Загустители для текстильной печати в зависимости от красителя и метода печати
Technical Guide Printing Process & Thickener Selection Updated July 2026 Direct Answer
Choose a textile printing thickener or pretreatment route by identifying the fabric, colourant system, printing method and fixation process before comparing viscosity or price. Sodium alginate is commonly used as a benchmark for reactive screen printing on cellulosic fabrics. Disperse printing on polyester requires a route compatible with disperse dyes and heat fixation. Conventional pigment printing normally depends on a synthetic thickener and binder system. Digital textile printing requires a process-specific pretreatment selected for reactive, disperse or pigment inkjet printing.
Colourant System
vs Printing Method
Reactive, disperse and pigment describe different colourant and fixation systems. Digital describes the method used to place ink droplets on the textile. Digital textile printing can therefore use reactive ink, disperse ink or pigment ink. A “digital printing paste” must be selected according to the specific digital ink and fabric route rather than treated as one universal fourth dye system.
Selection Hierarchy
Six Questions to Answer Before Selecting a Thickener
Product selection should follow the production route. Starting with a viscosity number or product price can lead to an unsuitable comparison. QUESTION 01
What Is the Fabric?
Confirm cotton, viscose, lyocell, polyester, silk, wool or a blended fabric before selecting the colourant and paste route. QUESTION 02
Which Colourant?
Identify reactive dye, disperse dye, pigment ink or another dye class. Different colourants require different fixation chemistry. QUESTION 03
Screen or Digital?
Conventional screen paste and digital fabric pretreatment have different preparation, rheology and application requirements. QUESTION 04
How Is It Fixed?
Confirm steaming, thermofixation, sublimation or binder curing, together with the intended temperature and time. QUESTION 05
What Is the Main Problem?
Identify low colour yield, bleeding, poor sharpness, difficult wash-off, unstable paste or unacceptable fabric handle. QUESTION 06
How Will It Be Tested?
Define the laboratory method, application trial and acceptance criteria before comparing candidate products.
Quick Process Matrix
Printing Process and Starting Thickener Route
The table provides an initial selection framework. Final suitability must be confirmed using the intended recipe, fabric and machinery.
| Технология печати | Typical Fabric | Starting Thickener or Paste Route | Fixation / Post-Treatment | Main Evaluation Points |
|---|---|---|---|---|
| Трафаретная печать активными красителями | Cotton, viscose, lyocell and suitable cellulosic fabrics | Sodium alginate benchmark; selected reactive CMS route may be evaluated | Steaming followed by washing and removal of unfixed dye and thickener | Colour yield, definition, penetration, wash-off and handle |
| Трафаретная печать методом распыления | Polyester and suitable polyester blends | Process-specific disperse printing thickener, including selected CMS or synthetic routes | Heat or steam fixation according to the dye and production route | Dispersion, screen running, fixation, sharpness and residue |
| Pigment screen printing | Cotton, polyester and many blended or mixed-fibre fabrics | Synthetic thickener combined with a compatible pigment binder and auxiliary system | Drying and binder curing | Rubbing fastness, colour strength, sharpness, curing and handle |
| Reactive digital printing | Cotton, viscose and lyocell; silk only with a validated silk-specific reactive process | Reactive digital fabric pretreatment such as DG-20 (formerly DP-R), subject to grade and process validation | Steaming and wash-off | Ink bleeding, edge definition, colour development and wash-off |
| Disperse digital printing | Polyester and suitable polyester blends | Process-specific direct-disperse fabric pretreatment where required; transfer-paper coating is a separate selection | Heat fixation or sublimation | Penetration, sharpness, ink spreading, fixation and fastness |
| Pigment digital printing | Cotton, polyester and suitable blends | Pigment digital fabric pretreatment such as DP-P, coordinated with the actual pigment ink and binder system | Drying and curing | Rubbing fastness, definition, colour strength and hand feel |
Product names and internal model codes are not universal industry standards. Confirm the applicable TDS and trial procedure before use.
Реактивная трафаретная печать
Choosing a Thickener for Reactive Printing
Reactive dyes form chemical bonds with suitable fibres such as cotton and viscose during fixation. The thickener must control the printing paste without consuming a significant part of the reactive dye or preventing its transfer to the fibre.
Sodium alginate is widely used as the reference thickener for conventional reactive printing because its structure generally has limited reaction with reactive dyes and it can provide useful screenability, colour yield and wash-off performance when the complete process is controlled.[1] 01
Вариант с альгинатом натрия

Use sodium alginate as the initial benchmark when evaluating reactive screen printing on cotton, viscose or other suitable cellulosic fibres.
- Compare HV, MV and LV under the same test method
- Confirm stock-paste concentration
- Evaluate screen release and edge definition
- Review colour yield, wash-off and fabric handle
Review sodium alginate grades 02
Reactive CMS Route

FSX CMS denotes a commercial synthetic printing-thickener family. Evaluate an exact grade or controlled blend only for its documented printing route; do not infer carboxymethyl-starch chemistry or a degree of substitution from the family name.
- Confirm grade suitability for reactive printing
- Compare colour yield and outline sharpness
- Check background cleanliness and wash-off
- Do not assume universal one-to-one replacement
CMC is not automatically a direct alginate replacement.
Selected CMC grades may be useful in specialty printing and other industrial systems, but conventional reactive printing suitability depends on degree of substitution, purity, dye interaction and the complete recipe. It must be proven through controlled trials.
Disperse Screen Printing
Choosing a Thickener for Polyester Disperse Printing
Disperse dyes are designed for hydrophobic fibres, particularly polyester. The printing paste must maintain a stable dye dispersion, transfer cleanly through the screen and release the dye during the selected heat-fixation process.
A reactive printing thickener should not be transferred directly to disperse printing simply because it gives a similar laboratory viscosity. The dye, auxiliary, acidity, heat treatment and residue requirements are different.
FS-05 CMS Route
FSX Chemical positions FS-05 as a starting CMS route for selected disperse screen-printing trials.
- Confirm powder dispersion and hydration
- Review screen running and paste stability
- Evaluate definition after fixation
- Check residue, washing and fabric handle
Synthetic Thickener Route
A process-specific synthetic thickener may also be used when the formulation requires low dosage, salt tolerance or a particular rheological profile.
- Confirm compatibility with dispersing agents
- Check the valid pH and electrolyte range
- Evaluate heat stability
- Review removal or residual-film behaviour
Direct printing and transfer printing are different routes.
Direct disperse printing places the colourant on the fabric before fixation. Sublimation transfer printing first prints transfer paper and then transfers the dye to polyester under heat. Their paste, coating and ink requirements should not be treated as identical.
Pigment Screen Printing
Why Pigment Printing Requires a Binder System
Pigments do not have the same fibre affinity or chemical fixation route as reactive and disperse dyes. In conventional pigment printing, the pigment is normally fixed to the fabric through a polymeric binder film.
The printing paste therefore commonly includes a pigment dispersion, synthetic thickener, binder and other auxiliaries. Research on textile pigment printing evaluates both colour properties and dry or wet rubbing fastness because binder formation and curing affect the final result.[2]
Thickener Responsibilities
- Control screen-printing rheology
- Limit unwanted spreading
- Support even pigment distribution
- Remain compatible with the binder and auxiliaries
Binder Responsibilities
- Attach pigment particles to the fabric
- Develop rubbing and washing resistance
- Form correctly during curing
- Balance fastness with fabric softness
Do not select pigment paste by viscosity alone.
Binder compatibility, curing temperature, curing time, pigment loading, rubbing fastness and fabric handle may be more important than matching one initial viscosity value.
Цифровая печать на текстиле
Why Digital Printing Uses a Separate Pretreatment Decision
In conventional screen printing, the dye, thickener and most auxiliaries are combined in the colour paste before application. In textile inkjet printing, many functional chemicals are instead applied to the fabric through pretreatment, while the printer jets a low-viscosity ink through fine nozzles.[3]
The pretreatment helps control droplet spreading, penetration, edge definition, colour development and fixation. Select it for the ink chemistry and textile substrate. DG-20 is the current reactive pretreatment code formerly called DP-R. It is applied to the fabric; this does not qualify the product as an ink ingredient.

Цифровая печать активными чернилами
DG-20 (formerly DP-R) is an FSX candidate for reactive inkjet fabric pretreatment on suitable cellulosic fabrics. Confirm the exact TDS, application method and complete-process trial; any silk use needs its own validated dye and fixation conditions.
- Confirm fabric absorbency and preparation
- Review thickener, alkali and humectant requirements
- Evaluate bleeding, definition and colour development
- Confirm steaming and wash-off conditions
Confirm the Exact Disperse Grade
Цифровая печать дисперсными чернилами
For direct-disperse inkjet printing on polyester, confirm whether fabric pretreatment is required and select an exact grade for the ink, substrate and heat-fixation route. If a legacy record says DP-D, request the current grade identity and applicable TDS before specifying it. Do not transfer a fabric-pretreatment recipe to sublimation transfer paper or printer ink.
- Confirm direct or transfer printing
- Review coating or pretreatment dosage
- Evaluate droplet spreading and penetration
- Confirm heat fixation or sublimation
DP-P
Цифровая печать пигментными чернилами
DP-P remains a pigment digital fabric-pretreatment candidate. Confirm the applicable grade documents, fabric, pigment ink, binder location and curing process through a complete trial; do not treat the route label as approval for every natural or synthetic fabric.
- Confirm pigment ink and binder system
- Evaluate surface ink control and edge sharpness
- Review curing and rubbing fastness
- Balance colour strength with fabric handle
TEST
Digital Trial Boundary
Evaluate fabric pretreatment with the actual ink, fabric, application method, dried or wet pretreatment state, print settings, drying and fixation process. Retain a previously qualified reference and assess final fabric quality; a successful coating trial does not establish printhead-ink compatibility.
- Do not rely only on laboratory viscosity
- Check filtration and coating uniformity
- Confirm pretreatment-application equipment compatibility and monitor printing on the treated fabric; do not add ordinary pretreatment to printhead ink
- Confirm production-side repeatability
Review digital printing paste routes
Fixation and Post-Treatment
Why Fixation Determines Product Selection
| Маршрут | Typical Fixation Direction | Post-Treatment Focus | Selection Risk |
|---|---|---|---|
| Реактивный краситель | Steaming or another validated reactive fixation process | Removal of unfixed dye, alkali, auxiliaries and thickener | Poor wash-off may reduce cleanliness and handle |
| Disperse dye | Heat fixation, high-temperature steaming or sublimation, depending on the route | Removal of surface dye or residual paste where required | Incorrect heat response may reduce colour or definition |
| Пигмент | Binder drying and curing | Usually no dye wash-off route equivalent to reactive printing | Under-curing can reduce fastness; over-curing may affect handle |
| Digital inkjet | Depends on reactive, disperse or pigment ink chemistry | Must follow the corresponding ink and fibre route | “Digital” alone does not define the required fixation process |
Performance Evaluation
What to Check During a Printing Trial
The same acceptance criteria should not be applied blindly to every process, but the following indicators provide a useful evaluation framework.
- Paste preparation and hydration
- Viscosity stability during use
- Screen release or pretreatment uniformity
- Edge definition and fine-line sharpness
- Colour yield or colour strength
- Ink or paste penetration
- Чистота фона
- Bleeding or uncontrolled spreading
- Fixation efficiency
- Wash-off or residue removal
- Dry and wet rubbing fastness
- Готовая тканевая ручка
Rheology affects print application and definition.
Thickeners are used to control paste movement and reduce unwanted dye migration. The useful rheological profile depends on the application method rather than one universally ideal viscosity. [5]
Common Selection Errors
Six Mistakes to Avoid
Choosing by viscosity alone
Similar viscosity values do not prove equivalent dye compatibility, rheology, wash-off, fixation or fabric handle.
Ignoring fabric composition
Cotton, viscose and polyester require different colourant and fixation routes. A product proven on one fibre may fail on another.
Mixing screen and digital logic
Screen-printing colour paste and digital pretreatment perform different functions and should not be compared only by dosage or viscosity.
Ignoring fixation
A thickener or pretreatment must remain compatible with steaming, heat fixation, sublimation or binder curing.
Comparing price per kilogram only
Dosage, dye or ink consumption, washing, rejected fabric and batch adjustment may change the real production cost.
Skipping the production trial
Laboratory testing is useful for screening, but final approval requires the buyer’s actual machinery, recipe and process.
Buyer Information
What to Send for Process-Based Grade Matching
- Состав и структура ткани
- Reactive, disperse or pigment colourant
- Screen or digital printing method
- Direct or transfer digital route
- Current product name and specification
- Current recipe and dosage
- Target viscosity and test method
- Steaming, heating or curing conditions
- Current production problem
- Required fastness and fabric handle
- Monthly consumption
- Required TDS, SDS and batch COA
For viscosity comparisons, review Как сравнить методы определения вязкости загустителей для текстильной печати .
For a material-route comparison, review the CMC, CMS, sodium alginate and digital printing paste selection guide .
FSX Chemical Routes

Product Routes Available for Initial Evaluation
| Семейство продуктов | FSX Routes | Initial Application Direction | Required Confirmation |
|---|---|---|---|
| Альгинат натрия | HV / MV / LV | Печать активными красителями на текстиле | Stock-paste concentration, print method, colour and wash-off |
| CMS | CN-R / FS-05 / H5 | Reactive, disperse and selected specialty routes | Dye system, fabric, preparation, fixation and trial result |
| CMC | HD / MD / LD | Selected printing, specialty and industrial formulations | DS, viscosity method, purity and full recipe compatibility |
| Паста для цифровой печати | DG-20 (formerly DP-R) / grade-confirmed disperse candidate / DP-P | Reactive, disperse and pigment inkjet printing | Ink, fabric, product form, dosage, printer and fixation route |
Часто задаваемые вопросы покупателей
Часто задаваемые вопросы
Which thickener is normally considered first for reactive printing?
Sodium alginate is commonly used as the initial benchmark for conventional reactive printing on cotton, viscose and suitable cellulosic fabrics. Selected CMS alternatives may also be tested, but they require controlled recipe and printing trials. Can the same thickener be used for reactive and disperse printing?
It should not be assumed. Reactive and disperse dye systems use different fabrics, auxiliaries, fixation conditions and post-treatment. A grade must be validated for the intended printing process. Is sodium alginate the default thickener for pigment printing?
No. Conventional pigment printing normally relies on a compatible synthetic thickener and binder system. Pigment fixation, curing, rubbing fastness and fabric handle must be evaluated together. Is digital printing paste mixed directly into the printer ink?
Do not add an ordinary digital fabric pretreatment to printer ink. The printer requires a separately formulated and qualified ink. Any proposed ink ingredient needs independent formulation, filtration, stability and printhead-compatibility qualification; fabric-pretreatment trials do not provide that approval. Can one digital pretreatment be used for reactive, disperse and pigment inks?
It should not be assumed. Reactive, disperse and pigment inks have different fibre interactions, fixation processes and auxiliary requirements. Use a route developed and tested for the specific ink system. Is the lowest-priced thickener the lowest-cost option?
Not necessarily. Buyers should also consider dosage, colour yield, ink or dye consumption, washing, curing, rejected fabric, machine cleaning and batch consistency. What is required before approving a product for bulk supply?
Confirm the product grade, laboratory method, application trial, fixation route, final print result, batch specification, packing, documents and commercial conditions.
Об этом техническом руководстве
This guide is intended for textile printing mills, dye and paste formulators, chemical distributors and procurement teams comparing process-specific thickener and digital fabric-pretreatment routes.
FSX Chemical
Компания «Фошань Фушисинь Полимер Файбер», ООО.
Обновлено в июле 2026 года
Техническая документация
Supporting Process and Printing Research
These sources provide technical context. Commercial product selection must still be confirmed using the applicable TDS, batch information and customer production trial.
- Schneider, R. and Šostar-Turk, S. Research discussing sodium alginate and alternative thickeners in reactive dye printing. View research record
- Neral, B., Šostar-Turk, S. and Vončina, B. “Properties of UV-cured pigment prints on textile fabric.” The study evaluates a pigment printing paste containing synthetic thickener, binder and pigment dispersion. View research record
- “Recent developments in the preparatory processes for the digital printing of textiles.” Technical discussion of fabric pretreatment and digital textile printing workflow. View publication record
- Research on disperse dye inkjet printing of polyester and the relationship between ink formulation, spreading, printability and heat fixation. View research record
- “Rheological study of interactions between non-ionic surfactants and polysaccharide thickeners used in textile printing.” Technical discussion of rheology, shear behaviour and print definition. View research record
Start with the Printing Process, Not Only the Product Name
Send your fabric, dye or ink system, printing method, current product, viscosity method, fixation process and target result. FSX Chemical can review an initial sodium alginate, CMS, CMC or digital printing paste route for controlled sample evaluation.
Запросить подбор продукта по образцу Запросить коммерческое предложение📧 Электронная почта: Service@fsxchemical.com
Связанные публикации
Как сравнить методы определения вязкости загустителей для текстильной печати
Как читать TDS, SDS и COA для загустителей, используемых в текстильной печати
CMC, CMS, альгинат натрия и паста для цифровой печати: практическое руководство по выбору
Альгинат натрия для печати активными красителями на текстиле: марки, вязкость и применение
CMC для текстильной печати: руководство по выбору марок и закупкам
Текстильная печатная паста на основе целлюлозы: оценка марки CMC и поставщиков
Альгинат натрия и CMC в текстильной печати: сравнение характеристик и стоимости
Альгинат натрия для реактивной цифровой печати на текстиле: предварительная обработка и выбор марки
Как приготовить печатную пасту на основе альгината натрия: растворение, концентрация и контроль качества
Альгинат натрия в текстильной печати: экологические аспекты и вопросы, связанные со сточными водами
Reactive Dye Fixation in Textile Printing: Sodium Alginate and Process Control
Sodium Alginate Mesh Size: Dissolution, Filtration and Textile Printing Performance
Быстрые ссылки
Отправьте запрос
Бесплатные образцы · Ответ в течение 24 часов
Отправьте свои требования к продукции
Сообщите название продукта, область применения, количество, пункт назначения, а также предоставьте техническое описание продукта (TDS), фотографию образца или имеющиеся у вас документы. Компания FSX Chemical рассмотрит эту информацию и порекомендует дальнейшие действия для подготовки коммерческого предложения, подбора образца или выбора продукта.