In lưới quay so với in lưới phẳng: Yêu cầu về tính lưu biến của chất làm đặc thay đổi như thế nào

Flat and rotary screen printing use the same basic transfer principle but expose printing paste...

Flat-screen and rotary-screen textile printing both force color paste through patterned screen openings, but they do not expose the thickener to the same mechanical history. Flat-screen printing is typically a reciprocating, semi-continuous process in which a squeegee crosses a stationary screen and the screen is then lifted before the fabric advances. Rotary-screen printing is continuous: paste is supplied inside a rotating cylindrical screen while an internal squeegee or magnetic-rod system forces paste through the design at production speed. Because the paste experiences different shear, residence time, recovery and circulation conditions, the rheology that works on one machine may not transfer directly to the other. This guide explains how to compare low-shear body, shear thinning, elasticity, structural recovery and long-run stability before selecting a textile printing thickener.

Same Screen-Printing Principle, Different Mechanical History

Flat-screen and rotary-screen textile printing share the same basic principle:

Printing paste is forced through open areas of a patterned screen and deposited on the fabric.

But the mechanics are different.

In flat-screen printing, a flat screen is placed over the fabric, a squeegee traverses the image area, the screen is lifted and the fabric advances to the next repeat.

In rotary-screen printing, a cylindrical screen rotates continuously with the moving fabric while paste is supplied inside the screen and forced outward through the design openings.

Textile process references describe flat-screen printing as a semi-continuous reciprocating process and rotary-screen printing as a continuous, higher-productivity process. Published rotary-screen research also shows that screen mesh, machine settings and print-paste rheology jointly affect paste deposit and penetration.

This leads to the first important rule:

The machine changes the shear history of the paste, so machine selection changes the rheology requirement.

That does not mean every rotary paste must be thinner than every flat-screen paste.

It means the complete flow-and-recovery profile must match the machine.

How Flat-Screen Printing Exposes the Paste to Shear

Flat-screen printing is usually intermittent.

A typical cycle is:

Screen Down → Squeegee Stroke → Paste Through Mesh → Screen Lift → Fabric Advance → Next Stroke

During the squeegee stroke, the paste experiences significant shear as it moves across the screen and through the open mesh.

After the stroke, however, part of the paste may remain relatively stationary on the screen before the next cycle.

This creates several rheological demands:

  • Enough low-shear body to prevent uncontrolled spreading
  • Good flow during the squeegee stroke
  • Recovery after transfer
  • Resistance to excessive paste drying or skinning during intermittent dwell
  • Repeatable viscosity between successive strokes

Flat-screen printing may therefore tolerate a different low-shear structure than a continuous rotary line, but the correct target depends on:

  • Automatic vs. manual flat screen
  • Stroke speed
  • Number of squeegee passes
  • Screen open area
  • Fabric absorbency
  • Time between strokes

Do not reduce flat-screen rheology to a rule such as “flat screen needs higher viscosity.”

How Rotary-Screen Printing Exposes the Paste to Shear

Rotary-screen printing is continuous.

The fabric travels under cylindrical screens while paste is continuously supplied inside each screen.

An internal blade, roller or magnetic-rod squeegee system forces paste through the pattern.

Commercial rotary systems are designed for high-volume production and consistent long runs.

This creates a different operating history:

Feed / Circulation → Screen Interior → High Shear at Transfer Zone → Deposit on Moving Fabric → Continued Paste Residence and Recirculation

The paste must therefore maintain useful rheology not only for one stroke but through a long, repeated mechanical history.

Important risks include:

  • Progressive viscosity drift
  • Excessive shear thinning that does not recover
  • Foam accumulation
  • Evaporation during long runs
  • Temperature rise
  • Deposit variation from beginning to end

Rotary-screen production often makes long-run rheological stability more commercially visible because even a small change can affect many meters of fabric.

Why One Viscosity Number Cannot Define Machine Suitability

A Brookfield or rotational-viscometer value is useful only under a defined method.

It usually describes one point in the paste’s flow behavior.

Screen printing exposes paste to a range of shear rates.

Research on textile printing thickeners shows that both flow and viscoelastic properties are strongly connected with print-quality parameters, and screen-printing studies show that paste behavior changes substantially between low-shear rest conditions and the high-shear conditions present during passage through screen openings.

Therefore, two pastes can both read:

30,000 mPa·s

under one test method and still behave differently in:

  • Pumping
  • Squeegee transfer
  • Mesh passage
  • Phục hồi
  • Độ thâm nhập

The correct comparison is:

Low-Shear Body + High-Shear Flow + Elasticity + Recovery + Holding Stability

1. Low-Shear Body: Holding the Pattern Before and After Transfer

At low shear, the printing paste needs enough structure to resist uncontrolled movement.

This helps support:

  • Pattern definition
  • Reduced bleeding
  • Stable paste on the screen
  • Controlled penetration

For flat-screen printing, low-shear body can be especially visible during the interval between strokes.

For rotary screen, low-shear body remains important after the paste leaves the screen and before drying, but excessive rest viscosity can create problems in feed and transfer.

The correct target is therefore not maximum rest viscosity.

It is enough structure to control the design without making the paste difficult to move.

2. Shear Thinning: Flowing Through the Screen

Textile printing pastes often need pseudoplastic or shear-thinning behavior.

Under squeegee or screen-transfer shear, apparent viscosity decreases so the paste can move through the screen openings.

Once shear is reduced, the paste can recover part of its original structure.

Research on textile printing rheology summarizes the desired balance as:

Lower viscosity under high shear for application + Higher viscosity at low shear for pattern control

If shear thinning is too weak:

  • Transfer can be incomplete.
  • Higher pressure may be needed.
  • Screen filling can become poor.

If shear thinning is excessive:

  • Paste can become too fluid during machine operation.
  • Penetration can become excessive.
  • Edges can soften.

Rotary lines often reveal excessive long-duration shear thinning more quickly because the paste experiences repeated continuous shear.

3. Structural Recovery: What Happens After the Paste Leaves the Screen?

After the paste passes through the screen, the shear rate drops sharply.

The paste should recover enough structure to stop uncontrolled lateral flow.

Recovery that is too slow can lead to:

  • Bleeding
  • Blurred fine lines
  • Haloing
  • Excess penetration

Recovery that is too fast or too strong can also create problems if the paste does not level sufficiently after transfer.

This can contribute to:

  • Uneven solid areas
  • Surface texture
  • Poor penetration

Flat and rotary machines can therefore prefer different recovery windows depending on:

  • Fabric speed
  • Time before drying
  • Lớp lắng đọng dạng bột nhão
  • Design coverage

Structural recovery should be evaluated on the actual machine, not inferred from static viscosity.

4. Elasticity and Stringiness

Viscoelasticity affects how printing paste deforms and separates from the screen.

Some elasticity can support recovery.

Too much elasticity can create:

  • Stringiness
  • Poor screen release
  • Uneven deposit
  • Tail or edge defects

Published textile-thickener research notes that elasticity influences both passage through screen openings and subsequent flow through textile fibers.

This property can become especially important when transferring a formula between flat and rotary machines because screen separation mechanics differ.

Do not assume a highly elastic paste that performs well on one machine will automatically release cleanly on the other.

5. Long-Run Stability: Why Rotary Often Exposes Hidden Weaknesses

Rotary-screen printing is designed for continuous high-volume production.

That means a paste may remain in the machine system for an extended period while experiencing:

  • Repeated shear
  • Circulation
  • Mechanical pumping
  • Air incorporation
  • Temperature variation
  • Evaporation

A useful rotary-screen paste should therefore be checked at:

  • Start of run
  • After a defined production interval
  • Mid-run
  • Near the end of the intended production window

So sánh:

  • Độ nhớt
  • Bọt
  • Screen running
  • Hiệu suất màu
  • Pattern definition

A paste that gives an excellent 10-meter sample but drifts after 1,000 meters has not passed a realistic rotary-screen qualification.

6. Intermittent Dwell: Why Flat-Screen Paste Can Fail Differently

Flat-screen printing introduces intermittent waiting periods.

During these periods, paste on the screen can:

  • Lose water at the surface
  • Become locally thicker
  • Dry around fine openings
  • Change transfer between strokes

This creates defects such as:

  • Fine-mesh blocking
  • Uneven first stroke after a pause
  • Increasing squeegee pressure requirement
  • Pattern inconsistency after machine stops

For flat-screen production, evaluate pause/restart behavior in addition to continuous printing behavior.

A useful trial can include a controlled machine stop followed by a restart to see whether paste recovery and screen openness remain acceptable.

Paste Deposit and Penetration

Machine type changes how paste is deposited onto and into the fabric.

Rotary-screen research has shown that paste application and penetration are affected jointly by:

  • Screen mesh
  • Machine settings
  • Paste rheology

The same thickener can therefore give different:

  • Wet pickup
  • Độ thâm nhập
  • Surface color
  • K/S
  • Độ sắc nét khi in

when moved between flat and rotary machines.

When transferring a formula, do not adjust viscosity alone.

Measure or observe the printed paste deposit and final penetration.

Screen Mesh and Squeegee Settings Still Matter

Machine architecture is only one part of the system.

Screen mesh, engraving/open area, squeegee pressure, squeegee type and speed also change the shear and deposit.

For this article, the important principle is:

Machine Type × Screen Geometry × Squeegee Conditions × Paste Rheology = Printing Result

A thickener should not be labeled “rotary grade” or “flat-screen grade” without knowing the screen and machine conditions.

Fine mesh can require easier high-shear flow than an open design.

Higher pressure can force more paste through the screen and change penetration.

These variables should be recorded during grade matching.

Fabric Construction Changes the Required Rheology

The same flat or rotary machine can require different paste behavior on different fabrics.

Important variables include:

  • Woven vs. knitted
  • Fabric weight
  • Surface hairiness
  • Absorbency
  • Stretch
  • Open vs. dense construction

A highly absorbent cotton fabric may pull paste rapidly into the structure.

A smooth polyester surface can retain more paste at the surface.

Therefore, machine comparison should always be made on the same fabric when possible.

Otherwise, fabric effects can be mistaken for rheology effects.

In bằng thuốc nhuộm phản ứng

Reactive printing pastes often use sodium alginate or other carefully selected thickeners for cellulosic fabrics.

When moving from flat to rotary screen, evaluate:

  • Complete-paste viscosity after dye and alkali
  • Shear thinning
  • Fine-line definition
  • Độ thâm nhập
  • Color yield after steaming
  • Rửa trôi

The same sodium alginate concentration may need adjustment if the rotary machine produces a different deposit or penetration.

However, do not make a dosage change before measuring the actual print result.

In phân tán

Polyester disperse screen printing adds another requirement: the thickener must release the dye effectively during thermal fixation.

A paste can run well on a rotary screen but still reduce final K/S if the thickener film restricts dye release.

When comparing flat and rotary disperse printing, check:

  • Duy trì sự ổn định
  • Screen running
  • Printed deposit
  • Cố định bằng nhiệt
  • Final K/S
  • Wash-off / reduction clearing

Machine rheology and thermal-fixation performance must both pass.

In bằng mực màu

Pigment printing adds binder to the rheology problem.

The complete paste may contain:

  • Dung dịch phân tán sắc tố
  • Binder
  • Chất làm đặc
  • Fixer
  • Auxiliaries

When changing machine type, evaluate whether the binder/thickener system maintains:

  • Chuyển hình ảnh lên màn hình
  • Pattern definition
  • Duy trì sự ổn định
  • Curing performance
  • Vải dệt tay
  • Độ bền khi cọ xát

Do not increase thickener only to solve a machine-transfer problem if the extra polymer solids worsen hand after curing.

How to Transfer a Paste from Flat Screen to Rotary Screen

Do not begin by changing several formulation variables at once.

Step 1: Use the Existing Flat-Screen Paste as the Reference

Bản ghi:

  • Thickener grade
  • Nồng độ
  • Viscosity method
  • Vải
  • Screen
  • Squeegee conditions
  • Printed result

Step 2: Run the Same Paste on Rotary at Controlled Speed

Observe:

  • Feed stability
  • Đoạn trích trên màn hình
  • Deposit
  • Pattern definition
  • Độ thâm nhập

Step 3: Check Long-Run Change

Recheck paste and print after a meaningful production interval.

Step 4: Adjust One Rheology Variable at a Time

Possible directions include:

  • Thickener concentration
  • Grade / molecular structure
  • Compound-thickener ratio

Do not assume the rotary version simply needs a lower viscosity.

How to Transfer a Paste from Rotary Screen to Flat Screen

The reverse transfer requires a different check.

A paste optimized for continuous rotary running may show:

  • Too much spreading during flat-screen dwell
  • Different recovery after the squeegee stroke
  • Screen drying during pauses
  • Different paste deposit from multiple strokes

Run the same paste first, then evaluate whether:

  • Low-shear body needs adjustment
  • Recovery needs adjustment
  • Water retention needs improvement
  • The number of squeegee strokes should change

Again, change the minimum number of variables needed to identify the cause.

Laboratory Rheology Test Plan

For a technical comparison, use the complete printing paste rather than the thickener stock solution alone.

At minimum, standardize:

  • Thickener concentration
  • Nước
  • Dye/pigment/binder formula
  • Nhiệt độ
  • Bổ sung nước
  • Thời gian giữ

Đơn vị đo lường:

Low-Shear Viscosity

Represents paste body during storage/rest conditions.

Higher-Shear Viscosity

Shows how easily the paste flows under application stress.

Phục hồi

Measure whether viscosity/structure rebuilds after a high-shear interval.

Viscoelasticity Where Equipment Is Available

Storage/loss response can help identify excessively elastic or weak-gel behavior.

If the mill does not have a rheometer, build a practical correlation using:

  • Multiple viscometer speeds
  • Controlled high-speed mixing
  • Recovery measurement after mixing
  • Standardized screen-print trials

The laboratory target is to reproduce machine-relevant behavior, not to generate rheology data with no production connection.

Production Trial and Approval Criteria

Approve a thickener for flat or rotary screen only after production-scale validation.

Bản ghi:

  • Machine type
  • Tốc độ máy
  • Screen specification
  • Squeegee type/settings
  • Fabric lot
  • Paste batch
  • Starting viscosity
  • Độ nhớt giữa chu kỳ
  • Độ nhớt khi chảy qua khe hở
  • Print quality

Đánh giá:

  • Beginning-to-end shade consistency
  • Pattern definition
  • Độ thâm nhập
  • Screen cleanliness
  • Bọt
  • Sự gián đoạn do máy móc
  • Final K/S / fastness / hand after full processing

The approval target should be an operating window, not one perfect sample.

Troubleshooting Flat vs. Rotary Screen Problems

Vấn đề được ghi nhậnCác biến cần kiểm tra trước tiênĐừng vội kết luận
Paste works on flat but spreads on rotaryShear thinning, recovery, deposit, machine speedRotary always needs a thicker paste
Paste works on flat but transfers poorly on rotaryHigh-shear flow, screen geometry, feed stabilityHigher squeegee pressure is the only solution
Paste works on rotary but blocks during flat-screen pausesWater retention, surface drying, dwell timeThe thickener is unsuitable in all flat-screen systems
Rotary quality drifts during a long runShear history, temperature, foam, evaporation, holding stabilityThe initial viscosity proves long-run stability
Same viscosity gives different penetrationScreen, squeegee, rheology, fabricSame Brookfield value means same application
Fine lines improve but solid areas become unevenRecovery, leveling, paste depositMaximum structural recovery is always best
Machine transfer improves but final color dropsDeposit, dye mobility, fixation, wash-offMachine rheology alone defines product suitability

Tổng chi phí trong quá trình sử dụng

Machine-specific rheology affects more than print quality.

Bao gồm:

  • Liều lượng chất làm đặc
  • Paste preparation
  • Pumping energy
  • Tốc độ máy
  • Screen interruptions
  • Waste paste
  • Sửa lại
  • Final washing or curing

A useful framework is:

Total Cost in Use = Thickener Cost + Preparation + Machine Efficiency + Downtime + Post-Treatment + Rework + Quality Loss

A thickener that costs more per kilogram can be the lower-cost rotary route if it maintains long-run viscosity and reduces interruptions.

A lower-cost product can be the better flat-screen route if it provides stable print definition without drying on the screen.

Compare cost per acceptable printed meter, not powder price alone.

Bạn nên cung cấp những thông tin nào cho nhà cung cấp chất làm đặc?

For useful flat-vs-rotary grade matching, provide:

  • Rây phẳng hoặc rây quay
  • Machine manufacturer/model where relevant
  • Tốc độ sản xuất
  • Screen mesh/engraving
  • Squeegee type and settings
  • Fabric composition and construction
  • Dye/pigment route
  • Current thickener product/TDS
  • Liều lượng hiện tại
  • Viscosity and full test method
  • Complete or simplified formula
  • Thời gian giữ keo
  • Current defect: spreading, transfer, blocking, drift, penetration or cost

FSX Chemical có thể sử dụng thông tin này thông qua Mẫu và việc kết hợp to compare sodium alginate, CMC, CMS or other route-appropriate thickeners under matched machine conditions.

How Should Thickener Rheology Be Matched to Flat or Rotary Screen?

Một chuỗi quyết định thực tiễn là:

Machine Mechanics → Shear History → Low-Shear Body → High-Shear Flow → Recovery → Paste Deposit → Finished Print → Long-Run Repeatability

Các nguyên tắc chính là:

  1. Flat and rotary screen use the same transfer principle but expose paste to different mechanical histories.
  2. Same viscosity does not mean the same flow, recovery or machine behavior.
  3. Rotary production places strong emphasis on continuous shear and long-run stability.
  4. Flat-screen production adds intermittent dwell, pause/restart and screen-drying risks.
  5. Screen mesh, squeegee and fabric must be recorded before changing the thickener.
  6. The final acceptance standard is stable production and finished-print quality—not a viscosity number alone.

Các câu hỏi thường gặp

1. Does rotary-screen printing need lower-viscosity paste than flat-screen printing?

Not as a universal rule. Rotary printing often needs excellent high-shear flow and long-run stability, while flat screen can place more emphasis on low-shear hold and pause/restart behavior. Test the actual machine.

2. Why can the same paste work on flat screen but fail on rotary screen?

Rotary printing exposes the paste to continuous feed, repeated shear, circulation and longer machine residence. A paste can therefore drift or thin differently during a long run.

3. Why can a rotary paste fail on flat screen?

Flat-screen dwell between strokes can expose weak low-shear body, slow structural recovery or surface drying that was less visible on the continuous rotary line.

4. Is Brookfield viscosity enough to select a thickener?

No. It should be combined with shear-thinning, recovery, elasticity and machine-print testing.

5. What rheology is generally useful for screen printing?

A useful paste often has sufficient viscosity at low shear, lower apparent viscosity under application shear and enough recovery after transfer to control spreading.

6. Does faster rotary speed always require lower paste viscosity?

No. Speed changes shear, residence and deposit conditions, but the correct adjustment can involve rheology, screen specification, squeegee settings or thickener grade—not viscosity alone.

7. Why does rotary print quality change from the beginning to the end of a run?

Check repeated shear, paste temperature, evaporation, foam, holding stability and feed conditions.

8. Why does flat-screen paste dry in the screen?

Possible causes include long dwell, low humidity, excessive paste concentration, poor water retention or fine mesh. Diagnose the complete system.

9. Does higher structural recovery always give sharper printing?

No. Excessively fast or strong recovery can reduce leveling and cause uneven solid areas. The target is a balanced recovery window.

10. Can the same sodium alginate grade be used for both flat and rotary reactive printing?

Often it can be evaluated on both, but concentration and process settings may need adjustment. Approve the grade on each machine.

11. Should I change thickener before changing screen or squeegee settings?

Not automatically. Machine settings and rheology interact. Record the current screen/squeegee conditions and change one major variable at a time.

12. What should I send FSX Chemical for flat-vs-rotary matching?

Send machine type, speed, screen, squeegee conditions, fabric, dye route, current thickener, dosage, viscosity method, formula and the current machine defect.

Match Thickener Rheology to Your Flat or Rotary Screen

If the same printing paste behaves differently after moving between flat and rotary screen machines, FSX Chemical can help determine whether the next trial should focus on thickener grade, concentration, shear recovery or machine/process conditions.

For a useful technical comparison, send:

  • Your current thickener sample, TDS or COA
  • Rây phẳng hoặc rây quay
  • Tốc độ máy
  • Screen mesh/engraving
  • Squeegee type/settings
  • Fabric composition and construction
  • Dye/pigment route
  • Current thickener dosage
  • Độ nhớt và phương pháp thử nghiệm toàn diện
  • Complete or simplified formula
  • Thời gian giữ keo
  • Current screen-running, spreading, penetration, color or cost target

Bắt đầu bằng Mẫu và việc kết hợp for a controlled machine comparison.

Đánh giá Alginat natri, CMC, CMS và Hỗn hợp in kỹ thuật số for route-specific thickener information.

Bạn cũng có thể Yêu cầu báo giá trực tiếp từ nhà máy after the suitable rheology route is confirmed or Liên hệ với FSX Chemical để thảo luận về các vấn đề kỹ thuật📧 Email: Service@fsxchemical.com

The most useful question is not “Which viscosity is best for rotary or flat screen?” It is “What rheological profile gives stable transfer, recovery and print quality under this machine’s real shear history?”

Liên hệ nhanh

Gửi yêu cầu của bạn

hoặc

Mẫu thử miễn phí · Trả lời trong vòng 24 giờ

Thắc mắc về sản phẩm & Hỗ trợ

Gửi yêu cầu về sản phẩm của bạn

Vui lòng cung cấp tên sản phẩm, ứng dụng, số lượng, điểm đến và bất kỳ tài liệu kỹ thuật (TDS), hình ảnh mẫu hoặc tài liệu nào mà quý khách đã có. FSX Chemical sẽ xem xét thông tin này và đề xuất bước tiếp theo liên quan đến báo giá, đối chiếu mẫu hoặc lựa chọn sản phẩm.

Thông tin sản phẩm Tên sản phẩm, cấp loại, mẫu mã, ảnh nhãn mác hoặc mã tham chiếu của nhà cung cấp.
Các tài liệu có sẵn TDS, SDS, COA, ảnh mẫu, danh mục sản phẩm hoặc dữ liệu thử nghiệm.
Chi tiết đơn hàng Số lượng dự kiến, hình thức đóng gói, nước nhập khẩu, cảng hoặc điều kiện thương mại.
Yêu cầu hoặc Vấn đề Quy trình in trên vải, yêu cầu về công thức, vấn đề hiện tại hoặc chỉ tiêu hiệu suất.