The Role of Carboxymethyl Starch in Cost-Effective Textile Printing

Carboxymethyl starch can play an important role in cost-effective textile printing when viscosity efficiency, formulation...

Carboxymethyl starch can be cost-effective only when a confirmed grade meets the required print quality at a lower comparable cost per accepted finished fabric. Evaluate dosage, preparation, filtration, machine operation and post-treatment together. This article discusses the generic starch derivative; it does not establish the composition of a commercial FSX CMS product.

Carboxymethyl Starch, commonly abbreviated as CMS, is a modified starch derivative that can be evaluated as a thickening and rheology-control component in selected textile printing formulations. Depending on the application, it may be used as the main thickener or as one component of a compound thickener system.

However, the economic value of CMS should not be determined only by its price per kilogram. A lower-cost raw material can become expensive if it requires excessive dosage, produces difficult filtration, causes machine interruptions or increases rejected fabric.

A cost-effective CMS system is therefore one that achieves the required viscosity, rheology, printing performance and finished-fabric quality at an acceptable total manufacturing cost.

What Is Carboxymethyl Starch?

Carboxymethyl starch is a chemically modified starch in which carboxymethyl groups are introduced into the starch structure. The modification can improve the ability of the starch derivative to disperse or hydrate in water and allows manufacturers to produce grades with different viscosity and application characteristics.

Commercial CMS products are not identical. Their behavior can vary according to raw-material source, degree of substitution, molecular characteristics, purity, particle profile, moisture and production process.

CMS as a textile thickener

In textile processing, a suitable CMS grade may provide viscosity, suspension, water retention and film-forming behavior. These properties can make CMS useful in selected printing, compound thickener and sizing formulations.

CMS is a product family, not one universal material

Two CMS grades may have similar product names while showing different hydration, viscosity, electrolyte response, filtration and printing performance.

Buyers considering the FSX CMS commercial product route should confirm the exact offered grade and current documents. FSX CMS is a commercial synthetic printing-thickener family; its trade name and page address do not establish carboxymethyl-starch composition or a starch DS. This article’s starch-specific discussion applies only to a confirmed carboxymethyl starch material.

Why Cost-Effective Does Not Mean the Lowest Price

Purchasing departments often begin a thickener comparison with price per kilogram. This is understandable, but it does not show the actual cost of producing acceptable printed fabric.

Raw-material price

This is the purchase price of the CMS or competing thickener before considering dosage, freight, inventory and processing.

Effective dosage

A lower-priced product may require a higher addition level to achieve the same rheology and application performance.

Preparation cost

Mixing time, hydration time, temperature control, filtration and labor all contribute to the real cost of the printing paste.

Machine cost

Screen cleaning, filter replacement, pumping difficulty, slower production and unplanned stops can outweigh a small difference in raw-material price.

Quality cost

Poor edge definition, uneven solid areas, incorrect penetration or difficult post-treatment can create rework and rejected fabric.

Total cost in use

A CMS grade should therefore be considered economical only after it meets the same finished-fabric quality standard as the existing product.

How CMS Functions in Textile Printing

CMS can influence several parts of the printing process simultaneously. Understanding these functions helps formulators decide whether the material can contribute to cost optimization.

Viscosity development

CMS increases resistance to flow and can help establish the body required for controlled paste application.

Rheology control

The way a CMS-containing paste changes under shear influences pumping, screen passage, transfer and recovery after application.

Water retention

CMS can influence how water remains in the paste and moves between the formulation and the fabric.

Suspension

In suitable formulations, CMS can support the distribution of dyes, pigments or other dispersed components.

Film behavior

Starch derivatives can contribute to a film on the textile surface. This may be useful in some processes but excessive surface residue can affect handle or removal.

Compound-thickener formulation

CMS may be combined with other natural, modified or synthetic polymers to adjust viscosity efficiency, rheology, stability and cost.

1. Viscosity Efficiency and Dosage Optimization

One of the first economic questions is how much product is required to reach a useful operating range.

Do not compare dosage from viscosity alone

A candidate that reaches the same single-point viscosity at a lower concentration may appear more economical, but the printing result must still be equivalent.

Compare at equal concentration first

An initial equal-concentration comparison can screen product behavior only after the basis is stated. Equal as-supplied mass compares the purchased products; it does not necessarily compare equal dry material or equal polymer. Use a common-SOP challenge to assess handling within the present process. For application qualification, prepare each confirmed grade by its documented procedure and verify readiness before measurement.

Optimize after baseline testing

Once the candidate is technically acceptable, dosage can be adjusted in controlled steps to determine the lowest practical level that still meets production requirements.

Record the complete viscosity method

  • CMS concentration and basis: as supplied, defined dry residue or assayed polymer; stock solution versus complete paste
  • জলের উৎস
  • মিশ্রণ ও হাইড্রেশন প্রক্রিয়া
  • পরিমাপের তাপমাত্রা
  • ভিসকোমিটার মডেল
  • Spindle or rotor
  • ঘূর্ণন গতি
  • Reading time and unit

Cost calculations based on unrelated viscosity methods can lead to an incorrect commercial conclusion.

2. Rheology and Print-Paste Transfer

Cost-effective printing requires a paste that performs efficiently on the machine, not simply one that appears thick in a laboratory container.

Flow during pumping

Excessive resistance can increase pumping difficulty and reduce stable circulation.

Flow through the screen

The paste should move through the screen openings under production shear without requiring excessive pressure.

Transfer onto the fabric

A highly structured paste may show good standing viscosity but transfer incompletely, producing weak or uneven printed areas.

Recovery after application

After shear decreases, the paste should recover enough structure to control spreading and penetration.

Multi-speed testing

Comparing apparent viscosity at several rotational speeds characterizes rate response within that instrument setup. It does not establish timed recovery or guarantee screen behavior. If recovery is part of the target, define a prior-shear stage, a fixed subsequent setting and elapsed observation times. Brookfield’s RSX manual, section 2.5.8, illustrates a time-resolved recovery test; it is not evidence that every CMS grade is thixotropic or that its example settings suit textile paste.

3. CMS in Disperse Textile Printing

CMS can be evaluated in selected disperse printing systems, particularly when the formulator requires starch-derived viscosity and rheology properties.

Polyester fabric

Disperse dyes are widely associated with polyester printing. The thickener should be tested with the actual polyester construction, printing machine and fixation route.

Paste transfer

CMS should provide sufficient body while allowing the color paste to pass through the screen and transfer uniformly.

Fixation behavior

Evaluate the CMS formulation through the full thermal fixation or other approved process rather than judging only the wet print.

Surface quality

Final assessment should include print definition, solid-area uniformity, migration where relevant and residual surface feel.

Application-specific approval

CMS should not be described as the universal thickener for every disperse dye system. Dye chemistry, machine conditions and formulation design remain important.

4. CMS in Compound Thickener Systems

One of the most useful approaches to cost optimization is not replacing one thickener completely but developing a controlled compound system.

Why use a blend?

Different polymers can contribute different properties. One component may provide economical viscosity, while another improves shear response, filtration, stability or final fabric performance.

CMS with other modified polysaccharides

CMS may be evaluated together with সিএমসি or another compatible polymer when the formulation requires a different balance of viscosity, film behavior and water retention.

CMS with synthetic rheology modifiers

A hybrid natural-modified and synthetic system may allow the formulator to adjust shear response without relying on one polymer alone.

Do not blend by price alone

Increasing the percentage of the lowest-cost component can change filtration, recovery, chemical tolerance and wash-off.

Use controlled formulation experiments

Change the declared polymer ratio in a planned matrix, specifying whether the ratio uses as-supplied mass, defined dry residue or assayed polymer. Rebalance carrier water and final batch mass consistently, and record any resulting changes in salts, pH or other ingredients. Use independent preparations and confirm relevant combinations before attributing an improvement to one component; a mixture comparison may include interactions.

5. CMS and Fabric Considerations

The same CMS formulation may behave differently on fabrics with different fibre chemistry, construction and absorbency.

পলিয়েস্টার

Polyester is an important substrate when CMS is evaluated for selected disperse printing systems. Surface preparation and thermal history can influence paste transfer.

Blended fabrics

A polyester blend may show different absorption and surface properties from a 100% polyester fabric.

Lightweight fabrics

Lightweight materials may show excessive penetration or residual surface stiffness more easily.

Dense fabrics

Dense constructions may require stronger transfer and leveling to produce uniform color.

Fabric preparation

Oils, softeners, finishing agents or inconsistent pretreatment can create defects that should not automatically be blamed on CMS.

6. Hydration and Paste Preparation

Preparation efficiency directly affects both performance and manufacturing cost.

Prepare the water phase

Use a controlled water source and confirm that the mixing vessel is clean.

Establish circulation

Start appropriate liquid movement before introducing powdered CMS.

Add the powder gradually

Excessively rapid addition can create lumps that require additional mixing or filtration.

Standardize mixing conditions

Record batch size, mixer type, impeller, rotational speed, powder-addition time and total mixing duration.

Allow the required hydration time

Follow the confirmed powder grade’s documented dispersion, temperature and hydration procedure. Define a readiness endpoint using repeatable viscosity observations together with checks for undissolved material and filtration, rather than appearance or a universal waiting time alone. A fixed-time preparation is a separate handling challenge, not proof of the fully prepared grade’s application limit.

Avoid unnecessary processing

Longer mixing is not automatically better. Excessive processing can add labor, energy, foam and temperature variation without improving the paste.

7. Chemical Compatibility

CMS cost calculations are meaningful only when the product remains stable in the complete printing formulation.

Dyes

Test representative colorants, including production shades with relatively high chemical loading.

ইলেক্ট্রোলাইটসমূহ

Salts and other ionic components may influence the apparent viscosity and polymer interactions.

পিএইচ

Different printing processes operate under different pH conditions. Measure viscosity and physical stability after the final pH is established.

Binders and crosslinkers

If CMS is evaluated in a pigment or coating-related formulation, compatibility with binder chemistry must be confirmed.

অন্যান্য পলিমার

Compound systems should be checked for gel formation, separation, viscosity drift and filtration after all polymers are combined.

8. Filtration and Machine Reliability

A small raw-material saving can disappear quickly when the paste requires frequent filtration or causes machine interruptions.

Use a defined filtration method

Record the filter material, opening size, sample quantity and filtration conditions.

Test the hydrated CMS first

This helps identify incomplete hydration, coarse material or contamination before other chemicals are introduced.

Test the complete paste

Additional residue may develop after dyes, salts or other formulation components are added.

Inspect the residue

Inspect the retained material and compare the polymer stock, completed paste and suitable controls. Treat incomplete dispersion, gel, precipitation, fibres and contamination as hypotheses until follow-up checks support the assignment; residue amount or appearance alone is not a chemical identification.

Record production cleaning

Screen cleaning, filter changes and line flushing should be included in the commercial comparison.

9. Holding and Storage Stability

Printing paste may remain in preparation tanks or circulation systems for hours before it is completely consumed.

Monitor viscosity over time

Test immediately after preparation, after complete hydration and after the normal production holding period.

Check physical condition

  • বিচ্ছেদ
  • Settling
  • Gel development
  • Skin formation
  • Foam retention
  • Filtration change

Prevent evaporation during comparison

Open containers can lose water, increasing solids and apparent viscosity.

Evaluate stored paste on fabric

Evaluate held paste against both the agreed specification and finished-fabric criteria. A shift beyond a release limit requires investigation even if a small print appears acceptable; it may signal a changing process window. Compare fresh and held paste at the same temperature and measurement conditions.

10. Print Definition and Color Uniformity

Cost reduction is not successful when it produces wider print edges, broken details or uneven solid colors.

Use a controlled test design

  • Fine lines
  • Small text
  • Sharp corners
  • Dots
  • Closely spaced design elements
  • Large solid areas

Evaluate edge control

Check whether color remains within the intended pattern after printing and fixation.

Evaluate penetration

Inspect the face and reverse side of the fabric according to the required end use.

Evaluate large solid areas

Poor leveling or incomplete paste transfer may become more obvious in large dark areas than in small laboratory patterns.

Compare after post-treatment

Final color and definition should be evaluated after the complete thermal, washing or finishing process.

11. Fixation, Removal and Fabric Handle

The economic effect of a thickener continues after the printing machine.

স্থিরীকরণ

The CMS formulation should be tested using the normal process temperature, time and equipment.

Removal

Where the process requires the thickener to be removed, assess how easily the residual CMS system is washed or otherwise removed from the textile.

ফ্যাব্রিক হ্যান্ডেল

Excessive polymer deposition can make a textile feel stiff or coated. This is particularly important on lightweight fabrics.

Additional washing cost

A lower-cost thickener that requires extra washing, higher water use or reprocessing may not provide a lower total cost.

12. Batch Consistency and Production Control

Cost optimization must remain stable from shipment to shipment. Frequent recipe adjustment increases laboratory and production cost.

Useful batch checks may include

  • Commercial grade identity
  • দৃষ্টি
  • Moisture where relevant
  • pH under the defined method
  • Viscosity under the defined method
  • জলসঞ্চার
  • ছাঁকন
  • Representative application performance

একটি অপারেটিং পরিসর ব্যবহার করুন

Commercial specifications should control meaningful variation rather than assuming every production batch will produce one identical number.

Connect documents with the commercial grade

The sample, quotation, TDS, purchase order, package label and batch COA should refer to the same product code.

The supplier’s general production and QC capability should also form part of the sourcing decision. Buyers can review the FSX Chemical Manufacturing & Quality information when evaluating a long-term supply route.

CMS vs Sodium Alginate

CMS and sodium alginate are both polysaccharide-derived materials, but they should not be treated as automatic substitutes.

সোডিয়াম অ্যালজিনেট

সোডিয়াম অ্যালজিনেট is a common starting thickener for conventional reactive dye printing on suitable cellulosic textiles.

সিএমএস

CMS may be considered in selected disperse printing, compound-thickener and other application-specific formulations.

Cost comparison

A valid economic comparison should consider the required dosage, formulation changes, filtration, printing performance, fixation, post-treatment and rejected-fabric risk.

Raw-material price alone does not establish that one is economically superior to the other.

CMS vs CMC

CMS and CMC are both chemically modified polysaccharides, but their base polymers and application behavior differ.

সিএমসি

CMC is derived from cellulose and may be evaluated in selected printing, coating, sizing and compound formulations.

সিএমএস

CMS is starch-based and may offer different hydration, film and viscosity characteristics.

Do not compare only viscosity grades

Two products with the same nominal viscosity can differ in dosage, rheology, chemical tolerance and final textile behavior.

Compound formulations

In some applications, using CMS and CMC together may be more useful than forcing one polymer to provide all required properties.

CMS vs Synthetic Thickeners

Synthetic textile thickeners can provide strong rheology control at relatively low addition levels in selected processes, while CMS offers a modified starch-based route with different preparation and film characteristics.

Compare preparation

Some synthetic systems require controlled pH activation or neutralization, while CMS preparation focuses more on powder dispersion, hydration and formulation compatibility.

Compare chemical tolerance

Electrolytes, binders and pH can affect synthetic and CMS-based systems differently.

Compare final handle

The amount and type of polymer remaining on the fabric can influence softness and surface feel.

Compare total formula cost

Evaluate the entire formulation rather than the thickener ingredient in isolation.

How to Calculate the Real Cost in Use

The most useful commercial comparison is the total cost required to produce an acceptable quantity of finished printed fabric.

Cost AreaWhat to IncludeWhy It Matters
Thickener materialDelivered price and optimized dosageShows actual thickener cost per batch
Other formulation chemicalsAdditional polymers, stabilizers, auxiliaries and defoamersA cheaper CMS may require a more complex formula
প্রস্তুতিLabor, mixing, hydration, energy and filtrationLong preparation increases operating cost
Machine operationSpeed, cleaning, filter changes and downtimeMachine efficiency can outweigh raw-material savings
WasteFilter residue, tank residue and unused pasteUnused material increases effective dosage
Post-treatmentFixation, washing, water, energy and processing timeDifferent polymers may change downstream requirements
QualityReprinting, rejected fabric and customer claimsQuality failure usually has a much higher cost than the thickener
SupplyFreight, inventory, MOQ and batch variationStable supply reduces hidden production risk

Calculate cost per accepted m² = total in-scope monetary run cost ÷ accepted finished area, using the same currency, accounting boundary, fabric, shade, coverage and quality criteria. Record consumption on the price’s as-supplied basis; if an assay-based comparison is added, state and align the assay and reporting bases rather than substituting nonvolatile residue for active polymer. Count delivered freight, consumed material, wasted paste and rework only once in the ledger. Report accepted yield beside unit cost; a run with zero accepted output cannot demonstrate a finite unit-cost saving.

Step 1: Select the current reference

Use a representative sample of the thickener currently approved for production.

Step 2: Record the existing cost structure

Record price, dosage, preparation time, filtration, machine performance and relevant post-treatment cost.

Step 3: Align the test method

Define two comparisons. First, a common-SOP challenge uses the same declared water, concentration basis, equipment and preparation deadline to assess fit within the existing process. Second, prepare each confirmed grade by its documented procedure to the agreed endpoint for application qualification. Condition to the same final measurement temperature, use comparable measuring settings and record any preparation differences. Do not rank a partly hydrated sample as the fully prepared grade.

Step 4: Compare basic paste properties

  • জলসঞ্চার
  • সান্দ্রতা
  • রিওলজি
  • পিএইচ
  • ছাঁকন
  • ফেনা
  • স্থিতিশীলতা বজায় রাখা

Step 5: Prepare the complete printing paste

Use the actual dyes and auxiliaries rather than comparing only CMS in water.

Step 6: Complete a fabric trial

Test definition, transfer, penetration and solid-area uniformity using representative production fabric.

Step 7: Complete fixation and post-treatment

Evaluate final color, surface condition, handle and required durability.

Step 8: Optimize dosage

Reduce or adjust the CMS level only after the candidate has demonstrated acceptable baseline performance.

Step 9: Conduct a production trial

Monitor paste and fabric from the beginning to the end of a representative run.

Step 10: Calculate cost per acceptable production unit

Compare the candidate with the current system only after both meet the same quality requirements.

How to Optimize a CMS-Based Compound Thickener

Compound thickener development can create a better cost-performance balance than replacing one polymer completely.

Define the role of each polymer

Identify which component provides base viscosity, shear response, structural recovery, suspension, water retention or film properties.

Create a controlled formulation matrix

Test several defined CMS-to-secondary-polymer ratios instead of changing the recipe randomly.

Keep total solids visible

Record each product’s as-supplied dose, carrier contribution and any defined dry-residue result. A lower dose of one polymer may be offset by other material in the formula, but total nonvolatile residue is not automatically active thickener content. Keep the recipe mass balance and analytical basis visible when comparing blends.

Evaluate chemical compatibility

Polymer blends can behave differently after dyes, salts, binders or pH adjustment are introduced.

Evaluate the complete process

Select the blend that provides the required machine behavior and finished fabric at the best practical total cost.

Common Cost-Optimization Mistakes

Choosing the lowest quotation

Price per kilogram does not include dosage, preparation, machine or quality cost.

Comparing only viscosity

Similar viscosity does not prove similar rheology, filtration or printing performance.

Reducing dosage too quickly

An aggressive reduction may create unstable transfer or lower print quality before the optimum level is identified.

Using CMS as a universal replacement

A formula developed for sodium alginate or synthetic thickener may require redesign rather than simple weight-for-weight replacement.

Ignoring post-treatment cost

Additional washing or difficult removal can eliminate the original material saving.

Ignoring production consistency

A low-cost product requiring frequent batch correction increases hidden laboratory and machine costs.

Changing several variables together

Changing CMS grade, dosage, auxiliaries and machine settings at the same time makes it difficult to identify the reason for a result.

Troubleshooting CMS Printing Problems

পর্যবেক্ষিত সমস্যাসম্ভাব্য কারণসমূহসুপারিশকৃত পরীক্ষাগুলি
CMS forms lumpsFast powder addition, weak circulation, unsuitable water or incomplete dispersionReview addition rate, mixing pattern, temperature and hydration
Viscosity is below targetIncorrect dosage, incomplete hydration, high temperature or chemical interactionCheck weighing, hydration, temperature and complete formula
Viscosity is too highExcess dosage, evaporation, low temperature or unsuitable gradeReview solids, container closure, temperature and grade selection
Excessive filter residuePoor hydration, gel formation, chemical precipitation or contaminationInspect residue and test CMS and final paste separately
Poor screen transferExcessive viscosity, unsuitable rheology or filtration problemsReview multi-speed behavior, solids and screen conditions
Printed edges spreadWeak structural recovery, excessive pickup or high fabric absorbencyReview rheology, dosage, fabric and application settings
Solid areas are unevenPoor leveling, excessive paste structure, foam or incomplete transferReview flow, foam, screen pressure and formulation
Paste changes during storageContinued hydration, evaporation, pH change or polymer interactionMonitor viscosity, temperature, pH and holding conditions
Fabric feels too stiffExcess CMS, excessive pickup, surface film or insufficient removalReview dosage, application quantity and post-treatment
Cost is lower but rejection rate risesFormula optimized for raw-material price rather than final qualityRecalculate cost using acceptable finished fabric as the basis

Information to Send for CMS Grade Matching

Accurate technical and commercial information allows a supplier to evaluate whether CMS offers a realistic cost-optimization route.

Current thickener information

  • Current product name and grade
  • TDS, SDS or recent COA
  • Current product price where comparison is required
  • বর্তমান মাত্রা
  • Viscosity and complete measurement method
  • Preparation procedure and hydration time

Printing information

  • Dye or pigment system
  • Current complete paste formulation
  • Flat-screen, rotary-screen or other application method
  • Production speed
  • Normal paste holding time
  • Fixation and post-treatment route

Fabric information

  • Fibre composition
  • কাপড়ের ওজন
  • Construction
  • Surface treatment
  • Representative fabric sample where possible

Cost information

  • Current thickener cost per batch
  • প্রস্তুতি সময়
  • Filter or screen-cleaning frequency
  • Paste waste
  • Additional washing or post-treatment
  • Current quality or rejection issue

Separate a Chemistry Screening Trial from a Commercial Cost Trial

First identify the reference and candidate, including product form and concentration basis. Use an equal-concentration comparison only where technically meaningful. Then optimize each formula within its validated range and compare production at the same finished-fabric quality. A supplier’s nominal viscosity or one successful print does not establish economic equivalence.

StageRequired RecordGate
IdentityGrade-specific TDS, sample label and stated chemistryResolve generic CMS versus commercial-name ambiguity
Technical trialFull recipe, independent preparations, machine and post-treatmentAll required final quality criteria pass
Cost trialActual consumption, processing, waste and accepted areaComparable cost with no duplicate ledger entries
Bulk verificationApproved sample, shipment lot and incoming testsRelease only the agreed grade and demonstrated process scope

Use the cost-per-accepted-fabric guide to define the comparison boundary. No saving percentage is implied without measured trial data.

How FSX Chemical Supports CMS Projects

FSX Chemical offers commercial CMS and related textile thickener routes for grade evaluation. Confirm the specific product identity, preparation instructions and application scope from its current documents before using a generic starch-based formulation assumption.

Commercial CMS matching should begin with the current product TDS, printing route, full viscosity method and cost objective. If the confirmed candidate chemistry differs from carboxymethyl starch, use the candidate-specific preparation and qualification plan instead of transferring this article’s chemistry assumptions.

Technical review may include

  • Review of the current thickener TDS or physical sample
  • Identification of the required CMS function
  • Alignment of viscosity test methods
  • Selection of a candidate commercial CMS grade
  • Evaluation of CMS as a primary or compound-thickener component
  • Provision of relevant TDS and SDS information
  • Representative sample support
  • Guidance for side-by-side testing
  • Review of laboratory and production-trial feedback
  • First commercial batch verification planning

Buyers can submit their current product and process information through FSX Chemical Samples & Matching .

The final commercial decision should be based on printing performance and total cost in use. A lower-priced CMS should not be approved if it creates additional process cost or reduces finished-fabric quality📧 ইমেইল: service@fsxchemical.com

দ্রুত যোগাযোগ

আপনার প্রয়োজনীয়তা পাঠান

অথবা

বিনামূল্যে নমুনা · ২৪ ঘণ্টার প্রতিক্রিয়া

পণ্যের অনুসন্ধান ও সহায়তা

আপনার পণ্যের প্রয়োজনীয়তা পাঠান

পণ্যের নাম, ব্যবহার, পরিমাণ, গন্তব্য এবং আপনার কাছে থাকা যেকোনো TDS, নমুনা ছবি বা ডকুমেন্ট শেয়ার করুন। FSX Chemical এই তথ্য পর্যালোচনা করবে এবং কোটেশন, নমুনা মিলানো বা পণ্য নির্বাচনের পরবর্তী ধাপের জন্য পরামর্শ দেবে।.

পণ্যের তথ্য পণ্যের নাম, গ্রেড, মডেল, লেবেলের ছবি বা সরবরাহকারীর রেফারেন্স।.
উপলব্ধ নথিপত্র টিডিএস, এসডিএস, সিওএ, নমুনা ছবি, পণ্যের তালিকা বা পরীক্ষার তথ্য।.
অর্ডার বিবরণ আনুমানিক পরিমাণ, প্যাকেজিং, গন্তব্য দেশ, বন্দর বা বাণিজ্যিক শর্ত।.
আবেদন বা সমস্যা টেক্সটাইল প্রিন্টিং প্রক্রিয়া, ফর্মুলেশনের প্রয়োজন, বর্তমান সমস্যা বা লক্ষ্য কর্মক্ষমতা।.