Cách chọn chất làm đặc phù hợp cho quá trình in trên vải

The right textile printing thickener depends on more than the dye system. Fibre composition, fabric...

Textile printing thickener selection often begins with a question about viscosity, product price or dye compatibility. These factors are important, but they do not provide enough information to select the correct product.

The fabric itself is one of the most important parts of the selection process. Cotton, viscose, polyester, nylon, silk, wool and blended fabrics interact differently with water, dyes, pigments, binders and printing pastes.

Even two fabrics made from the same fibre can produce different results. Fabric weight, weave or knit structure, yarn density, absorbency, surface finish and previous chemical treatments can change paste pickup, penetration, spreading and drying.

Select the colorant chemistry and printing route first, then evaluate the thickener on the production fabric. Fibre composition alone does not establish chemical compatibility. The candidate must support preparation, filtration, application and stability while meeting the finished-textile requirements.

Why Fabric Should Come First in Thickener Selection

A printing thickener controls how the color paste or pretreatment moves before, during and after application. The fabric determines how that paste is accepted by the textile surface.

Fabric influences paste pickup

Open, textured or absorbent fabrics may accept more paste than dense, smooth or previously treated fabrics. The same machine settings can therefore produce different application quantities.

Fabric influences penetration

Some textile constructions allow the paste to move quickly through the surface, while others retain more material near the top of the fabric.

Fabric influences print definition

Fine lines and small details can appear sharp on one fabric but spread or break on another because the surface, yarn structure and absorbency are different.

Fabric influences drying and fixation

Fabric weight, moisture content and construction can change drying speed, heat transfer and the behavior of the colorant during fixation or curing.

Fabric influences final handle

A formulation that leaves an acceptable surface on a heavy fabric may create noticeable stiffness or residue on a lightweight textile.

The fabric should therefore be part of the original inquiry, laboratory comparison and production trial.

Build a Fabric Profile Before Requesting Samples

A useful fabric profile helps the supplier identify a practical thickener route before sending unrelated samples.

Record the fibre composition

  • 100% cotton
  • Viscose or rayon
  • Polyester
  • Nylon
  • Lụa
  • Len
  • Cotton-polyester blend
  • Other natural, synthetic or blended fibres

Record the fabric construction

  • Woven or knitted
  • Fabric weight
  • Yarn count
  • Thread or loop density
  • Surface texture
  • Stretch or dimensional movement
  • Single-layer or raised construction

Record previous treatments

  • Scouring
  • Bleaching
  • Mercerizing
  • Heat setting
  • Optical brightening
  • Water-repellent treatment
  • Softener or finishing treatment
  • Digital printing pretreatment

Record the printing route

Confirm the colorant system, printing machine, application method, fixation process and final quality target.

Provide a representative fabric sample

A physical sample or production lot provides more useful information than a description such as “cotton fabric” or “polyester cloth” alone.

Main Textile Printing Thickener Families

The families below provide starting directions, not automatic approvals. Sodium alginate and CMC identify polymer chemistries; FSX CMS is a commercial synthetic thickener family. Compound thickeners and digital printing pastes are application-specific formulations, so their grade documents and intended process must also be checked.

Thickener FamilyCommon Starting RouteImportant Fabric ConsiderationsMain Caution
Alginat natriReactive printing on suitable cellulosic fabricsFabric absorbency, construction, penetration, wash-off and handleNot a universal route for pigment, disperse or every digital process
Carboxymethyl celluloseSelected printing, compound thickener, coating and sizing formulationsSurface film, penetration, electrolyte response and removalSimilar viscosity does not prove equivalent fabric performance
FSX CMS (commercial synthetic thickener family)Selected disperse, compound and specialized printing formulationsFilm behavior, paste transfer, wash-off and fabric handleNot an automatic one-to-one replacement for sodium alginate
Synthetic thickenerPigment printing and specialized formulationsBinder compatibility, surface coverage, curing and handlePerformance depends on pH, binder and complete formula
Compound thickenerApplication-specific reactive, pigment or disperse systemsFabric-specific rheology, penetration, pickup and stabilityCompound products with similar viscosity may have different compositions
Digital printing pasteReactive, disperse or pigment digital pretreatmentUniform pickup, ink spreading, drying, fixation and surface handleMust be matched to the specific fabric and ink route

The available FSX product directions can be reviewed through the textile printing thickener product range .

1. Selecting a Thickener for Cotton and Viscose

Cotton and viscose are cellulosic fibres commonly printed with reactive dyes. A suitable thickener must be evaluated together with the dye, alkali, salt, humectant, fabric and fixation process.

Sodium alginate as a starting route

Alginat natri is a common starting route for reactive printing on suitable cellulosic fabrics. Commercial grades can differ in viscosity, hydration, filtration and rheological behavior.

Cotton and viscose are not identical

Viscose may show different moisture absorption and paste penetration from a cotton fabric of similar weight. The dosage and rheological balance should therefore be confirmed separately.

Evaluate fabric absorbency

Highly absorbent material may allow excessive paste penetration or edge spreading. A less absorbent or tightly constructed fabric may require stronger transfer and leveling.

Check wash-off and handle

Evaluate the finished fabric after the complete steaming and washing process. Residual thickener or incomplete removal may affect the surface and handle.

Consider a compound route carefully

CMC, FSX CMS or another candidate may be evaluated in a validated reactive compound formulation. Confirm dye compatibility, fixation, wash-off and handle at the proposed composition; matching stock-paste viscosity does not establish a direct replacement for sodium alginate.

2. Selecting a Thickener for Polyester

Polyester can be printed through disperse or pigment routes, and it is widely used in digital textile production. Each route requires a different starting formulation.

Disperse screen printing

CMS, selected synthetic thickeners or application-specific compound products may be evaluated according to the disperse dye, paste stability, printing equipment and fixation process.

Pigment printing on polyester

The thickener must remain compatible with the pigment dispersion, binder, crosslinking system and curing conditions.

In kỹ thuật số phân tán

A dedicated disperse digital printing paste should be evaluated with the actual polyester fabric, application method, ink, drying and fixation route.

Heat setting may influence the surface

Previously heat-set or finished polyester may accept pretreatment differently from unfinished material. Use the production fabric during approval.

Check migration and surface quality

Final evaluation should include shade uniformity, definition, surface appearance, fixation and any color movement during thermal processing.

3. Selecting a Thickener for Nylon, Silk and Wool

Nylon, silk and wool may use acid-dye or other specialized printing routes; silk can also be printed with suitable reactive systems. Confirm the actual fibre, dye class and fixation procedure before selecting a thickener. A cotton reactive formulation is not automatically suitable for these fabrics.

Confirm the dye system first

Identify whether the application uses acid dyes, metal-complex dyes, pigments or another colorant route.

Protect sensitive fabric handle

Silk and lightweight wool fabrics can show residual stiffness or surface buildup more clearly than heavy fabrics.

Control penetration

Fine, open or highly absorbent constructions may require careful control of paste transfer and structural recovery.

Check pH and chemical compatibility

The thickener must remain stable under the pH and auxiliary conditions used by the selected acid or specialized printing process.

Request an application-specific grade

Do not assume that a general sodium alginate, CMC, CMS or digital paste is automatically approved for nylon, silk or wool. Request a suitable candidate and complete fabric testing.

4. Selecting a Thickener for Blended Fabrics

Blended fabrics can be more difficult because each fibre component may respond differently to water, colorants, binders and fixation.

Cotton-polyester blends

The printing route may target one fibre, use pigments across both fibres or require a combined process. The thickener should be selected according to the actual colorant strategy.

Different absorption within one fabric

One fibre may absorb or retain more liquid than another, which can affect local penetration, sharpness and shade.

Different fixation requirements

A combined dye process may use more complicated thermal or chemical conditions than a single-fibre system.

Pigment routes may simplify coloration but still require testing

Pigments can color multiple fibre types through a binder film, but binder compatibility, curing, rubbing performance and handle remain important.

Use the actual blend ratio and fabric construction

A candidate tested on 100% cotton or 100% polyester cannot automatically represent a blended production fabric.

5. Consider Fabric Weight and Construction

Fibre composition describes the material, but construction determines how yarns, loops and open spaces interact with the printing paste.

Lightweight fabrics

Lightweight materials may be more sensitive to strike-through, excessive penetration and residual stiffness.

Heavy fabrics

Heavy or dense fabrics may require sufficient transfer and penetration to avoid weak surface coverage or incomplete coloration.

Open woven structures

Open structures can allow the paste to move through the fabric more easily. Back-side contamination and loss of definition should be checked.

Dense woven structures

Tight constructions may retain more paste near the surface and require appropriate flow and leveling.

Knitted fabrics

Knitted textiles may stretch or distort during application and drying. Paste pickup and pattern dimensions should be monitored.

Raised or textured fabrics

Fleece, brushed, ribbed or textured surfaces may require different transfer and penetration from a smooth plain weave.

6. Evaluate Fabric Absorbency

Absorbency influences how quickly liquid moves into and across the fabric. It should be measured or compared rather than assumed from fibre name alone.

High absorbency may cause

  • Rapid penetration
  • Loss of surface color concentration
  • Wider print edges
  • Uneven pickup across variable fabric areas
  • Greater sensitivity to application quantity

Low absorbency may cause

  • Excessive surface retention
  • Slow drying
  • Uneven leveling
  • Poor wetting
  • Surface smearing before fixation

Do not correct absorbency only by increasing viscosity

A higher viscosity may reduce flow but can also reduce transfer or create an excessive surface film. Pretreatment, wetting, application quantity and rheology should be reviewed together.

Test several fabric lots when necessary

Scouring, finishing and raw-material variation may cause absorbency differences between production lots.

7. Check Surface Treatments and Residual Chemicals

Previous textile processing can influence wetting, chemical compatibility and print uniformity.

Residual oils or waxes

Incomplete preparation may create poor wetting, missing areas or uneven paste pickup.

Softener residues

Some finishing materials may change surface energy or interact with binders, pretreatments and colorants.

Water-repellent finishes

A water-repellent surface can prevent uniform paste application. Changing the thickener alone may not solve the problem.

Variable pH or residual chemicals

Residual alkali, acid, salt or detergent can alter the local printing chemistry.

Optical brighteners and other finishes

These materials may affect apparent shade, curing or final evaluation.

Compare prepared and untreated fabric where practical

This can help determine whether a defect originates from the printing paste or the incoming textile.

8. Match the Thickener to the Printing Method

The same fabric may require different paste behavior when printed by flat-screen, rotary-screen or digital equipment.

In trên màn hình phẳng

Evaluate screen passage, squeegee transfer, pattern definition, penetration and paste recovery after application.

In lụa quay

The paste must also circulate and pass through the rotary screen under repeated production shear. Long-run stability becomes especially important.

Digital textile printing

In many digital systems, the thickening function is part of a fabric pretreatment applied before inkjet printing. Uniform pickup and controlled ink spreading are central evaluation points.

Padding or coating

The formulation must provide uniform wet pickup or coating weight across the fabric width without excessive foam or leveling defects.

Do not transfer a screen-printing formula directly to digital use

The equipment, application quantity and role of the paste are different. Use an application-specific digital printing route.

9. Define the Required Viscosity and Rheology

Viscosity provides a useful control value, but fabric performance depends on how the paste flows and recovers under different conditions.

Use a complete viscosity method

  • Nồng độ mẫu
  • Nguồn nước
  • Quy trình trộn và ngâm nước
  • Nhiệt độ đo
  • Instrument and spindle
  • Tốc độ quay
  • Reading time and unit

Evaluate flow during application

The paste should move sufficiently through the screen or application equipment and transfer uniformly onto the fabric.

Evaluate structural recovery

Measure flow as shear rate changes and, where time dependence matters, measure recovery after a defined shear history. Shear thinning is a decrease in apparent viscosity with increasing shear rate; it does not by itself prove time-dependent recovery. Connect both observations with spreading, penetration and leveling on the fabric.

The fabric changes the preferred rheology

A highly absorbent lightweight fabric may require a different balance from a dense, smooth and low-absorbency textile.

Do not select the highest viscosity automatically

Excessive viscosity can reduce transfer, produce uneven solid areas or increase machine resistance.

10. Test Chemical Compatibility

The thickener must remain suitable after dyes, pigments, salts, alkalis, binders and auxiliaries are added.

Reactive formulations

Test the selected sodium alginate or compound route with representative reactive dyes, alkali, salt and humectant levels.

Pigment formulations

Confirm compatibility with the actual pigment dispersion, binder, crosslinker and curing system.

Disperse formulations

Evaluate paste stability, dye distribution, fixation conditions and final polyester surface quality.

CMC and CMS formulations

CMC và CMS may respond differently to pH, electrolytes, dyes and other polymers.

Ghi lại các thay đổi ngay lập tức và chậm trễ

Check viscosity, appearance, separation and filtration immediately after formulation and after the normal holding period.

11. Review Filtration and Paste Stability

A thickener that produces the correct initial viscosity may still be unsuitable when it creates residue or changes during storage and production.

Test filtration using a defined method

Record filter material, opening size, sample quantity, filtration condition and time.

Inspect the retained material

Determine whether residue consists of incompletely hydrated powder, gel, precipitated chemicals, fibre contamination or foreign matter.

Kiểm tra độ ổn định của vị thế nắm giữ

  • Sự thay đổi độ nhớt
  • Sự tách biệt
  • Thanh toán
  • Khả năng giữ bọt
  • Skin formation
  • Phát triển gel
  • Khả năng lọc sau khi bảo quản

Use the actual factory holding period

A short laboratory observation may not represent a paste stored or circulated for several hours.

Connect stability with fabric performance

Print or apply both fresh and stored paste to determine whether changes affect pickup, definition, shade or handle.

Quick Selection Matrix by Fabric and Printing Route

Fabric and RoutePractical Starting Thickener RouteCritical Fabric Tests
Cotton reactive screen printingSodium alginate or validated reactive compound thickenerDefinition, penetration, dye compatibility, wash-off and handle
Viscose reactive printingMatched sodium alginate or reactive compound routeAbsorbency, spreading, penetration, shade and residual handle
Polyester disperse screen printingCMS, synthetic or application-specific compound thickenerTransfer, fixation, migration, levelness and surface appearance
Polyester pigment printingBinder-compatible synthetic or compound thickenerCoverage, curing, rubbing performance and fabric handle
Cotton-polyester pigment printingValidated pigment thickener and binder systemUniformity across both fibres, curing, rubbing and handle
Reactive digital printing on cottonDedicated reactive digital printing pastePretreatment pickup, definition, fixation, wash-off and handle
Disperse digital printing on polyesterDedicated disperse digital printing routeUniform application, drying, fixation and migration behavior
In kỹ thuật số bằng mực màuDedicated binder-compatible pigment pretreatmentInk spreading, curing, rubbing performance and handle
Nylon, silk or wool printingApplication-specific acid or specialized printing thickenerpH compatibility, definition, fixation, washing and softness

This matrix identifies initial product families only. The final commercial grade requires controlled testing on the actual production fabric.

Step 1: Select the production fabric

Use the actual fabric or a technically representative production lot.

Step 2: Select the current reference

Include the thickener or paste currently approved for routine production.

Step 3: Define acceptance criteria

Record the required preparation, viscosity, filtration, stability, transfer and final fabric performance.

Step 4: Standardize paste preparation

  • Use the same water source
  • Sử dụng cùng một cơ sở nồng độ
  • Sử dụng các thùng chứa và máy trộn giống hệt nhau
  • Control addition time
  • Control mixing and hydration time
  • Measure at the same temperature

Step 5: Test the stock paste

  • Dispersion or powder wetting
  • Sự hình thành khối u
  • Thời gian bù nước
  • Độ nhớt
  • Lọc
  • Foam and physical stability

Step 6: Prepare the complete formulation

Add the actual dyes, pigments, salts, alkalis, binders and auxiliaries in the normal sequence.

Step 7: Test the holding period

Measure and inspect the completed paste after the normal factory holding time.

Step 8: Apply to the fabric

Use representative screen, coating, padding or digital pretreatment conditions.

Step 9: Complete post-treatment

Follow the normal drying, steaming, fixation, curing and washing process.

Step 10: Compare finished fabric

Evaluate definition, penetration, shade, levelness, handle and relevant durability before making a commercial decision.

How to Evaluate the Printed Fabric

Final approval should be based on the finished textile rather than the prepared paste alone.

Inspect fine lines, small text, corners and closely spaced pattern elements.

Độ thâm nhập

Check the face and reverse side of the fabric. The preferred depth depends on the design, construction and end use.

Color spreading

Determine whether color moves beyond the intended pattern boundary.

Solid-area levelness

Inspect large printed areas for mottling, uneven pickup, foam marks or incomplete transfer.

Shade and color strength

Compare candidates after identical fixation and post-treatment rather than from the wet print.

Wash-off or curing

Evaluate residual material, binder performance and the effectiveness of the normal downstream process.

Tay cầm bằng vải

Check stiffness, stickiness, surface buildup and differences between printed and unprinted areas.

Relevant fastness or durability

Complete the testing required by the buyer’s product and customer standards.

How to Move from One Fabric to Another

A formula approved for one fabric should not be transferred automatically to another material, even when the fibre name is the same.

Thay đổi từng biến một

Begin by keeping the approved formula and recording how the new fabric changes pickup, penetration and definition.

Compare fabric preparation

Confirm whether both fabrics have the same scouring, bleaching, heat setting or finishing history.

Compare absorbency and construction

Record fabric weight, density, thickness, surface texture and wetting behavior.

Adjust dosage or rheology in controlled steps

Avoid changing thickener grade, application quantity, auxiliaries and machine settings simultaneously.

Repeat final textile evaluation

The new fabric requires its own fixation, wash-off, curing, handle and durability checks.

Create separate approved recipes when necessary

Maintaining different controlled formulas for different fabric groups may be more reliable than forcing one recipe to cover every textile.

Cách so sánh tổng chi phí sử dụng

The lowest thickener price does not automatically produce the lowest cost per acceptable metre of printed fabric.

Material cost

Include delivered price and actual optimized dosage.

Chi phí chuẩn bị

Bao gồm các công đoạn: thêm bột, trộn, ngâm nước, gia nhiệt, làm mát, nhân công và lọc.

Application cost

Include machine speed, pickup control, screen cleaning, filter changes and corrective additions.

Waste cost

Include unused paste, filter residue, tank residue and rejected batches.

Fabric-quality cost

Include reprinting, additional washing, off-quality fabric and customer claims.

Fabric-change cost

A thickener that requires major reformulation for every fabric may create additional laboratory, inventory and production complexity.

Compare products only after they meet the same finished-fabric and production requirements.

Information to Send to the Supplier

Fabric information

  • Fibre composition and blend ratio
  • Woven or knitted construction
  • Fabric weight
  • Surface texture
  • Absorbency or wetting information
  • Previous preparation or finishing treatment
  • Representative fabric sample

Printing information

  • Reactive, disperse, pigment, acid or digital route
  • Hệ thống thuốc nhuộm, bột màu hoặc mực in
  • Flat-screen, rotary-screen or digital equipment
  • Current printing speed or application conditions
  • Fixation, curing or steaming process
  • Washing and finishing process

Current product information

  • Current thickener name and grade
  • TDS, SDS hoặc COA hiện tại
  • Liều lượng hiện tại
  • Độ nhớt và phương pháp thử nghiệm toàn diện
  • Quy trình chuẩn bị
  • Current paste or powder sample

Performance information

  • Main printing defect
  • Desired definition or penetration
  • Required fabric handle
  • Filtration or stability problem
  • Cost or dosage objective
  • Printed-fabric photographs or sample

Common Fabric-Based Selection Mistakes

Selecting only by fibre name

Two cotton fabrics can differ in weight, construction, absorbency and preparation.

Using one formula for every fabric

A formula approved for a heavy woven fabric may not suit a lightweight knit or open construction.

Choosing the highest viscosity

Excessive viscosity may reduce transfer and produce uneven surface coverage.

Ignoring fabric preparation

Residual oils, softeners or water-repellent finishes can create defects that cannot be corrected by changing the thickener alone.

Chỉ tiến hành thử nghiệm trong nước sạch

The final dyes, pigments, binders and auxiliaries may change the paste behavior.

Evaluating only the wet print

Shade, definition, wash-off and handle may change after fixation and washing.

Approving one small fabric area

The test should represent normal fabric variation and production application.

Skipping the first-batch verification

The first commercial thickener batch should be compared with the approved sample before routine production use.

Vấn đề được ghi nhậnPossible Fabric or Paste CausesCác kiểm tra được khuyến nghị
Print edges spreadHigh absorbency, slow structural recovery, excessive pickup or low paste bodyReview fabric wetting, rheology, dosage and application quantity
Excessive reverse-side penetrationLightweight or open construction, excessive pressure or low paste structureReview fabric construction, machine pressure, pickup and rheology
Poor surface coverageDense or textured fabric, insufficient transfer, excessive viscosity or poor wettingReview transfer, paste flow, fabric surface and application amount
Uneven solid areasVariable absorbency, foam, poor leveling or inconsistent fabric preparationCompare fabric lots, paste uniformity, foam and preparation
Weak color after washingInsufficient fixation, excessive penetration, incompatible thickener or incorrect dye conditionsReview formulation, fabric preparation, fixation and wash-off
Fabric feels stiffExcessive paste pickup, poor removal, binder film or heavy surface depositionReview dosage, pickup, washing, curing and thickener route
Pretreatment applies unevenlyVariable fabric wetting, unstable viscosity, foam or coating equipment variationCheck absorbency, paste stability, filtration and pickup records
One fabric lot prints differentlyDifferent preparation, absorbency, weight, construction or residual finishCompare incoming-fabric data and conduct a controlled wetting test
Correct viscosity but poor definitionUnsuitable rheology, fabric absorbency, excessive application or surface treatmentReview multi-speed behavior, fabric profile and application conditions

A Two-Fabric Trial to Separate Fabric and Paste Effects

When a candidate works on one fabric but fails on another, use a small comparison matrix before changing its dosage. This proposed trial separates incoming-fabric variation from the effect of the thickener.

  1. Choose two fabric lots. Include an approved production lot and the lot showing the defect. Record fibre composition, construction, preparation, absorbency and residual finish; condition and sample them consistently.
  2. Prepare two complete pastes. Compare the approved reference with the candidate using recorded water, mixing, chemical additions and holding time. Check both stock-paste and complete-paste properties.
  3. Apply all four combinations. Print each paste on each fabric under controlled machine settings. Record actual pickup or deposit, because identical settings do not guarantee identical application quantities.
  4. Finish and interpret. Use the same approved fixation and washing or curing route. If both pastes fail only on the suspect lot, investigate fabric preparation first. If the candidate fails on both lots, investigate its formulation and application behavior.

Judge edge definition, levelness, penetration, shade and handle against buyer-defined criteria. A passing result supports only the tested fabric and process window.

How FSX Chemical Supports Fabric-Based Grade Matching

FSX Chemical supplies sodium alginate, CMC, CMS, digital printing paste and related textile printing thickener routes for printing mills, formulators, importers and distributors.

Fabric-based grade matching begins by identifying the fibre, construction, printing route and final textile requirement before selecting a candidate commercial grade.

Buyers can provide

  • Fabric composition, weight and construction
  • Representative fabric sample
  • Hệ thống thuốc nhuộm, bột màu hoặc mực in
  • Printing or pretreatment equipment
  • Current thickener TDS or sample
  • Current dosage and preparation method
  • Viscosity value and complete test method
  • Printed-fabric photographs or samples
  • Main definition, penetration, stability or handle problem
  • Estimated quantity, packaging and destination

Technical review may include

  • Identification of a suitable thickener family
  • Review of the current product specification
  • Alignment of viscosity and preparation methods
  • Recommendation of a candidate commercial grade
  • Provision of relevant TDS and SDS information
  • Representative sample support
  • Guidance for side-by-side fabric testing
  • Review of laboratory and production-trial results
  • Batch documentation for the confirmed commercial grade

Buyers can submit their fabric and current product through Mẫu hóa chất FSX và việc so sánh .

A recommended product remains a candidate for controlled evaluation. Final approval depends on the customer’s fabric, complete formulation, equipment, fixation process and finished-textile requirements📧 Email: Service@fsxchemical.com

Liên hệ nhanh

Gửi yêu cầu của bạn

hoặc

Mẫu thử miễn phí · Trả lời trong vòng 24 giờ

Thắc mắc về sản phẩm & Hỗ trợ

Gửi yêu cầu về sản phẩm của bạn

Vui lòng cung cấp tên sản phẩm, ứng dụng, số lượng, điểm đến và bất kỳ tài liệu kỹ thuật (TDS), hình ảnh mẫu hoặc tài liệu nào mà quý khách đã có. FSX Chemical sẽ xem xét thông tin này và đề xuất bước tiếp theo liên quan đến báo giá, đối chiếu mẫu hoặc lựa chọn sản phẩm.

Thông tin sản phẩm Tên sản phẩm, cấp loại, mẫu mã, ảnh nhãn mác hoặc mã tham chiếu của nhà cung cấp.
Các tài liệu có sẵn TDS, SDS, COA, ảnh mẫu, danh mục sản phẩm hoặc dữ liệu thử nghiệm.
Chi tiết đơn hàng Số lượng dự kiến, hình thức đóng gói, nước nhập khẩu, cảng hoặc điều kiện thương mại.
Yêu cầu hoặc Vấn đề Quy trình in trên vải, yêu cầu về công thức, vấn đề hiện tại hoặc chỉ tiêu hiệu suất.