Chất làm đặc tổng hợp so với CMC và CMS trong in màu: Những thay đổi nào về tính lưu biến, khả năng phai màu và cảm giác khi chạm vào vải?

Synthetic acrylic thickener, CMC and CMS can create different rheology, dosage requirements, binder compatibility, residue...

Synthetic acrylic thickeners, CMC and CMS can all be evaluated in selected pigment-printing systems, but they do not create the same rheology, solids load, binder interaction or finished-fabric feel. Synthetic thickeners are commonly favored where high thickening efficiency, tailored shear thinning and low addition levels are required, while CMC and CMS can provide useful pseudoplastic flow and may be considered in selected formulations or compound-thickener systems. The correct comparison should therefore be made in the complete pigment-binder paste and on the cured fabric—not from water viscosity alone. This guide compares the three routes through rheology, binder compatibility, post-cure washability or residue behavior, fabric hand, dosage and Total Cost in Use.

Which Thickener Route Is Best for Pigment Printing?

There is no universal winner.

For many conventional pigment-printing systems, synthetic acrylic or polyacrylate thickeners are a common starting route because they can deliver strong thickening efficiency at relatively low dosage and can be designed for useful shear-thinning and recovery behavior.

CMC and CMS can still be evaluated in selected pigment systems, especially when the mill is exploring:

  • Different rheological profiles
  • Higher water retention
  • Compound-thickener systems
  • Cost optimization
  • Specific binder / pigment combinations

The correct selection sequence is:

Complete Paste Compatibility → Rheology → Screen Transfer → Curing → Fastness → Post-Cure Residue / Washability → Fabric Hand → Total Cost in Use

Do not select by viscosity, raw-material name or price per kilogram alone.

Important Comparison Boundary: Pigment Printing Is Binder-Film Printing

Pigment printing differs fundamentally from reactive printing.

Pigment particles do not chemically react with the fiber in the same way reactive dyes do.

The binder forms a film that holds pigment on the textile surface after drying and curing.

Therefore, the thickener should be evaluated as a rheology-control component inside the binder system.

This changes how “wash-off” should be interpreted.

In conventional pigment printing:

  • The binder film is intended to remain.
  • The process may not include the same intensive wash-off used after reactive printing.
  • Residual thickener, surface cleanliness and hand still matter.
  • If a post-cure wash is used, the thickener’s removability and interaction with the binder film should be checked.

Do not apply reactive-printing wash-off rules directly to pigment printing.

The Three Thickener Routes at a Glance

Tuyến đườngTypical StrengthMain Risk to Check
Synthetic acrylic / polyacrylateHigh thickening efficiency, tunable rheology, low dosage potentialElectrolyte / pH / binder sensitivity
CMCPseudoplastic flow, water retention, broad availabilityHigher dosage, binder interaction, residue / hand
CMSPseudoplastic flow, cost potential, compound-system flexibilityGrade variability, hydration, binder compatibility

These are route-level tendencies, not product guarantees.

Commercial grades can behave very differently inside each category.

Synthetic Acrylic / Polyacrylate Thickener

Synthetic acrylic thickeners are widely used in pigment-printing systems because the chemistry can be designed for:

  • High thickening efficiency
  • Low addition level
  • Strong shear thinning
  • Controlled recovery
  • Easy liquid dosing

Many grades are pH-responsive and may require correct neutralization.

Their most important technical checks are:

  • Activation pH
  • Khả năng tương thích của chất kết dính
  • Khả năng dung nạp chất điện giải
  • Duy trì sự ổn định
  • Complete-paste rheology

A synthetic grade that gives very high water viscosity can still fail in the real pigment formula if binder or pigment salts collapse the polymer structure.

CMC for Selected Pigment-Printing Systems

CMC is an anionic cellulose derivative with well-known pseudoplastic behavior.

Its performance depends strongly on:

  • Mức độ thay thế
  • Trọng lượng phân tử
  • Độ tinh khiết
  • Nồng độ
  • Salt / binder environment

CMC can be worth evaluating when the mill wants:

  • A polysaccharide-based rheology route
  • Strong water retention
  • A different low-shear / high-shear balance
  • A compound-thickener component

However, CMC should not be assumed to be a direct one-for-one substitute for a synthetic pigment-printing thickener.

It may require a different dosage and can create different:

  • Paste solids
  • Độ đàn hồi
  • Chuyển hình ảnh lên màn hình
  • Post-cure residue
  • Vải dệt tay

Grade selection should be based on the complete binder-containing formula.

CMS for Selected Pigment-Printing Systems

CMS is a carboxymethylated starch derivative with pseudoplastic rheology.

Selected CMS grades can be evaluated as:

  • Primary rheology-control components in specific pigment systems
  • Compound-thickener components
  • Cost-optimization routes

Published pigment-printing work has compared carboxymethylated starch with carboxymethyl cellulose in cotton pigment printing and found that performance depended on the formulation and binder conditions rather than polymer identity alone.

This is important because CMS should not be treated as “cheap CMC.”

Its:

  • Substitution
  • Starch structure
  • Trọng lượng phân tử
  • Độ tinh khiết
  • Bổ sung nước

can produce a distinctly different rheological profile.

Rheology Comparison: Shear Thinning, Recovery and Elasticity

All three routes can show pseudoplastic behavior, but the degree and recovery profile can differ.

Synthetic Acrylic

Often provides strong, designable shear thinning and can be formulated for rapid recovery.

CMC

Typically shows non-Newtonian pseudoplastic behavior, with flow strongly influenced by DS, molecular weight and concentration.

CMS

Also commonly shows pseudoplastic behavior, but the exact profile depends on starch source, substitution and modification route.

For screen printing, the key comparison is:

Low-Shear Body → High-Shear Flow → Recovery → Elasticity

không:

Which sample has the highest Brookfield number?

Why the Same Viscosity Does Not Mean the Same Printing Behavior

Two pastes can both measure 30,000 mPa·s under one viscometer condition and still differ in:

  • Flow through the screen
  • Squeegee pressure requirement
  • Độ thâm nhập
  • Structural recovery
  • Stringiness
  • Leveling

One-point viscosity should therefore be treated as a QC value, not a complete rheological description.

When possible, compare:

  • Multi-speed viscosity
  • Quá trình phục hồi sau khi chịu lực cắt có kiểm soát
  • Machine screenability

Khả năng tương thích với máy đóng bìa

Binder compatibility is critical in pigment printing.

Chất kết dính có thể thay đổi:

  • pH
  • Electrolyte level
  • Cân bằng chất hoạt động bề mặt
  • Total solids
  • Viscoelasticity

Chất làm đặc tổng hợp

Can be highly efficient but may be sensitive to the specific binder chemistry or ionic load.

CMC

Can respond to binder salts and ionic conditions and should be checked for viscosity drift or flocculation.

CMS

Can also interact with binder / auxiliaries and should be evaluated for delayed thickening, thinning, separation or foam.

Use the same binder and pigment package for all three comparisons.

Electrolyte and pH Sensitivity

All three routes can respond to ionic conditions, but not in the same way.

Synthetic Polyacrylate

Often sensitive to charge screening, especially in conventional highly ionic systems, although hydrophobically modified grades can show improved tolerance.

CMC

Salt tolerance depends strongly on DS, molecular weight and substitution uniformity.

CMS

Salt / alkali response depends on substitution, starch backbone and grade design.

Therefore, compare:

Water Viscosity

và:

Complete Pigment-Paste Viscosity

for every route.

Dosage and Polymer Solids

Synthetic thickeners are often attractive because relatively low addition levels can create strong viscosity.

CMC and CMS may require higher as-supplied dosage depending on grade.

Higher dosage can increase:

  • Polymer solids in the paste
  • Dry surface residue
  • Viscosity sensitivity
  • Potential impact on fabric hand

But dosage alone is not enough.

For liquid synthetic thickeners, calculate active polymer solids.

For CMC / CMS, account for moisture and active dry material.

The fair comparison is:

Required Dosage → Actual Polymer Solids → Printing Performance → Finished Hand → Cost

Screen Transfer and Print Definition

Good print definition requires:

  • Clean screen passage
  • Controlled paste deposit
  • Limited lateral spreading
  • Appropriate structural recovery

Synthetic thickener can offer a strong balance where high-shear flow and rapid recovery are required.

CMC or CMS can also provide useful definition when the grade and dosage create the right pseudoplastic profile.

Do not compare print sharpness at unmatched viscosity or unmatched paste deposit.

Penetration and Surface Color

Thickener route changes how the pigment-binder paste moves into the textile.

Too much penetration can reduce:

  • Surface color concentration
  • Độ sắc nét của cạnh

Too little penetration can create:

  • Surface-heavy deposits
  • Uneven coverage in some constructions

Compare penetration on the same:

  • Vải
  • Screen
  • Squeegee
  • Binder level

Otherwise, process variation can be mistaken for thickener behavior.

Wash-Off, Residue and Post-Cure Cleanliness

Wash-off must be interpreted carefully in pigment printing.

Conventional pigment printing is designed around a cured binder film, so the objective is not to remove the entire printed film after curing.

Instead, evaluate:

  • Loose surface residue
  • Hydrophilic thickener residue
  • Post-cure washing response if the process includes washing
  • Fabric cleanliness
  • Hand after any post-treatment

Chất làm đặc tổng hợp

Low dosage can reduce total thickener solids, but the polymer may remain partly associated with the cured binder film. “Easy wash-off” should not be assumed without testing.

CMC

CMC is water-soluble before curing, but in a pigment system some polymer can become physically trapped in the binder film or remain as surface residue. Post-cure washability must therefore be measured on the actual binder system.

CMS

CMS is also hydrophilic and can be removable in water before film formation, but final residue depends on formulation, binder cure and dosage.

Do not transfer reactive-printing wash-off assumptions directly into pigment printing.

Fabric Hand

Fabric hand is often where the thickener routes become commercially different.

Hand depends on:

  • Binder film
  • Thickener solids
  • Lớp lắng đọng dạng bột nhão
  • Quá trình làm cứng
  • Fabric construction

A lower-dose synthetic thickener can reduce added polymer solids and may help support a softer hand if binder and curing are also optimized.

CMC or CMS may require higher solids depending on the grade, which can increase the risk of a heavier or stiffer surface.

But this is not universal.

A well-optimized CMC or CMS compound system can still produce acceptable hand, while an over-bindered synthetic-thickener system can become very stiff.

The final comparison must be made after curing.

Rubbing Fastness and Curing

Rubbing fastness is primarily controlled by the pigment binder and curing process.

The thickener contributes indirectly by affecting:

  • Pigment distribution
  • Phân phối bìa hồ sơ
  • Lớp lắng đọng dạng bột nhão
  • Độ thâm nhập

Higher binder concentration can improve rubbing fastness but may also increase stiffness.

Therefore, do not select a thickener route only because it produces a deeper wet print.

So sánh:

  • Xoa khô
  • Chà ướt
  • Wash fastness where relevant
  • Vải dệt tay

after identical curing.

Duy trì sự ổn định

Compare fresh paste with held paste.

Bản ghi:

  • Độ nhớt
  • pH
  • Nhiệt độ
  • Bọt
  • Sự tách biệt
  • Gel / floc

Synthetic

Watch for pH or electrolyte-related viscosity drift.

CMC

Watch for hydration completion, salt response and delayed viscosity change.

CMS

Watch for hydration, formulation interaction and storage stability.

A paste that is stable only when fresh is not suitable for a long production holding window.

Màn hình phẳng so với màn hình xoay

The thickener route should be evaluated on the intended machine.

Màn hình phẳng

Important factors include:

  • Độ bám dính ở điều kiện ma sát thấp
  • Pause / restart behavior
  • Recovery after squeegee stroke

Máy sàng quay

Important factors include:

  • Khả năng bơm
  • Lực cắt liên tục
  • Circulation stability
  • Mid-run and end-run viscosity

A route that works in flat screen may need dosage or grade adjustment in rotary screen.

Can Synthetic Thickener Be Blended with CMC or CMS?

Yes, compound-thickener systems can be evaluated.

The purpose of blending is not simply to reduce cost.

A blend can be designed to change:

  • Low-shear body
  • Shear-thinning profile
  • Phục hồi
  • Water retention
  • Phản ứng điện giải
  • Polymer solids

Published textile-printing research has shown that mixtures of modified polyacrylic acid with small amounts of CMS can create useful rheological behavior in selected systems.

However, there is no universal synthetic/CMC or synthetic/CMS ratio.

Compound systems must be tested for:

  • Khả năng tương thích
  • Duy trì sự ổn định
  • Chuyển hình ảnh lên màn hình
  • Quá trình làm cứng
  • Tay

Practical Selection Matrix

Khu vực lựa chọnSynthetic AcrylicCMCCMS
Typical thickening efficiencyOften highTùy thuộc vào cấp lớpTùy thuộc vào cấp lớp
Shear-thinning design flexibilityCaoModerate / grade-dependentModerate / grade-dependent
pH activation requirementCommon in some gradesNormally no acrylic-style activationNormally no acrylic-style activation
Electrolyte sensitivityCó thể có ý nghĩa quan trọngDepends on DS / gradeDepends on substitution / grade
Typical dosage levelThường thấp hơnOften higherOften higher
Khả năng tương thích của chất kết dínhPhải xác minhPhải xác minhPhải xác minh
Post-cure residue / handOften benefits from low solids if optimizedDepends on dosage / binder trappingDepends on dosage / binder trapping
Compound-thickener potentialCaoPossiblePossible

This table is a route-selection aid, not a product specification.

How to Compare the Three Routes in the Laboratory

Use the same:

  • Chất màu
  • Binder
  • Fixer
  • Auxiliaries
  • Vải
  • Quá trình làm cứng

Then:

Step 1: Build Each Grade to a Useful Rheology Window

Do not force equal dosage.

Step 2: Measure Fresh Complete-Paste Viscosity

Use the same instrument and method.

Step 3: Run Multi-Speed / Recovery Comparison

Compare screen-relevant rheology.

Step 4: Hold the Paste

Check end-of-shift stability.

Step 5: Print the Same Fabric

Keep screen and squeegee conditions constant.

Step 6: Cure Identically

Sau đó, hãy so sánh:

  • K/S / màu
  • Định nghĩa về in ấn
  • Độ thâm nhập
  • Chà khô / chà ướt
  • Post-cure residue or wash response
  • Tay

For a controlled grade comparison, FSX Chemical can review current products or TDS through Mẫu và việc kết hợp.

Phê duyệt thử nghiệm sản xuất

Only the best laboratory candidates should move to production.

Bản ghi:

  • Thickener route and grade
  • Liều lượng
  • Công thức đầy đủ
  • Độ nhớt khi bắt đầu / giữa / kết thúc quá trình chạy
  • Tốc độ máy
  • Hành vi trên màn hình
  • Beginning-to-end shade
  • Curing result
  • Độ bền khi cọ xát
  • Vải dệt tay

Approve a route only if it remains stable across the intended production window.

When Does Synthetic Thickener Usually Make More Sense?

Synthetic acrylic thickener is often worth prioritizing when the mill needs:

  • High thickening efficiency
  • Low dosage
  • Tailored shear thinning
  • Fast liquid incorporation
  • Low added polymer solids

It is especially attractive when the binder / pigment system has already been optimized for synthetic rheology modifiers.

But electrolyte tolerance and pH activation must be checked.

When Can CMC Be Worth Evaluating?

CMC may be worth testing when the mill wants:

  • A polysaccharide rheology route
  • Strong water retention
  • A different screen-transfer profile
  • A compound formulation
  • An alternative supply route

Selection should focus on:

  • DS
  • Trọng lượng phân tử
  • Độ tinh khiết
  • Khả năng tương thích của chất kết dính
  • Required dosage

Do not assume one generic CMC grade represents all textile CMC products.

When Can CMS Be Worth Evaluating?

CMS may be worth evaluating when the mill wants:

  • Cost optimization
  • Compound-thickener flexibility
  • Pseudoplastic flow
  • Alternative rheology

Selection should focus on:

  • Substitution
  • Độ tinh khiết
  • Bổ sung nước
  • Khả năng tương thích của chất kết dính
  • Duy trì sự ổn định

Selected CMS grades can be technically useful, but the result is formulation-specific.

Common Comparison Mistakes

1. Comparing Equal Dosage Only

Different grades have different thickening efficiency.

2. Comparing Water Viscosity Only

Pigment and binder can change the complete paste substantially.

3. Assuming Synthetic Always Gives Softer Hand

Binder solids, dosage and curing can dominate hand.

4. Assuming CMC / CMS Must Wash Out Completely

In pigment printing, binder film can retain or trap part of the hydrophilic thickener.

5. Treating CMS as Cheap CMC

The polymer backbone and rheology are different.

6. Using Reactive-Printing Wash-Off Logic

Pigment printing is binder-film printing and must be evaluated differently.

7. Selecting by Price per Kilogram

Working dosage and finished-fabric result determine real cost.

Bảng khắc phục sự cố

Observed DifferenceCác biến cần kiểm tra trước tiênĐừng vội kết luận
Synthetic paste is thinner after binderpH, electrolytes, binder compatibilitySynthetic route is unsuitable
CMC needs higher dosageGrade, DS, molecular weight, target rheologyHigher dosage means worse overall cost
CMS gives different screen feelShear thinning, recovery, hydrationSame viscosity means same rheology
Synthetic gives softer handPolymer solids, binder film, paste depositAll synthetic grades will do the same
CMC/CMS leaves more residueDosage, curing, post-cure wash, binder trappingPolysaccharide route is automatically poor
Rubbing fastness differsBinder distribution, curing, paste depositThickener chemistry alone controls fastness
Lab result good, rotary run driftsContinuous shear, holding time, temperatureLab viscosity predicts long-run stability
Compound system outperforms single polymerBlend rheology and compatibilityOne polymer must always be best

Tổng chi phí trong quá trình sử dụng

Compare the three routes using:

Total Cost in Use = Thickener Cost + Dosage + Preparation + Binder / Formula Adjustment + Machine Efficiency + Curing + Rework + Quality Loss

A synthetic thickener can have a higher price per kilogram but lower working dosage.

CMC or CMS can have a lower raw-material cost but require more solids or different preparation.

A compound system may reduce cost only if it also maintains:

  • Độ ổn định của hỗn hợp dán
  • Screen performance
  • Fastness
  • Tay

Compare cost per acceptable printed meter—not cost per kilogram of thickener.

Bạn nên cung cấp những thông tin nào cho nhà cung cấp chất làm đặc?

For a useful synthetic-vs-CMC-vs-CMS comparison, provide:

  • Current thickener product / TDS
  • Liều lượng hiện tại
  • Độ nhớt và phương pháp thử nghiệm toàn diện
  • Dung dịch phân tán sắc tố
  • Binder and dosage
  • Thiết bị cố định / thiết bị phụ trợ
  • Final paste pH
  • Vải
  • Rây phẳng hoặc rây quay
  • Screen mesh / engraving
  • Thời gian giữ
  • Curing condition
  • Main target: rheology, hand, residue, fastness or cost

FSX Chemical có thể sử dụng thông tin này thông qua Mẫu và việc kết hợp to identify whether a synthetic, CMC, CMS or compound route deserves the next controlled trial.

Đánh giá CMC, CMS và Các ứng dụng của chất làm đặc trong in ấn dệt may for route-specific product information.

How Should a Mill Compare Synthetic Thickener, CMC and CMS for Pigment Printing?

A practical sequence is:

Match Complete-Paste Rheology → Compare Dosage & Solids → Hold → Screen Print → Cure → Check Fastness → Check Residue / Wash Response → Check Hand → Calculate Total Cost in Use

Các nguyên tắc chính là:

  1. Synthetic thickener, CMC and CMS should not be compared at equal dosage alone.
  2. Same viscosity does not mean same shear thinning, recovery or print definition.
  3. Binder compatibility must be checked for all three routes.
  4. Wash-off in pigment printing means post-cure residue and cleanliness, not reactive-style removal of the printed film.
  5. Fabric hand depends on binder film, thickener solids, paste deposit and curing together.
  6. The best route is the one that delivers the required production window at the lowest Total Cost in Use.

Các câu hỏi thường gặp

1. Is synthetic thickener better than CMC or CMS for pigment printing?

Not universally. Synthetic acrylic thickeners are a common starting route because of high efficiency and tailored rheology, while selected CMC, CMS or compound systems can be useful in specific formulations.

2. Why do synthetic thickeners often use lower dosage?

Many acrylic/polyacrylate products are designed for high thickening efficiency, but actual dosage still depends on solids, pH, electrolyte load and formula.

3. Can CMC be used in pigment printing?

Selected CMC grades can be evaluated, especially where a polysaccharide rheology route or compound system is desired. Binder compatibility and dosage must be verified.

4. Can CMS be used in pigment printing?

Yes, selected CMS grades have been studied in pigment-printing systems, but the result depends on grade, binder, pigment and formulation.

5. Which route gives the best shear thinning?

It depends on the commercial grade. Synthetic acrylic systems often offer more rheology-design flexibility, but CMC and CMS are also pseudoplastic and can provide useful screen behavior.

6. Which route gives the softest fabric hand?

There is no universal answer. Lower polymer solids can help, but binder dosage, curing and paste deposit often dominate final hand.

7. Does CMC wash off better than synthetic thickener?

Not automatically in pigment printing. CMC is water-soluble before curing, but part of it can be retained in or under the cured binder film. Test the real post-cure process.

8. Does CMS leave more residue?

Residue depends on grade, dosage, hydration, binder film and post-treatment. Do not assume residue from polymer family alone.

9. Can synthetic thickener be blended with CMC or CMS?

Yes. Compound systems can be evaluated to tune rheology, solids, water retention or cost, but the blend must be tested for compatibility and curing performance.

10. Should the three routes be compared at the same viscosity?

Compare them inside the same useful complete-paste rheology window, then evaluate screen transfer, definition, curing, hand and cost.

11. Which route is cheapest?

Compare Total Cost in Use. A lower raw-material price can be offset by higher dosage, longer preparation, lower machine efficiency or poorer hand.

12. What should I send FSX Chemical for comparison testing?

Send your current thickener or TDS, dosage, viscosity method, pigment, binder, fabric, machine route, curing conditions and main target so the most relevant route can be selected for trial.

Compare Synthetic Thickener, CMC and CMS Under the Same Pigment Formula

If your mill is deciding between synthetic acrylic thickener, CMC, CMS or a compound-thickener route, FSX Chemical can help structure a controlled comparison based on complete-paste rheology and finished-fabric performance rather than water viscosity alone.

Để nhận được bài đánh giá kỹ thuật hữu ích, vui lòng gửi:

  • Your current thickener sample, TDS or COA
  • Liều lượng hiện tại
  • Độ nhớt và phương pháp thử nghiệm toàn diện
  • Dung dịch phân tán sắc tố
  • Binder and fixer system
  • Final paste pH
  • Fabric and screen route
  • Thời gian giữ
  • Curing condition
  • Current rheology, wash/residue, hand or cost target

Bắt đầu bằng Mẫu và việc kết hợp để tiến hành một thử nghiệm có đối chứng so sánh giữa nhóm đối chứng và nhóm thí nghiệm.

Đánh giá CMC, CMS và Các ứng dụng của chất làm đặc trong in ấn dệt may for route-specific selection.

Bạn cũng có thể Yêu cầu báo giá trực tiếp từ nhà máy after the suitable thickener route and working dosage are confirmed or Liên hệ với FSX Chemical để thảo luận về các vấn đề kỹ thuật📧 Email: Service@fsxchemical.com

The best pigment-printing thickener is not determined by polymer family alone. It is the route that gives the required rheology, binder compatibility, cured fastness, acceptable residue and hand, and the lowest practical Total Cost in Use.

Liên hệ nhanh

Gửi yêu cầu của bạn

hoặc

Mẫu thử miễn phí · Trả lời trong vòng 24 giờ

Thắc mắc về sản phẩm & Hỗ trợ

Gửi yêu cầu về sản phẩm của bạn

Vui lòng cung cấp tên sản phẩm, ứng dụng, số lượng, điểm đến và bất kỳ tài liệu kỹ thuật (TDS), hình ảnh mẫu hoặc tài liệu nào mà quý khách đã có. FSX Chemical sẽ xem xét thông tin này và đề xuất bước tiếp theo liên quan đến báo giá, đối chiếu mẫu hoặc lựa chọn sản phẩm.

Thông tin sản phẩm Tên sản phẩm, cấp loại, mẫu mã, ảnh nhãn mác hoặc mã tham chiếu của nhà cung cấp.
Các tài liệu có sẵn TDS, SDS, COA, ảnh mẫu, danh mục sản phẩm hoặc dữ liệu thử nghiệm.
Chi tiết đơn hàng Số lượng dự kiến, hình thức đóng gói, nước nhập khẩu, cảng hoặc điều kiện thương mại.
Yêu cầu hoặc Vấn đề Quy trình in trên vải, yêu cầu về công thức, vấn đề hiện tại hoặc chỉ tiêu hiệu suất.