curing, rejected fabric, machine cleaning and batch consistency. What is required before approving a product for bulk supply?

Confirm the product grade, laboratory method, application trial, fixation route, final print result, batch specification, packing, documents and commercial conditions.

About This Technical Guide

This guide is intended for textile printing mills, dye and paste formulators, chemical distributors and procurement teams comparing process-specific thickener and digital fabric-pretreatment routes.

FSX Hóa chất
Công ty TNHH Sợi Polymer Foshan Fushixin.
Updated July 2026

Technical References

Supporting Process and Printing Research

These sources provide technical context. Commercial product selection must still be confirmed using the applicable TDS, batch information and customer production trial.

  1. Schneider, R. and Šostar-Turk, S. Research discussing sodium alginate and alternative thickeners in reactive dye printing. View research record
  2. Neral, B., Šostar-Turk, S. and Vončina, B. “Properties of UV-cured pigment prints on textile fabric.” The study evaluates a pigment printing paste containing synthetic thickener, binder and pigment dispersion. View research record
  3. “Recent developments in the preparatory processes for the digital printing of textiles.” Technical discussion of fabric pretreatment and digital textile printing workflow. View publication record
  4. Research on disperse dye inkjet printing of polyester and the relationship between ink formulation, spreading, printability and heat fixation. View research record
  5. “Rheological study of interactions between non-ionic surfactants and polysaccharide thickeners used in textile printing.” Technical discussion of rheology, shear behaviour and print definition. View research record

Start with the Printing Process, Not Only the Product Name

Send your fabric, dye or ink system, printing method, current product, viscosity method, fixation process and target result. FSX Chemical can review an initial sodium alginate, CMS, CMC or digital printing paste route for controlled sample evaluation.

Yêu cầu mẫu đối chiếu Yêu cầu báo giá📧 Email: Service@fsxchemical.com

Liên hệ nhanh

Gửi yêu cầu của bạn

hoặc

Mẫu thử miễn phí · Trả lời trong vòng 24 giờ

Thắc mắc về sản phẩm & Hỗ trợ

Gửi yêu cầu về sản phẩm của bạn

Vui lòng cung cấp tên sản phẩm, ứng dụng, số lượng, điểm đến và bất kỳ tài liệu kỹ thuật (TDS), hình ảnh mẫu hoặc tài liệu nào mà quý khách đã có. FSX Chemical sẽ xem xét thông tin này và đề xuất bước tiếp theo liên quan đến báo giá, đối chiếu mẫu hoặc lựa chọn sản phẩm.

Thông tin sản phẩm Tên sản phẩm, cấp loại, mẫu mã, ảnh nhãn mác hoặc mã tham chiếu của nhà cung cấp.
Các tài liệu có sẵn TDS, SDS, COA, ảnh mẫu, danh mục sản phẩm hoặc dữ liệu thử nghiệm.
Chi tiết đơn hàng Số lượng dự kiến, hình thức đóng gói, nước nhập khẩu, cảng hoặc điều kiện thương mại.
Yêu cầu hoặc Vấn đề Quy trình in trên vải, yêu cầu về công thức, vấn đề hiện tại hoặc chỉ tiêu hiệu suất.