Khám phá các giải pháp hóa chất dệt may mới cho in phun kỹ thuật số
A new digital textile printing chemical should be qualified against a specific ink, fabric and application route before production use. Start with a controlled comparison against the approved pretreatment, then check finished-print quality, operating stability and cost per accepted output. Fabric-side pretreatment paste is separate from printhead ink; a promising laboratory print alone does not approve a new formulation for routine production.
Digital inkjet printing has changed the way textile manufacturers approach short runs, complex designs, color variation and production flexibility. However, advances in printers and inks do not remove the importance of textile chemistry.
An inkjet printer can place extremely small droplets with high precision, but the final result still depends on what happens when those droplets meet the fabric. If the textile surface absorbs liquid too quickly, allows excessive lateral migration or interacts poorly with the ink chemistry, the apparent precision of the printer can be lost.
This is where textile pretreatment chemistry becomes important. Digital printing paste, surface-control auxiliaries and application-specific thickener systems can help prepare the fabric before printing and create a more controlled environment for the ink.
The most useful new chemical solutions are not necessarily completely new polymer families. Innovation can also come from better matching of existing chemistries to reactive, disperse and pigment inkjet systems, improved filtration, more controlled rheology, better fabric-surface management and more systematic grade matching.
This article explores these solution directions and explains how textile printers can evaluate them without confusing fabric pretreatment chemistry with the tightly controlled formulation of digital ink itself.
Why Digital Inkjet Printing Needs Different Chemistry
Conventional screen printing and digital inkjet printing both place color on textile, but the physical delivery systems are fundamentally different.
In conventional printing, the color paste itself contains a substantial rheology-control system and is mechanically transferred through a screen.
In digital inkjet printing, the ink must remain within a tightly controlled fluid window suitable for the ink-delivery system and printhead. The fabric-side chemistry therefore performs an important part of the surface-control function.
The digital process separates two functions
The ink provides the colorant system and must remain suitable for jetting. The pretreatment prepares the textile surface and helps control how the jetted liquid behaves after impact.
This separation is one reason digital textile printing requires application-specific chemical development rather than simply adapting a traditional screen-printing paste.
Digital Ink Is Only One Part of the System
When a digital print appears weak, blurred or uneven, it is easy to assume that the ink is the only variable that needs to change.
In reality, final print performance can be influenced by several connected factors:
- Ink chemistry
- Fabric fibre composition
- Fabric preparation
- Pretreatment chemistry
- Pretreatment pickup
- Drying conditions
- Printer settings
- Ink laydown
- Quá trình cố định hoặc đóng rắn
- Washing where required
A new chemical solution should therefore be evaluated as part of the total printing system rather than expected to solve every defect independently.
Where Pretreatment Chemistry Works
Digital printing paste and related textile pretreatment chemicals generally act on the fabric before inkjet printing.
A simplified process can be represented as:
Fabric → Pretreatment → Drying → Digital Printing → Fixation or Curing → Washing or Finishing → Finished Textile
Xử lý sơ bộ
The chemical system is applied to the textile using the appropriate coating, padding, spraying or other controlled process.
Sấy khô
The treated fabric is dried to a condition suitable for printing. Residual moisture should remain sufficiently controlled for a fair process comparison.
Digital printing
The ink is jetted onto the prepared textile surface.
Quá trình cố định hoặc đóng rắn
The required treatment depends on reactive, disperse or pigment chemistry.
Post-treatment
Washing, finishing or other steps are completed according to the printing route before final fabric evaluation.
Solution 1: Process-Specific Pretreatment
One of the most important developments in digital textile chemistry is the move away from one universal printing paste toward process-specific pretreatment.
Reactive, disperse and pigment inks use different colorant chemistry and fixation mechanisms. Their pretreatment systems should therefore be evaluated independently.
| Ink Route | Typical Fabric Direction | Pretreatment Focus | Final Evaluation |
|---|---|---|---|
| Phản ứng | Cotton, viscose and suitable cellulosic or natural-fibre systems | Migration control, moisture, definition and fixation compatibility | After steaming and washing |
| Phân tán | Polyester and suitable blends | Surface uniformity, filtration and thermal-process compatibility | After thermal fixation and required cleaning |
| Chất màu | Various fabrics depending on the ink and binder system | Migration control, binder interaction and surface behavior | After curing and fastness evaluation |
Selecting by ink chemistry first is more reliable than selecting a digital printing paste only by viscosity.
Reactive Inkjet Chemistry
Reactive digital textile printing is commonly evaluated on suitable cellulosic fabrics such as cotton and viscose.
The pretreatment needs to work together with the reactive ink and the subsequent fixation and washing process.
Important technical targets include
- Uniform pretreatment application
- Controlled ink migration
- Fine-line definition
- Stable shade development
- Compatibility with fixation chemistry
- Practical wash-off
- Acceptable final fabric handle
For reactive inkjet pretreatment, DG-20 is the current FSX product name formerly described as DP-R. Confirm its current TDS and the intended fabric-side application before trial.
A candidate pretreatment should be judged after the complete printing, fixation and washing sequence rather than from the wet print alone.
Disperse Inkjet Chemistry
Disperse digital printing is primarily associated with polyester and suitable polyester-blend fabrics.
The chemical requirements differ from reactive printing because the fiber, ink system and thermal fixation route are different.
Important evaluation areas include
- Độ đồng đều trong quá trình tiền xử lý
- Dispersion stability
- Lọc
- Surface cleanliness
- Fine-detail definition
- Độ đồng đều của vùng rắn
- Compatibility with thermal fixation
For direct disperse printing onto polyester, request an FSX candidate documented for that application and confirm the current grade and product form. Sublimation transfer printing onto paper is a different route; it does not establish a need for the same fabric pretreatment.
A product used successfully for reactive printing should not automatically be transferred to a polyester disperse process.
Pigment Inkjet Chemistry
Pigment digital printing presents another chemical challenge because pigment colorants generally depend on binder-film formation and curing rather than dye-fibre reaction alone.
The chemistry must balance
- Sự di chuyển của mực
- Khả năng tương thích của chất kết dính
- Color appearance
- Định nghĩa về in ấn
- Quá trình làm cứng
- Hiệu suất chà xát
- Cảm giác khi chạm vào vải
FSX Chemical uses DP-P as the starting route for pigment digital printing trials.
More pretreatment or binder is not automatically better. A system that produces strong surface color but unacceptable stiffness may require further formulation optimization.
Solution 2: Rheology-Controlled Pretreatment
Digital pretreatment chemistry needs more than a target viscosity. The way the formulation flows during preparation and application can influence how uniformly it reaches the fabric.
Standing viscosity
A routine viscosity measurement can help monitor batch preparation, but the test method must be clearly defined.
Application rheology
Different pretreatment machines generate different shear conditions. Two products with similar standing viscosity may therefore produce different pickup and surface distribution.
Structural stability
The formulation should remain practical during storage and application without excessive separation, gel formation or uncontrolled viscosity drift.
New-generation pretreatment development increasingly benefits from viewing viscosity and rheology as connected but different properties.
Solution 3: Filtration and Low-Residue Performance
Digital printing paste is normally used on the fabric side rather than being jetted through the printhead, but filtration and residue still matter.
Pretreatment systems can pass through mixers, filters, pumps, coating equipment, padding systems or spraying equipment before they reach the fabric.
Potential sources of residue include
- Incomplete polymer hydration
- Gel particles
- Sự không tương thích hóa học
- Foreign contamination
- Precipitated material
Use controlled filtration testing
Define the test purpose first. A common-SOP challenge uses the current plant preparation and filter procedure to check process fit. For application qualification, prepare each grade by its documented procedure and record dispersion, hydration or activation where applicable before comparing the ready-to-use formulations. Keep filter material and rating, effective area, sample-mass basis, temperature, driving pressure or gravity head, test duration and rinse procedure defined. Report throughput or blockage as well as retained material; a lower residue mass alone does not establish usable filtration capacity. For CMC specifically, Nouryon’s preparation guidance distinguishes dispersion from hydration and describes grade-dependent dissolution; it is not a preparation specification for every FSX pretreatment.
Inspect the retained material
Record how residue is collected, rinsed, dried or otherwise assessed. Filter-retained mass is not automatically insoluble contamination or polymer purity: retained material may include incompletely prepared polymer, incompatibility products and trapped liquid or dissolved components. Use preparation controls and appropriate analytical identification before assigning a cause; a staged addition test is a diagnostic comparison, not proof of one chemical mechanism.
Solution 4: Moisture and Fabric-Surface Control
Digital printing occurs at the interface between a precisely delivered liquid droplet and an irregular textile surface.
Fabric absorbency, capillary movement and residual moisture can strongly influence the visible print boundary.
Pretreatment can be evaluated for its ability to support
- More uniform fabric surface response
- Controlled liquid penetration
- Reduced unwanted lateral migration
- Consistent ink absorption
- Better definition of small printed elements
The objective is not to prevent all penetration. The correct amount depends on the fabric construction, visual requirement and printing system.
Solution 5: Binder-Compatible Pigment Systems
Pigment digital printing creates a particularly demanding balance between visual quality and finished-fabric properties.
Pretreatment chemistry should be evaluated together with the actual pigment ink and binder rather than as an isolated thickener system.
Check interaction with
- Pigment ink
- Hóa học chất kết dính
- Crosslinking system where applicable
- Fabric finish
- Curing temperature and time
Evaluate the final textile for
- Định nghĩa về in ấn
- Color uniformity
- Dry rubbing performance
- Wet rubbing performance where required
- Cảm giác khi chạm vào vải
Optimizing only color depth can produce an unbalanced pigment system.
Solution 6: Application-Specific Compound Thickeners
One polymer does not always provide the preferred combination of viscosity, rheology, surface control, stability and commercial cost.
Application-specific compound systems can combine different materials to create a more balanced pretreatment profile.
A compound system may be developed around
- Base viscosity
- Shear response
- Surface sizing
- Moisture management
- Lọc
- Duy trì sự ổn định
- Compatibility with other auxiliaries
More components also create more formulation variables, so compound systems should be developed through controlled experiments rather than uncontrolled blending.
Solution 7: Data-Based Grade Matching
One of the most practical advances in textile chemical sourcing is moving away from product-name matching toward data-based grade matching.
A buyer already using a successful digital printing paste can use that product as the technical benchmark for a new supplier evaluation.
Useful reference information includes
- Hiện nay, các sản phẩm đạt tiêu chuẩn nhà sản xuất và tiêu chuẩn thương mại
- TDS
- Recent COA where available
- Physical sample
- Viscosity and test method
- Liều lượng hiện tại
- pH
- Ink system
- Vải
- Pretreatment equipment
- Drying and fixation process
- Current printing problem
This allows a supplier to select a technically relevant candidate instead of recommending a generic digital printing thickener.
Controlling Ink Migration and Bleeding
Ink migration is one of the most visible problems in digital textile printing.
After the droplet reaches the fabric, liquid can travel vertically into the textile structure and laterally along yarn and fibre pathways.
Excessive lateral movement can appear as
- Blurred edges
- Color bleeding
- Loss of fine lines
- Reduced small-text clarity
- Poor separation between adjacent colors
Pretreatment can help control this movement, but the final result also depends on fabric absorbency, ink laydown, drying and fixation.
Increasing pretreatment concentration without controlled testing is therefore not a universal solution.
Improving Fine-Line Definition
High-resolution digital equipment should be evaluated using a test image capable of revealing chemical differences.
Include
- Fine horizontal lines
- Fine vertical lines
- Small text
- Sharp corners
- Fine dots
- Multi-color boundaries
- Gradients
- Dark solid areas
Fine structures are useful for detecting uncontrolled spreading, while large solid areas reveal transfer, uniformity and surface differences.
Evaluation should be repeated after the complete fixation and post-treatment process.
Understanding Color Yield
Pretreatment chemistry can influence how color develops on the fabric, but the phrase “better color yield” should be used carefully.
Final color depends on the complete printing system.
Important variables include
- Ink formulation
- Ink laydown
- Fabric preparation
- Pretreatment pickup
- Surface absorption
- Sấy khô
- Sự cố định
- Washing or curing
A fair comparison should use the same fabric, printer, ink and post-treatment for the current and candidate pretreatment systems.
Pretreatment Pickup and Drying
Even a well-designed chemical system can produce inconsistent results if pretreatment pickup varies across the fabric.
Monitor application quantity
Too little pretreatment may provide insufficient surface control, while excessive application may increase solids, drying demand or fabric stiffness.
Control application uniformity
Edge-to-center and lengthwise variation can create visible shade and definition differences.
Control drying
Fabric entering the printer at different moisture conditions may respond differently even when the chemical recipe is unchanged.
Pretreatment chemistry and pretreatment application therefore need to be optimized together.
Duy trì sự ổn định
A digital pretreatment system may remain in a preparation tank or application system for hours before it is fully consumed.
Useful stability checkpoints can include
- Immediately after preparation
- After full hydration or equilibration
- After normal production holding
- After circulation where applicable
Màn hình
- Độ nhớt
- pH
- Hình thức
- Sự tách biệt
- Bọt
- Lọc
Stable pretreatment can reduce the need for repeated correction during production and make digital output more predictable.
Fabric-Specific Selection
Digital chemical selection starts with the ink chemistry and delivery route, followed by the fibre, fabric construction and exact application point. A printer model or fabric name alone does not establish chemical compatibility.
Bông và viscose
Cellulosic textiles can absorb aqueous ink rapidly, making controlled reactive pretreatment particularly important.
Polyester
For polyester, distinguish direct disperse printing onto the textile from sublimation transfer through printed paper. Evaluate fabric pretreatment for the direct route where specified; do not transfer that requirement automatically to a paper-transfer process.
Blended fabrics
Blends can respond more complexly because the component fibres may differ in liquid absorption, colorant affinity and surface behavior.
Fabric construction matters too
Knitted and woven fabrics, different weights, yarn structures, densities and finishing histories can all influence pretreatment pickup and ink movement.
Keep Fabric Pretreatment Separate from Printhead Ink
One of the most important distinctions in digital textile chemistry is the difference between pretreatment paste and digital ink.
Digital ink is formulated for a tightly controlled jetting system. Independently adding a fabric-side thickener or pretreatment changes the qualified formulation and can affect jetting, stability or the ink-delivery system. Use only fluids approved for the relevant printer and ink route.
The FSX fabric-pretreatment route discussed here is evaluated on the textile, not as an ink-tank additive. Specialised jettable pretreatment inks are a separate equipment-qualified product category; their existence does not mean a conventional pretreatment paste can be jetted or mixed into colour ink.
The preferred route is
Select pretreatment → Apply to fabric → Dry → Print with approved ink → Fix or cure → Evaluate final textile
Ink formulation changes should be handled according to the requirements of the ink and printing-equipment system rather than by adding textile thickener independently.
Resource-Efficient Digital Textile Printing
Digital printing is often discussed in sustainability conversations, but no printing route should automatically be described as environmentally superior without examining the complete process.
Pretreatment chemistry can contribute to resource efficiency when it helps the process achieve acceptable quality with fewer avoidable failures and corrections.
Useful metrics include
- Pretreatment dosage
- Unused preparation
- Filtration residue
- Failed or reprinted fabric
- Drying demand
- Fixation or curing conditions
- Wash-off requirements
- Tính nhất quán của lô
Sustainability should therefore be evaluated through measurable process performance rather than a broad “eco-friendly” label.
How to Compare New and Existing Chemical Systems
A new pretreatment system should be compared against the product already approved in production whenever a reference is available.
| Evaluation Area | Current System | New Candidate |
|---|---|---|
| Commercial Grade | Record exact product | Record permanent candidate grade |
| Chuẩn bị | Document the current plant SOP | Label common-SOP challenge or separately documented grade-ready preparation; report changes |
| Độ nhớt | Record complete method | Use comparable conditions |
| pH | Record normal range | Compare under intended formulation |
| Lọc | Reference residue | Use identical filter method |
| Pretreatment Pickup | Current operating level | Baseline first, then optimize |
| Ink | Same ink system | Same ink system |
| Vải | Same fabric lot | Same fabric lot |
| Print Test | Current reference result | Same image and settings |
| Sau khi điều trị | Current process | Same process initially |
Recommended Laboratory Trial Workflow
Step 1: Identify the ink system
Confirm whether the process is reactive, disperse or pigment inkjet printing.
Step 2: Define the fabric
Record fibre composition, construction, weight and relevant previous treatment.
Step 3: Establish the current benchmark
Record the current pretreatment product, formula, dosage and known performance.
Step 4: Prepare the candidate
State whether the trial tests the unchanged plant SOP or a separately documented preparation route appropriate to the candidate. Record the product form, as-supplied dosage and concentration basis, water, mixing, temperature, preparation window and readiness criterion. An adjusted trial does not prove a drop-in replacement under the original SOP.
Step 5: Evaluate basic properties
- Hình thức
- Độ nhớt
- pH
- Lọc
- Physical stability
Step 6: Apply to the same fabric
Control application method and pickup as closely as possible.
Step 7: Dry under controlled conditions
Avoid allowing different residual moisture to distort the comparison.
Step 8: Print using the same ink and settings
Use a diagnostic test image containing fine details, color boundaries and solid areas.
Step 9: Complete normal fixation or curing
Use the standard process appropriate to the ink system.
Step 10: Complete washing where required
Final acceptance should be based on the finished textile.
Step 11: Optimize the candidate
Once technical suitability is established, adjust dosage or pretreatment pickup gradually to determine the practical operating window.
Production Scale-Up
A successful laboratory test is an important milestone, but it does not automatically prove production performance.
Scale changes several variables
- Batch size
- Mixer geometry
- Circulation
- Thời gian giữ
- Application speed
- Drying uniformity
- Fabric tension
- Production-environment conditions
Conduct a limited production trial
Before a limited production trial, agree the fabric lot, ink set, test image, run length, sampling positions and acceptance limits. Keep the approved pretreatment available. Start with fixed printing and post-treatment settings; record any later optimisation as a separate trial so its effect is not attributed to the chemistry alone.
Evaluate the whole run
Compare fabric from the beginning, middle and end rather than approving the candidate from the first printed section.
Verify the first commercial batch
Connect the first bulk delivery to the qualified commercial grade, TDS revision, batch COA and retained reference sample. Approval should state its scope: fabric, ink, application method and fixation route. A pass on one fabric is not blanket approval for other blends, printers or dye systems.
Decide Whether to Adopt, Investigate or Revert
Use the following as a proposed trial record, with limits agreed before the run. It is not a table of FSX performance guarantees.
| Checkpoint | Evidence to retain | Quyết định |
|---|---|---|
| Finished-print quality | Same test image after normal fixation and washing or curing; shade, definition, fastness and handle | Adopt only if all required properties meet the agreed specification |
| Run stability | Beginning, middle and end samples; pickup, bath condition, drying and operator adjustments | Investigate drift before extending the trial |
| Unexpected defect or equipment incompatibility | Time, material batch, settings and affected fabric; comparison with the approved reference | Pause candidate use, segregate affected output and revert through the mill’s approved procedure |
| Commercial readiness | Exact grade, TDS revision, batch documents, trial scope and cost per accepted output | Release only within the documented approval scope |
Have the mill’s process and quality personnel authorise the change. This prevents a visually stronger first print from becoming an uncontrolled whole-line chemical change.
Troubleshooting Common Digital Printing Problems
| Vấn đề được ghi nhận | Possible Chemical or Process Cause | What to Check |
|---|---|---|
| Color bleeding | Insufficient surface control or excessive liquid movement | Pretreatment pickup, rheology, fabric absorbency, drying and ink laydown |
| Weak fine-line definition | Ink migration or uneven pretreatment | Application uniformity, drying, fabric and ink amount |
| Weak color result | Multiple possible causes | Ink, pickup, fixation, washing and pretreatment together |
| Uneven shade | Nonuniform pretreatment or drying | Edge-to-center pickup and moisture distribution |
| High filter residue | Hydration, gel or incompatibility | Preparation method and staged chemical addition |
| Pretreatment viscosity drifts | Hydration, temperature, evaporation or instability | Holding time, tank condition and measurement method |
| Pigment print feels stiff | Excess solids or binder/paste balance | Pretreatment dosage, binder and curing |
| Lab result passes but production fails | Scale-up difference | Batch size, application equipment, pickup and drying |
Digital printing defects should be investigated as system problems. Not every weak print result is caused by the pretreatment, and not every problem can be corrected by increasing thickener concentration.
Tổng chi phí trong quá trình sử dụng
New textile chemical solutions should eventually be evaluated commercially, but purchase price alone is not enough.
Compare chemical consumption
Calculate cost using the practical pretreatment dosage or pickup required for acceptable production.
Compare preparation cost
Include mixing, filtration, labor and any repeated formula correction.
Compare production efficiency
Consider pretreatment stability, machine interruption, rejected fabric and reprinting.
Compare post-treatment
Drying, steaming, curing and washing requirements form part of the complete process economics.
Compare supply consistency
A lower-priced product can become expensive if batch variation creates repeated laboratory and production adjustments.
The preferred chemical solution is therefore the system that produces the required finished textile at an acceptable total cost and process risk.
How FSX Chemical Supports Digital Printing Development
FSX Chemical provides digital printing paste and textile pretreatment routes for reactive, disperse and pigment inkjet printing.
DG-20: Reactive Fabric Pretreatment
DG-20 is an FSX starting route for reactive fabric-pretreatment evaluation. Confirm the current TDS, preparation conditions and intended application; assess print definition, colour, fixation and wash-off in the complete process.
Direct-Disperse Pretreatment: Confirm the Grade
For direct disperse inkjet printing, confirm an application-specific FSX grade against its current TDS. Evaluate preparation, filtration, polyester application and thermal fixation before approval; do not infer suitability from an old product code.
DP-P
DP-P is the starting route for pigment digital printing where binder compatibility, curing, fastness and fabric hand feel need to be balanced.
Current-product matching
Buyers already using another digital printing paste can submit their existing product information through Mẫu và việc kết hợp .
Các thông tin hữu ích bao gồm
- Current product and commercial grade
- TDS or available COA
- Mẫu tham chiếu vật lý
- Reactive, disperse or pigment ink
- Fabric composition
- Liều lượng hiện tại
- pH
- Viscosity and test method
- Pretreatment application method
- Drying conditions
- Fixation or curing process
- Current problems such as bleeding, weak color or unclear edges
The objective is to identify an appropriate starting route and verify it through controlled laboratory and production testing rather than assume that one digital printing paste is suitable for every textile inkjet system.
Các câu hỏi thường gặp
What chemicals are used in digital textile printing?
The complete chemical system depends on the ink route and may include fabric pretreatment chemicals, rheology-control materials, moisture- management components, binders or fixation-related auxiliaries. The exact system should be selected for reactive, disperse or pigment printing.
What is digital printing paste?
Digital printing paste is a fabric-side pretreatment or thickening system used to help control textile surface behavior before or around inkjet printing.
Is digital printing paste added to digital ink?
It should not be treated as a general ink additive. Textile pretreatment thickeners are primarily evaluated on the fabric side, while digital ink must remain within the fluid requirements of its printhead and ink-delivery system.
What is the best pretreatment for reactive digital printing?
There is no universal best formulation. The correct pretreatment depends on the reactive ink, fabric, application method, drying, fixation and required finished-textile quality.
Can the same pretreatment be used for reactive and disperse ink?
A direct transfer should not be assumed. Reactive and disperse systems involve different fibres, colorants and fixation processes and should be evaluated separately.
What is important in pigment digital printing pretreatment?
Pretreatment should be evaluated together with the pigment ink, binder, curing conditions, print definition, rubbing performance and fabric hand feel.
Does higher pretreatment viscosity improve print sharpness?
Not automatically. Definition also depends on rheology, fabric absorbency, pickup, ink laydown, drying and fixation. Excessive viscosity or solids can create other problems.
Why is filtration important if the pretreatment does not pass through the printhead?
Gels and residue can still interfere with preparation, pumping, coating, padding, spraying and other pretreatment equipment.
How should I test a new digital printing chemical?
Compare it against the current approved system using the same fabric, ink, application method, drying, printer settings and post-treatment, then complete a controlled production trial.
Can FSX Chemical match my current digital printing paste?
Provide the current TDS or sample together with the ink route, fabric, pretreatment method and main production issue. FSX Chemical can review a reactive, direct-disperse or pigment pretreatment candidate; the exact grade and trial conditions must then be confirmed.
Technical Route References
Mimaki’s sublimation overview distinguishes transfer-paper and direct-to-fabric routes. Konica Minolta’s pretreatment-ink development illustrates a specialised equipment-qualified jettable category. These manufacturer examples explain process boundaries; they do not validate an FSX grade or approve third-party fluids for a printer.
Exploring a New Chemical Route for Digital Textile Printing?
Send FSX Chemical the TDS or physical sample of the digital printing paste you currently use together with your ink system, fabric, pretreatment method, dosage, pH and production conditions.
If your current challenge is bleeding, unclear fine lines, weak dark shades, high filtration residue, unstable pretreatment or inconsistent output between batches, include these details with your inquiry.
FSX Chemical can review the intended reactive, direct-disperse or pigment process and identify a candidate for side-by-side testing. Confirm the current product code and TDS before purchasing; retain the approved reference until the trial is accepted.
Final suitability should be confirmed using your actual ink, fabric, printing equipment and fixation or curing process before commercial conversion.
Request Digital Printing Paste Matching | Send Your Current Paste TDS or Printing Problem | Yêu cầu báo giá trực tiếp từ nhà máy📧 Email: Service@fsxchemical.com
Các bài viết liên quan
Chất làm đặc trong in vải theo loại thuốc nhuộm và quy trình in
CMC so với CMS so với natri alginat so với bột in kỹ thuật số: Hướng dẫn lựa chọn thực tiễn
CMC cho mực in gốc nước: Lựa chọn cấp độ và thử nghiệm tính tương thích
Hỗn hợp in vải gốc xenluloza: Loại CMC và đánh giá nhà cung cấp
So sánh giữa natri alginat và CMC trong in ấn dệt may: So sánh hiệu suất và chi phí
Alginat natri trong in vải kỹ thuật số phản ứng: Xử lý trước và lựa chọn loại sản phẩm
CMS for Textile Sizing and Digital Printing: Product Identity and Trial Guide
Cách chọn chất làm đặc phù hợp cho quá trình in trên vải
Các ứng dụng của natri alginat trong ngành dệt may: Bảng đánh giá mức độ phù hợp ứng dụng dành cho các nhà sản xuất
Hóa chất in trên vải và chức năng của chúng: 10 nhóm chính
So sánh các chất làm đặc trong in ấn dệt may: Natri alginat, CMC, CMS và Digital Paste
Hiểu về việc kiểm soát độ nhớt trong các quy trình in kỹ thuật số trên vải
Liên kết nhanh
Gửi yêu cầu của bạn
Mẫu thử miễn phí · Trả lời trong vòng 24 giờ
Gửi yêu cầu về sản phẩm của bạn
Vui lòng cung cấp tên sản phẩm, ứng dụng, số lượng, điểm đến và bất kỳ tài liệu kỹ thuật (TDS), hình ảnh mẫu hoặc tài liệu nào mà quý khách đã có. FSX Chemical sẽ xem xét thông tin này và đề xuất bước tiếp theo liên quan đến báo giá, đối chiếu mẫu hoặc lựa chọn sản phẩm.