Reliable textile printing batch control requires more than checking a Certificate of Analysis or one viscosity value. A strong testing program connects raw-material identity, preparation, rheology, filtration, complete-paste stability, printing behavior, post-treatment and batch-to-batch traceability before a batch is released for routine use.

Textile printing quality depends on a chain of chemical and process variables. A batch can meet a basic laboratory specification and still create problems during pumping, screen passage, fabric transfer, fixation, washing or curing.

This is why printing mills, formulators and textile chemical suppliers need a testing system that goes beyond a short COA checklist.

The most useful approach is to test at several levels: the incoming thickener or printing chemical, the prepared stock solution or paste, the complete production formulation, the actual printing application and the finished textile.

This guide lists the essential testing parameters for textile printing batches and explains which tests are routine QC measurements, which are application checks and which are especially important when qualifying a new supplier or first commercial batch.

What Does Textile Printing Batch Testing Mean?

Textile printing batch testing is the process of confirming that a specific batch of chemical or prepared printing paste remains suitable for its intended production process.

The objective is not only to confirm that the material matches a written specification. It is also to reduce the risk that a technically acceptable laboratory number hides a problem that becomes visible only during printing.

A useful batch-testing system should answer three questions

  1. Is this the correct product and batch?
  2. Does it meet the relevant laboratory requirements?
  3. Does it remain suitable for the actual printing process?

The importance of each test depends on the chemistry and application. Sodium alginate, CMC, CMS, pigment thickener and digital pretreatment should not all use an identical QC panel.

The Four Levels of Batch Testing

A strong testing program separates measurements according to where the material is in the production process.

Testing LevelWhat Is TestedMain Purpose
Level 1Incoming raw or commercial chemicalIdentity and basic batch conformity
Level 2Prepared stock solution or stock pasteHydration, viscosity, filtration and stability
Level 3Complete printing formulationCompatibility, rheology and holding stability
Level 4Printed and post-treated fabricApplication release and finished-textile quality

Not every production batch requires every possible test. Routine QC should focus on parameters that have proven useful for controlling the process, while new suppliers, new grades and problem batches should receive a broader evaluation.

1. Product Identity and Batch Traceability

Before any laboratory measurement, confirm that the material being tested is the intended commercial product.

Record

  • Manufacturer
  • Commercial product name or grade
  • Batch or lot number
  • Production or relevant reference date
  • Package identification
  • Purchase order or receiving reference

A technically excellent test result has little value if the sample cannot be connected to the actual production batch.

Traceability is particularly important when comparing retained samples, investigating complaints or verifying the first commercial shipment from a new supplier.

2. Appearance

Appearance is a simple but useful incoming and preparation check.

For powders, observe

  • Color
  • Powder or granular form
  • Visible agglomeration
  • Foreign material
  • Unusual odor where relevant

For liquids or prepared pastes, observe

  • Color
  • Uniformity
  • Sự tách biệt
  • Sedimentation
  • Gel particles
  • Excessive foam

Appearance alone does not prove quality, but a visible change from the approved reference can justify further investigation before release.

3. Moisture or Solids Content

For powders, distinguish a water-specific result from loss on drying under a defined method. For liquid or formulated products, identify whether the reported value is total nonvolatile content, dry residue or a separately documented active-polymer fraction. These quantities are not interchangeable.

Changes in a method-defined water, drying-loss or nonvolatile value can help investigate dosage and viscosity differences, but do not assign the difference to active polymer without a suitable assay. USP’s public loss-on-drying definition concerns volatile material removed under specified conditions, not a selective water measurement. A dried residue can include salts and other nonvolatile ingredients.

Use the parameter only when it is meaningful for the product

A routine QC panel should not include unnecessary tests simply because they are common on another chemical.

The method and acceptance range should be linked to the commercial product specification and the way the material is used.

4. pH

pH can be a useful identity and formulation-control parameter, especially where polymer behavior or printing chemistry is sensitive to the chemical environment.

Measure under a defined condition

The concentration, sample preparation and temperature should remain consistent.

Do not use one universal pH range

The correct range depends on the product and application.

Investigate pH together with viscosity

If both shift at the same time, the result may indicate formulation, raw-material or chemical-interaction differences.

5. Viscosity Under a Defined Method

Viscosity is one of the most important batch-control parameters for textile thickeners, but it is meaningful only when the test method is controlled.

Record

  • Nồng độ sản phẩm
  • Nguồn nước
  • Quy trình chuẩn bị
  • Thời gian và tốc độ trộn
  • Thời gian bù nước
  • Nhiệt độ đo
  • Instrument
  • Trục chính, rôto hay hình học
  • Tốc độ quay
  • Thời gian đọc
  • Unit

Two batches should not be judged different from viscosity data generated using different conditions.

The most useful viscosity specification is one that has been linked to successful production performance.

6. Hydration, Dissolution and Dispersion

A thickener can meet its final viscosity specification but still create poor preparation behavior.

Observe

  • Wetting
  • Sự hình thành khối u
  • Hydration speed
  • Độ đồng nhất của dung dịch hoặc hỗn hợp sệt
  • Undissolved particles

Hydration should be evaluated using a defined preparation method. Changing mixing speed or waiting time between batches makes comparison less useful.

For powdered thickeners, preparation behavior can directly influence labor, filtration, batch correction and production repeatability.

7. Filtration and Residue

Filtration is one of the most practical tests for textile printing thickeners and pretreatment systems.

A standardized filtration method should define

  • Nồng độ mẫu
  • Thời gian bù nước
  • Sample quantity
  • Filter material
  • Opening or mesh size
  • Pressure or gravity condition
  • Method for evaluating retained residue

Residue should be investigated, not only counted

Retained material may be incompletely hydrated polymer, gel, contamination or precipitation created by another chemical.

Stock-solution filtration and complete-paste filtration can provide different diagnostic information.

8. Rheological Behavior

A single viscosity result cannot completely describe how a printing paste behaves under changing shear.

Rheology influences

  • Pumping
  • Circulation
  • Đoạn trích trên màn hình
  • Paste transfer
  • Structural recovery
  • Định nghĩa về in ấn

Multi-speed measurements under the same spindle or geometry can compare rate-dependent response when batches share one single-point reading. They do not by themselves establish timed structural recovery or thixotropy. For that question, specify preshear, shear exposure, rest or low-shear stage and reading times. Do not treat the same RPM on different geometries as the same shear rate.

Rheological testing is especially valuable during grade qualification and troubleshooting, even if it is not included in every routine release panel.

9. Complete-Formula Compatibility

A stock thickener should not be approved for a new process only because it performs well in water.

Depending on the printing system, test with

  • Reactive dyes
  • Disperse colorants
  • Pigment dispersions
  • Muối
  • Chất kiềm
  • Sổ bìa cứng
  • Chất giữ ẩm
  • Chất làm ướt
  • Chất khử bọt
  • Các loại polymer khác

Observe whether viscosity, appearance, pH, filtration or stability changes after the complete formulation is prepared.

Staged addition can locate the point at which a change appears and guide the next comparison. It does not isolate one ingredient’s chemical mechanism: additions also change concentration, final mass, pH, ionic composition and mixing history. Use appropriately matched controls, record temperature and paste age, and test the suspected cause before assigning it. The NIST discussion of factor interactions explains a general limitation of one-factor interpretation; this is a proposed printing-paste investigation, not a validated NIST or FSX application method.

10. Holding Stability

Textile printing paste may remain in a preparation tank, circulation system or production area for hours before it is fully consumed.

Các điểm kiểm tra hữu ích có thể bao gồm

  • Immediately after preparation
  • After complete hydration
  • After the normal production holding period
  • Sau khi phát hành (nếu có)

Màn hình

  • Độ nhớt
  • pH
  • Hình thức
  • Sự tách biệt
  • Bọt
  • Lọc

A batch that meets specification only immediately after preparation may still create production instability.

11. Foam and Air Entrapment

Foam can interfere with paste preparation, sampling, application and printing uniformity.

Kiểm tra

  • Foam generated during mixing
  • Foam persistence during holding
  • Air entrainment during pumping
  • Compatibility of any defoamer with the formulation

Foam problems should not automatically be corrected by changing the thickener. Mixing conditions and formulation sequence may be the primary cause.

12. Fabric Pickup or Application Uniformity

For pretreatment, coating or other controlled application processes, the amount of formulation applied to the fabric can be as important as the formulation itself.

Evaluate

  • Application quantity
  • Edge-to-center uniformity
  • Lengthwise uniformity
  • Fabric moisture before application
  • Drying consistency

This is particularly important in digital printing pretreatment, where uneven pickup can create differences in ink migration, definition and shade.

13. Screen Passage and Machine Behavior

Laboratory data should be connected to the equipment that will actually use the paste.

For screen printing, evaluate

  • Đoạn trích trên màn hình
  • Squeegee transfer
  • Pumping and circulation where relevant
  • Screen cleaning frequency
  • Paste buildup
  • Production interruptions

A batch with acceptable viscosity but poor screen passage may have different rheology, filtration or hydration behavior.

14. Print Definition

Print definition is an application parameter that links paste rheology with the final visual result.

A useful diagnostic design can include

  • Fine horizontal lines
  • Fine vertical lines
  • Small text
  • Sharp corners
  • Dots
  • Adjacent color boundaries
  • Large solid areas

Fine structures reveal spreading and transfer problems that may not be visible in a simple solid-color laboratory print.

15. Penetration and Surface Control

The correct amount of penetration depends on the fabric, printing route and desired appearance.

Excessive penetration can contribute to

  • Weak surface appearance
  • Loss of fine detail
  • Unwanted strike-through

Insufficient penetration can contribute to

  • Poor coverage through the textile structure
  • Surface-heavy appearance
  • Application-specific uniformity problems

Penetration should be evaluated together with fabric absorbency, paste rheology, dosage and machine settings.

16. Color and Shade Consistency

Thickener or pretreatment chemistry can influence how colorant remains on or moves through the textile, but final color is always a system-level result.

For a fair batch comparison, keep constant

  • Fabric lot
  • Dye, pigment or ink
  • Formula
  • Application quantity
  • Machine settings
  • Quá trình cố định hoặc đóng rắn
  • Washing or finishing

Color differences should not automatically be attributed to the thickener without checking the rest of the process.

17. Fixation or Curing Performance

A printing batch should be judged after the relevant fixation step rather than from the wet print alone.

Reactive systems

Evaluate after the standard steaming or fixation route and subsequent washing.

Disperse systems

Evaluate after the applicable thermal fixation process.

Pigment systems

Evaluate after the binder’s approved drying/film-formation conditions and any required curing, followed by the specified durability tests.

A candidate batch that looks excellent before fixation may behave differently after the full production sequence.

18. Wash-Off and Surface Cleanliness

Wash-off is especially important in printing routes where unfixed material, residual thickener or auxiliaries must be removed after fixation.

Evaluate

  • Mức độ sạch của nền
  • Residual surface material
  • Change in print definition
  • Color appearance after washing
  • Tay cầm bằng vải

The most useful comparison uses the same washing procedure for reference and candidate batches.

19. Fastness Where Relevant

Fastness testing belongs to the finished-textile stage and should be selected according to the printing system and customer requirement.

Pigment systems may require particular attention to rubbing performance, while other printing routes may require their own relevant fastness tests.

Fastness should not be attributed to the thickener alone because colorant, binder, fixation and fabric also influence the result.

20. Fabric Hand Feel

Fabric hand feel can be important when a printing formulation leaves polymer or binder on the textile surface.

This is especially relevant to pigment systems and some digital pretreatment routes.

Compare after the complete process

Do not judge handle before curing, washing or finishing if those steps are part of normal production.

An apparently strong printing result may still be unacceptable if the resulting fabric becomes too stiff for the intended end use.

21. Batch-to-Batch Comparison

One isolated result cannot show whether a supplier or formulation is consistent over time.

Trend critical parameters across multiple batches

  • Độ nhớt
  • pH
  • Moisture or solids where relevant
  • Lọc
  • Bổ sung nước
  • Application result

The goal is not zero numerical variation. The goal is variation small enough that the process remains inside the approved operating window without repeated formulation correction.

22. Retained Samples

Retained samples can be valuable when investigating future batch differences.

A retained-sample system can help

  • Compare a complaint batch with an approved batch
  • Investigate method differences
  • Verify whether a material changed during storage
  • Support supplier discussions

Retained samples should be identified with the exact batch and stored under defined conditions appropriate to the product.

COA Testing vs Application Release Testing

A Certificate of Analysis and an application release test serve different purposes.

COA

A COA normally reports selected batch-specific quality parameters against the commercial specification.

Application release

An application test asks whether the batch works acceptably in the customer’s actual formulation, fabric and printing process.

A passing COA does not automatically guarantee printing performance, and a printing trial does not replace the need for a controlled commercial specification.

Strong supplier qualification uses both in the appropriate role.

Testing Sodium Alginate Batches

Alginat natri is commonly evaluated as a thickener for conventional reactive printing.

Useful batch checks can include

  • Hình thức
  • Moisture where specified
  • pH where relevant
  • Viscosity under the agreed method
  • Bổ sung nước
  • Lọc
  • Reactive-paste compatibility
  • Định nghĩa về in ấn
  • Fixation and wash-off

HV, MV and LV labels should not replace the actual viscosity specification and test method.

Testing CMC Batches

Carboxymethyl cellulose can be supplied in multiple grades with different viscosity and substitution characteristics.

Depending on the commercial specification, evaluate

  • Hình thức
  • Độ ẩm
  • pH
  • Độ nhớt
  • Degree of substitution where specified
  • Purity-related parameters where applicable
  • Hydration or dissolution
  • Lọc
  • Complete-formula behavior

Similar viscosity and DS do not by themselves prove that two CMC batches or supplier grades will print identically.

Testing CMS Batches

FSX CMS denotes a commercial synthetic printing-thickener family. Verify the exact grade and current TDS before choosing tests; do not assume starch composition or copy CMC substitution requirements from the abbreviation.

Relevant batch checks can include

  • Hình thức
  • Độ ẩm
  • pH
  • Độ nhớt
  • Bổ sung nước
  • Lọc
  • Độ ổn định của hỗn hợp dán
  • Đoạn trích trên màn hình
  • Application performance

The test panel should reflect the specific CMS grade and printing route rather than copy a sodium alginate or CMC specification automatically.

Testing Digital Printing Paste Batches

Hỗn hợp in kỹ thuật số should be evaluated according to the reactive, disperse or pigment inkjet route.

Batch evaluation can include

  • Hình thức
  • pH
  • Viscosity where relevant
  • Dispersion or preparation behavior
  • Lọc
  • Duy trì sự ổn định
  • Pretreatment pickup
  • Drying uniformity
  • Định nghĩa về in ấn
  • Sự di chuyển của mực
  • Quá trình cố định hoặc đóng rắn
  • Final fabric result

Digital pretreatment paste should be evaluated on the fabric side rather than treated as a general additive for digital ink.

Reactive Printing Batch Checklist

For a reactive printing batch, a practical control sequence can move from stock thickener to finished fabric.

  1. Confirm thickener grade and batch.
  2. Check stock-paste viscosity and hydration.
  3. Check filtration.
  4. Prepare the complete reactive color paste.
  5. Record viscosity after chemical addition.
  6. Check holding stability.
  7. Print the approved reference fabric or production fabric.
  8. Evaluate definition and penetration.
  9. Complete fixation.
  10. Complete wash-off.
  11. Compare final color and fabric quality.

Disperse Printing Batch Checklist

Polyester disperse printing requires a different application check from reactive printing.

  1. Confirm product and batch identity.
  2. Check viscosity and preparation behavior.
  3. Check filtration and paste uniformity.
  4. Prepare the complete disperse formulation.
  5. Evaluate holding stability.
  6. Print the production-representative polyester fabric.
  7. Evaluate screen passage and transfer.
  8. Complete the thermal fixation process.
  9. Evaluate final shade and surface cleanliness.

Pigment Printing Batch Checklist

Pigment printing requires the rheology system to work together with the binder and curing system.

  1. Confirm thickener, pigment and binder identities.
  2. Check complete-paste viscosity and stability.
  3. Check compatibility and filtration.
  4. Print a diagnostic design.
  5. Evaluate transfer and definition.
  6. Complete curing under the approved conditions.
  7. Evaluate final color and fabric handle.
  8. Check relevant rubbing or other fastness requirements.

How to Build a Representative Sampling Plan

Testing is only as useful as the sample represents the batch.

Define where the sample is taken

The correct sampling point depends on whether the material is a powder, liquid, stock paste or complete production batch.

Avoid sampling only the most convenient location

Where batch uniformity is a concern, the sampling procedure should be designed to detect meaningful variation.

Use clean and identified containers

Contamination or mislabeling can invalidate an otherwise good test.

Record sampling time

This is particularly important for pastes whose viscosity or stability changes during hydration or holding.

First-Batch Testing for a New Supplier

The first commercial batch from a new supplier deserves more testing than a routine repeat order from a fully qualified source.

Compare with the approved sample

Confirm commercial grade, appearance, viscosity method, filtration and other critical properties.

Review batch documentation

The package identity and available batch-specific documentation should match the commercial product that was approved.

Run a controlled application check

Where the process is critical, verify the first shipment in the complete printing formula before unrestricted production use.

Keep the first accepted batch as a future reference where practical

This can improve future batch-to-batch comparison.

Turn a Test Result into a Hold or Release Decision

Before testing a delivery, identify the approved grade specification, method revision and intended application. Agree acceptance limits from those requirements and validated process needs; do not choose a limit after seeing the new batch result. A historical average or a supplier’s example COA is not, by itself, the buyer’s release specification.

Decision itemEvidence to retainWhen to hold and investigate
Identity and samplingGrade, lot, package or vessel locations, sampling plan and sample age.Identity is unclear, labels disagree, or the sample cannot support the batch-uniformity question. A pooled sample can mask a problem in one package.
Laboratory resultApproved method and limit source; raw reading, units, preparation and relevant instrument conditions.A critical result is outside its agreed limit, the test method differs, or the method’s suitability is unresolved.
Application statusApproved recipe, fabric, equipment, post-treatment and trial scope.The batch is being proposed for an unqualified process, or required application checks fail despite a passing COA.
Release authorizationDisposition, reviewer, date, permitted use and any restrictions under the buyer’s procedure.No authorized decision exists. A satisfactory repeat reading alone does not erase the original exception.

For an unexpected result, preserve the original data and sample identification, check preparation and instrument suitability, and document why any retest or resampling is justified. Do not repeatedly test until a pass appears or average an unexplained failing result into compliance. Keep the material identified and controlled while disposition is pending.

This is a suggested manufacturing-QC workflow, not a claim that FSX holds a particular certification. Viscosity limits also require a valid method; Brookfield’s measurement guidance explains why instrument settings matter. Use the viscosity-drift investigation when that result is the exception.

Building a Practical Batch Release System

A strong QC system does not need to run every possible test on every production batch.

Instead, divide tests by purpose.

Test CategoryTypical Purpose
Routine ReleaseIdentity and critical batch-control parameters
Periodic VerificationBroader performance and method checks
New Supplier / New GradeFull technical and application qualification
Complaint InvestigationReference comparison and root-cause analysis
Production ChangeConfirm suitability after formula, fabric or machine changes

The release panel should focus on parameters proven to predict acceptable production performance.

Common Batch-Testing Mistakes

Testing only viscosity

Viscosity is important, but filtration, hydration, rheology and compatibility may explain printing differences that viscosity does not.

So sánh các phương pháp thử nghiệm khác nhau

Concentration, temperature, spindle and speed must be aligned before supplier values are compared.

Approving from the COA alone

A COA reports selected batch results against the stated specification; it does not independently establish the customer’s complete printing performance.

Changing several variables during a trial

Changing thickener, dosage, dye, fabric and machine settings at the same time prevents useful diagnosis.

Skipping post-treatment

Wet-print appearance does not prove final fixation, wash-off, fastness or handle.

Using an unrepresentative fabric

Application testing should use the actual or technically representative production fabric whenever possible.

Ignoring the first bulk batch

A sample trial should be connected with the commercial material through first-shipment verification.

How FSX Chemical Supports Batch and Grade Evaluation

FSX Chemical cung cấp các quy trình sản xuất chất làm đặc dùng trong in ấn dệt may, bao gồm alginat natri , CMC , CMS và hỗn hợp in kỹ thuật số .

Customers evaluating a new grade can begin with either their current commercial product or a clearly defined printing-process requirement.

Thông qua Mẫu và việc kết hợp , the current TDS, batch data, physical sample, viscosity method and printing conditions can be used to select a technically relevant candidate for controlled evaluation.

Các thông tin hữu ích bao gồm

  • Hiện nay, các sản phẩm đạt tiêu chuẩn nhà sản xuất và tiêu chuẩn thương mại
  • TDS hoặc COA gần đây
  • Mẫu tham chiếu vật lý
  • Độ nhớt và phương pháp thử nghiệm toàn diện
  • Liều lượng hiện tại
  • Printing formula
  • Vải
  • Reactive, disperse, pigment or digital route
  • Printing equipment
  • Fixation, curing or washing process
  • Current QC problem or target improvement

Final suitability should be confirmed under the customer’s actual formulation and production conditions rather than from laboratory specification data alone.

Các câu hỏi thường gặp

What are the most important testing parameters for a textile printing batch?

Important parameters can include product identity, appearance, viscosity, pH, moisture or solids where relevant, hydration, filtration, rheology, complete-formula stability and finished-fabric performance.

Is viscosity enough to release a textile thickener batch?

Not always. The required release panel depends on the product and process. Filtration, hydration, pH or other product-specific parameters may also be important.

Why must the viscosity test method be standardized?

Concentration, preparation, hydration time, temperature, instrument, spindle and rotational speed can all change the reported result.

Should every batch receive a full printing trial?

Not necessarily. A qualified routine process may use a smaller release panel, while new suppliers, new grades, first commercial batches and problem batches usually justify broader application testing.

What is the difference between a COA and internal batch testing?

A COA reports selected supplier batch results against the commercial specification. Internal batch testing verifies the parameters that the printing mill considers important for its own process and application.

Why is filtration important in textile printing?

Filtration can reveal incomplete hydration, gels, contamination or formulation incompatibility that may later affect screens, pumps or pretreatment equipment.

Why should the complete printing paste be tested?

Dyes, pigments, salts, alkalis, binders and other auxiliaries can change viscosity, rheology, filtration and stability after the stock thickener is prepared.

What should be checked on the finished fabric?

Depending on the printing route, evaluate print definition, penetration, color, fixation, wash-off, fastness and fabric handle after the normal post-treatment.

How should the first batch from a new supplier be tested?

Compare the first commercial batch with the approved sample, verify critical laboratory parameters and batch identity, and conduct a controlled application check where the process risk justifies it.

Should batch-to-batch variation be zero?

Zero numerical variation is not a practical requirement. The important goal is to keep critical properties within an approved range that maintains stable production and finished-textile quality.

Can the same QC panel be used for sodium alginate, CMC and CMS?

Some parameters may overlap, but the full panel should be product-specific. CMC may require substitution-related checks, while sodium alginate, CMS and digital pretreatment have different application priorities.

Can FSX Chemical help compare a current batch or supplier grade?

Customers can provide the current TDS, COA or physical sample together with the viscosity method and printing process so that a technically relevant candidate can be evaluated under comparable conditions.

Need to Build a Better Textile Printing Batch Test?

Send FSX Chemical the TDS, COA or physical sample of the thickener or printing paste you currently use together with your laboratory test methods and production process.

If your current issue is batch-to-batch viscosity variation, high filtration residue, unstable paste, poor screen passage, inconsistent definition or a difference between sample and bulk material, include these details with the inquiry.

A relevant sodium alginate, CMC, CMS, compound thickener or digital printing paste route can then be selected for controlled technical comparison where appropriate📧 Email: Service@fsxchemical.com

Request Batch & Grade Matching | Send Your Current TDS, COA or Sample | Yêu cầu báo giá trực tiếp từ nhà máy

Liên hệ nhanh

Gửi yêu cầu của bạn

hoặc

Mẫu thử miễn phí · Trả lời trong vòng 24 giờ

Thắc mắc về sản phẩm & Hỗ trợ

Gửi yêu cầu về sản phẩm của bạn

Vui lòng cung cấp tên sản phẩm, ứng dụng, số lượng, điểm đến và bất kỳ tài liệu kỹ thuật (TDS), hình ảnh mẫu hoặc tài liệu nào mà quý khách đã có. FSX Chemical sẽ xem xét thông tin này và đề xuất bước tiếp theo liên quan đến báo giá, đối chiếu mẫu hoặc lựa chọn sản phẩm.

Thông tin sản phẩm Tên sản phẩm, cấp loại, mẫu mã, ảnh nhãn mác hoặc mã tham chiếu của nhà cung cấp.
Các tài liệu có sẵn TDS, SDS, COA, ảnh mẫu, danh mục sản phẩm hoặc dữ liệu thử nghiệm.
Chi tiết đơn hàng Số lượng dự kiến, hình thức đóng gói, nước nhập khẩu, cảng hoặc điều kiện thương mại.
Yêu cầu hoặc Vấn đề Quy trình in trên vải, yêu cầu về công thức, vấn đề hiện tại hoặc chỉ tiêu hiệu suất.