Synthetic Printing Thickeners Manufacturer
Acrylic-based liquid thickeners for pigment, reactive and disperse
textile printing, with grade selection, technical guidance and samples for your process.
Textile Printing · Liquid Thickeners
সিন্থেটিক প্রিন্টিং ঘনকারী
Acrylic-based liquid thickeners for viscosity and flow control in pigment, reactive and disperse textile printing.
পিগমেন্ট প্রিন্টিং
Efficient thickening and viscosity adjustment for pigment and binder printing pastes.
প্রতিক্রিয়াশীল মুদ্রণ
Electrolyte-tolerant thickener for reactive dye printing on cotton and viscose.
ডিসপার্স প্রিন্টিং
For disperse dye printing on polyester with flat-screen or rotary-screen equipment.
গ্রেড নির্বাচন ও মিল নির্ধারণ
Share your current TDS and printing conditions for grade comparison and sample matching.
Synthetic Thickeners · Paste Rheology
What Are Synthetic Thickeners for Textile Printing?
Acrylic polymers that build paste viscosity
Synthetic printing thickeners are polymer additives that build viscosity and control printing-paste flow. FSX liquid grades are high-solids, anionic acrylate polymer dispersions for textile printing.
Paste rheology and print definition
Rheology describes how printing paste flows and deforms during application. Suitable paste behavior supports screen transfer and sharp print outlines, so viscosity alone does not fully describe printing performance.
Compatibility with the complete formulation
Dyes, pigments, binders and electrolytes can influence thickening efficiency and paste stability. The selected grade needs to suit the complete formulation, including any sodium alginate used for co-thickening.
Paste Rheology · Viscosity Control
Product Comparison · Synthetic Thickeners
Compare Synthetic Printing Thickener Grades
Compare application, thickening performance and reference dosage across three FSX liquid grades.
Pigment Printing Thickener
Efficient viscosity build and controlled paste flow for sharp print outlines and smooth screen running.
- সিস্টেম
- রঞ্জক মুদ্রণ
- সূত্রায়ন
- Pigment / binder
- দৃষ্টি
- Cream white viscous liquid
- Ionic nature
- Anionic
- Solid content
- 70 ± 2.0%
- Reference dosage*
- Approx. 1.4%
For stock-paste preparation or direct viscosity adjustment.
টিডিএস অনুরোধ করুন →
প্রতিক্রিয়াশীল মুদ্রণ ঘনকারী
Rapid thickening and strong electrolyte tolerance help maintain paste viscosity in reactive dye formulations.
- সিস্টেম
- প্রতিক্রিয়াশীল মুদ্রণ
- কাপড়
- Cotton / viscose
- দৃষ্টি
- Cream white viscous liquid
- Ionic nature
- Anionic
- Solid content
- 70 ± 2.0%
- Reference dosage*
- Flat ≈ 4.0% Rotary ≈ 3.5%
Use as the principal thickener or with sodium alginate.
টিডিএস অনুরোধ করুন →
ডিসপার্স প্রিন্টিং থিকনার
Efficient thickening at relatively low dosage, with stable paste rheology for flat-screen and rotary-screen printing.
- সিস্টেম
- বিস্তৃত মুদ্রণ
- কাপড়
- পলিয়েস্টার
- দৃষ্টি
- Milky white viscous liquid
- Ionic nature
- Anionic
- Solid content
- 70 ± 2%
- Reference dosage*
- Flat 2.0–2.5% Rotary 1.5–2.0%
Adjust addition level to shade depth and target paste viscosity.
টিডিএস অনুরোধ করুন →
Match Your Current Thickener
Compare your current product with an FSX grade using paste requirements, working dosage and printing results.
- ইনপুট
- TDS / sample
- লক্ষ্য
- Trial grade selection
- Printing system
- Pigment / reactive / disperse
- প্রক্রিয়া
- Fabric and machine
- লক্ষ্য সান্দ্রতা
- Include test conditions
- বর্তমান মাত্রা
- Include calculation basis
Identify the paste behavior or print quality you want to improve.
Request Matching →*TDS starting references; Flat = flat-screen and Rotary = rotary-screen. Confirm the dosage calculation basis and optimize in your complete printing formulation before production.
টেক্সটাইল প্রিন্টিং প্রয়োগসমূহ
Explore Applications by Fabric & Printing System
Explore synthetic thickener applications in pigment printing, cotton and viscose reactive printing, and polyester disperse printing.
Pattern Definition & Screen Transfer
Fine outlines and solid coverage depend on how the paste passes through the screen and spreads on the fabric.
Color Yield & Shade Depth
Assess color strength and evenness in the finished print, alongside paste stability during the printing run.
Fabric Handle & Aftertreatment
Review softness after pigment-print curing, or wash-off and residual paste after reactive and disperse printing.
Explore your printing application ↗
Technical Data · Liquid Thickeners
Synthetic Printing Thickener Specifications
All three grades are anionic acrylate polymer dispersions. Compare solid content, pH conditions and reference dosage below.
pH conditions differ between grades. Dosages are starting references; confirm the calculation basis and adjust for your complete printing paste.
| গ্রেড | দৃষ্টি | pH / Conditions | Solid Content | Reference Dosage* | Dosage Adjustment | ক্রিয়া |
|---|---|---|---|---|---|---|
| FSX 5112 Pigment printing thickener |
Cream white viscous liquid
|
6.0–7.0
1% aqueous dispersion |
70 ± 2.0%
|
Approx. 1.4%
|
Adjust for binder level, pigment loading,
auxiliaries and target viscosity.
|
টিডিএস অনুরোধ করুন |
| FSX YS-3169 Reactive printing thickener |
Cream white viscous liquid
|
6.0–7.0
1% aqueous dispersion |
70 ± 2.0%
|
Flat screen: ≈ 4.0%
Rotary screen: ≈ 3.5% |
Adjust for shade depth, machine type,
fabric and target viscosity.
|
টিডিএস অনুরোধ করুন |
| FSX YS-816 Disperse printing thickener |
Milky white viscous liquid
|
6.0 ± 0.5
25°C; dilution not stated in TDS |
70 ± 2%
|
Flat screen: 2.0–2.5%
Rotary screen: 1.5–2.0% |
Adjust for shade depth, fabric construction,
machine type and target viscosity.
|
টিডিএস অনুরোধ করুন |
Viscosity Testing
Record paste formulation and dosage. Compare at the same temperature, instrument, spindle, speed and time after preparation.
Standard Packaging
All three TDS documents specify 150 kg/drum and 108 drums per 20-foot container. Confirm pallet and loading arrangements for shipment.
Storage & Handling
Store cool and well ventilated; stir before use. The 5112 TDS specifies 5–40°C. Protect YS-3169 and YS-816 from water ingress.
Need a technical specification comparison?
Send your current TDS, viscosity test method and working dosage for an FSX grade review.
Application Trials · Grade Evaluation
How to Evaluate a Synthetic Printing Thickener
Compare a suitable FSX grade with your current thickener through laboratory paste trials and a production printing run.
Record your current process
Document the fabric, printing system, paste recipe and current dosage. Keep a reference print for comparison.
Establish the trial dosage
Start from the grade’s TDS guidance and adjust to target paste viscosity. Record test conditions and all recipe changes.
Compare paste & print results
Check paste stability, screen transfer, print definition and color yield. Assess fabric handle after the required aftertreatment.
Validate production performance
Run a production trial to confirm repeatability. Compare thickener cost at the validated dosage alongside print quality.
কারখানা / ল্যাব / মান নিয়ন্ত্রণ প্রুফ
কারখানা, ল্যাব এবং মান নিয়ন্ত্রণ প্রুফ
Request current product-specific production, testing and quality documents, then review the supplied sample and packing requirements before purchasing.
নমুনা মিলানো ও ব্যাচ QC
কারখানা উৎপাদন
ল্যাব যাচাইকরণ
ব্যাচ QC ও COA
রপ্তানি প্যাকিং
Technical Questions · Samples & Supply
Synthetic Printing Thickener FAQs
Answers on formulation compatibility, thickener replacement, sample requests and supply arrangements.
Share your recipe, mixing sequence, dosage and viscosity test conditions, with photos of the printing defect.
- Viscosity Loss
- Pattern Bleeding
- Screen Clogging
- High Thickener Dosage
01 Can synthetic thickeners be used with sodium alginate?
YS-3169 can be used as the principal thickener or together with sodium alginate in reactive printing on cotton and viscose. The combination and addition levels should follow your paste requirements and trial results; this guidance does not automatically apply to every synthetic grade.
02 Why does paste viscosity change after adding dyes or auxiliaries?
Colorants, binders and electrolytes can change thickening efficiency and paste stability. Check water quality, ingredient levels and mixing sequence. YS-3169 offers strong electrolyte tolerance, but performance still depends on the complete reactive printing formulation.
03 Can I replace my current thickener at the same dosage?
A one-to-one replacement should not be assumed. Establish the dosage needed for suitable paste flow and print quality, then compare stability and cost at that dosage. Equal product weight or solid content alone does not establish equivalent performance.
04 Can I request synthetic thickener samples for testing?
Yes. Send your printing system, fabric, current thickener TDS and trial requirements through the sample-matching page. FSX can review the application and recommend a trial grade; confirm sample quantity and shipping arrangements before dispatch.
05 What information is needed for a quotation?
Provide the grade or printing application, order quantity, destination port or delivery address, trade terms and packing requirements. If the grade is undecided, include your current TDS and working dosage for an initial technical review.
06 What are the packing, MOQ and delivery arrangements?
The three product TDS documents specify standard packing of 150 kg per drum. MOQ, pallet arrangements and delivery time require confirmation for the selected grade, order quantity and destination; request these details with your quotation.
07 Which technical documents should I request?
Request the current TDS for product specifications and application guidance, and the SDS for handling and storage. Confirm batch COA availability and the reported test items against your agreed specifications.