Low-Solids Pigment Printing with Acrylic Thickener: How to Improve Soft Hand Without Losing Fastness

Low-solids pigment printing should reduce unnecessary nonvolatile deposit while preserving the binder film and rheology...

Low-solids pigment printing means reducing unnecessary material deposited on the printed area while retaining the binder film, rheology and cure needed for the required color, hand and fastness. Compare complete-paste nonvolatile content and measured wet paste add-on, not thickener product solids alone. Report binder polymer, thickener polymer and total nonvolatile residue separately where their composition is verified. A lower product dose or softer unwashed print is not sufficient evidence of an approved low-solids system.

How Can Low-Solids Pigment Printing Improve Soft Hand Without Losing Fastness?

The safest route is to reduce unnecessary polymer solids while preserving the binder film and curing conditions required for pigment fixation.

A practical optimization sequence is:

Define Current Print Standard → Measure Total Paste Solids / Add-On → Build Efficient Thickener Window → Optimize Binder Only Within Fastness Limits → Control Deposit → Cure Correctly → Compare Hand and Rubbing Together

The key idea is:

Soft Hand ≠ Minimum Binder

and:

Low Solids ≠ Low Fastness.

A well-designed low-solids route uses:

  • Efficient acrylic thickener at the lowest useful dosage
  • Binder chemistry that achieves required fixation without excessive film build
  • Controlled paste add-on
  • Correct curing

to minimize stiffness while maintaining printing performance.

What Does “Low-Solids Pigment Printing” Actually Mean?

Use a declared basis: as-supplied product concentration, verified active-polymer concentration, method-defined nonvolatile residue or deposited mass per printed area. These are different quantities. Nonvolatile residue can include pigment, salts and other auxiliaries as well as polymers; an oven-solids result does not identify binder or thickener polymer by itself.

Relevant nonvolatile components include:

  • Pigment solids
  • Binder solids
  • Thickener polymer
  • Fixer / crosslinker solids
  • Other nonvolatile auxiliaries

The practical question is:

How much total nonvolatile material remains in the printed area after drying and curing?

A formula can use a low-solids thickener but still create a hard print if binder level and paste add-on are high.

Likewise, a formula can use a moderately concentrated liquid thickener at very low dosage and still produce a low total polymer deposit.

Therefore:

Product Solids ≠ Deposited Solids.

Why Does Pigment Printing Sometimes Feel Hard?

Pigment printing depends on a polymer film to hold insoluble pigment to the textile.

That film inevitably changes the surface compared with unprinted fabric.

Printed-area stiffness can increase because of:

  • High binder solids
  • High thickener polymer dosage
  • High pigment solids
  • Excess paste deposit
  • Over-crosslinking / harsh curing conditions
  • Multiple auxiliary solids accumulating in the print

The problem is therefore not simply “acrylic binder makes fabric hard.”

The actual hand is a system result:

Fabric + Pigment + Binder + Thickener + Add-On + Curing

This is why hand should be optimized only after print strength and fastness are inside the required range.

What Role Does Acrylic Thickener Play in Fabric Hand?

Acrylic thickener controls paste flow and deposit.

It does not provide the main pigment fixation.

However, thickener can influence hand in two ways.

1. Direct Polymer Deposit

Nonvolatile thickener polymer can remain in the printed area after curing.

More thickener solids can contribute to:

  • Higher surface polymer load
  • More film-like residue
  • Potential stiffness

2. Indirect Control of Paste Add-On

Rheology changes:

  • Screen transfer
  • Pénétration
  • Surface deposit

A high-efficiency thickener can therefore improve hand not only by using less polymer, but also by controlling how much paste reaches and remains on the fabric.

Why Binder Cannot Be Reduced Blindly

Binder is the main pigment-fixation component.

After curing, it forms a film that holds pigment to the textile.

Changing binder level can change both film properties and hand, but evaluate it at a controlled delivered pigment amount, comparable printed coverage and recorded wet paste add-on. Keep substrate, conditioning and the validated actual fabric cure history consistent. If deposit or curing changes as well, report those differences rather than attributing the result solely to binder concentration.

This creates the central low-solids tradeoff:

Binder Too Low → Weak Pigment Fixation / Poor Rubbing

Binder Too High → Heavy Film / Harder Hand

The correct target is:

Lowest Validated Binder Level Within the Tested Fabric, Deposit and Cure Window.

Do not reduce binder first and then try to recover fastness by adding more thickener.

Thickener cannot replace the fixation function of binder.

Pigment Loading and Total Deposit

Pigment solids themselves contribute to the mass deposited in the printed area.

Dark shades commonly use more pigment dispersion than pale shades.

This can increase:

  • Pigment solids
  • Surfactants / dispersants
  • Binder demand
  • Foam risk
  • Total film mass

A low-solids thickener route is therefore especially valuable in dark shades, because the formula already carries a larger pigment burden.

But dark-shade rheology should be measured directly.

Do not lower thickener dosage so far that screen transfer or color yield becomes unstable.

Fixer and Auxiliary Solids

Fixers, crosslinkers, softeners, wetting agents and defoamers can add both:

  • Functional benefit
  • Additional nonvolatile material

In a low-solids program, review every auxiliary by asking:

Does this ingredient solve a defined problem at this dosage?

Avoid adding multiple auxiliaries only because they existed in an older formula.

But do not remove a fixer or crosslinker without checking:

  • Chimie des liants
  • Curing requirement
  • Résistance au frottement
  • Customer specification

Low-solids optimization should remove redundant solids, not necessary functionality.

Paste Add-On vs. Formula Solids

Two pastes with the same solids percentage can leave different amounts of material on the fabric if the screen deposit is different.

For a defined drying method, calculate estimated paste nonvolatile content from the documented input fractions. If dᵢ is the as-supplied product dosage in wt% of final paste and nᵢ is its measured nonvolatile content in wt%, estimated paste nonvolatile content (wt%) = Σ(dᵢ × nᵢ ÷ 100). Include all ingredients and use the same test basis; verify the mixed paste where practical.

Estimated nonvolatile deposit (g/m² of printed area) = Wet paste add-on (g/m² of the same area) × Paste nonvolatile content (wt%) ÷ 100. Determine wet add-on from promptly weighed matched specimens or another validated method; use a registered solid-coverage test patch of known area, matched fabric reference and a defined weighing interval. Do not mix a printed-area deposit with a whole-width or unprinted-area basis.

Hypothetical mass balance—not a recommended formula: 60 g/m² wet paste with 10 wt% method-defined nonvolatile content gives an estimated 6 g/m² residue. In that same paste, 5 wt% binder product with a separately verified 40 wt% binder-polymer fraction contributes 1.2 g/m² binder polymer; 2 wt% thickener product at a verified 30 wt% thickener-polymer fraction contributes 0.36 g/m². These polymer amounts are parts of the total residue, not additional quantities to add again. The remaining residue comes from other ingredients. Curing reactions and volatile loss can change final mass, so this estimate is not an independent assay of the cured binder film.

Therefore, a low-solids program must control both:

  • Formula composition
  • Application deposit

Paste add-on is influenced by:

  • Screen mesh / engraving
  • Squeegee pressure
  • Squeegee speed
  • Stroke count
  • Paste rheology
  • Composition du tissu

Reducing unnecessary add-on can sometimes improve hand more effectively than making a major chemistry change.

Surface Color Yield and Penetration

Low-solids printing should not sacrifice apparent color yield.

If the paste becomes too fluid:

  • Penetration can increase.
  • Pigment can move deeper into the structure.
  • Surface color can weaken.

The operator may then compensate with more pigment or more paste deposit, which defeats the low-solids objective.

The better strategy is to use rheology to maintain:

Controlled Surface Deposit + Sufficient Coverage + Limited Unnecessary Penetration.

Evaluate face-side color and reverse-side penetration together.

Rheology as a Low-Solids Tool

A high-efficiency synthetic thickener can create useful printing rheology at low dosage.

The target profile is:

Low-Shear Body → Shear Thinning Under Screen Force → Controlled Recovery After Transfer

This helps:

  • Maintain print definition
  • Limit spreading
  • Control deposit
  • Reduce unnecessary polymer addition

The lowest-viscosity paste is not automatically the lowest-solids solution.

If it requires more pigment, more binder or more paste add-on to compensate for poor transfer, total deposited solids can actually increase.

High Thickening Efficiency vs. High Polymer Deposit

One important reason synthetic acrylic thickeners are widely used in pigment printing is that a small polymer dosage can generate substantial viscosity.

This can reduce:

  • Thickener solids deposited
  • Residual polymer film
  • Potential hand penalty

compared with a less efficient thickening route that needs much more polymer.

But thickening efficiency should always be compared in the complete formula.

A grade that is extremely efficient in water but collapses after binder or pigment can require higher production dosage and lose the low-solids advantage.

Therefore, evaluate:

Working Dosage in Complete Paste

not:

Water Thickening Efficiency Alone.

Build a Thickener Dosage–Rheology Curve

Prepare several thickener levels around the current dosage.

For each point, record:

  • Final pH
  • Low-shear viscosity
  • Higher-shear viscosity
  • Recovery
  • Screen transfer
  • Paste add-on
  • Définition de l'impression
  • Tissu à la main

The objective is to identify:

Lowest Thickener Dosage That Keeps the Complete Paste Inside the Approved Printing Window.

Do not select the dosage from viscosity alone.

Build a Binder-Level Curve

After the thickener working window is stable, build a small binder curve.

For each binder level, keep:

  • Pigment
  • Épaississant
  • Screen settings
  • Curing conditions

controlled.

Then evaluate:

  • Dry rubbing
  • Wet rubbing
  • Wash performance if required
  • Rendement en couleur
  • Tissu à la main

The lowest passing point in this binder ladder is a candidate operating level for the tested system, not a universal minimum. Repeat near the pass/fail transition with measured binder and pigment deposition, comparable coverage, the same fabric lot, actual cure history and conditioning. Confirm that the selected level remains acceptable across the intended production variation before release.

Do not identify the “softest” sample before confirming fastness.

Build a Thickener × Binder Matrix

TestLower BinderCurrent BinderHigher Binder
Lower ThickenerTestTestOptional
Current ThickenerTestReferenceOptional
Higher ThickenerUsually diagnostic onlyDiagnosticAvoid unless needed

For every useful point, record:

  • Viscosity / rheology
  • Paste add-on
  • K/S or agreed shade
  • Dry / wet rubbing
  • Hand

This matrix compares the tested thickener and binder combinations. Interpret hand together with measured paste, binder and pigment deposition, actual cure and fastness. If deposit changes between cells, the response includes that application difference; the matrix alone does not isolate polymer chemistry or prove a single cause. Include repeats where the decision is sensitive to small differences.

Curing Efficiency: The Hidden Variable

A low-solids binder system can only deliver fastness if the binder forms the intended film.

Curing depends on:

  • Chimie des liants
  • Crosslinker / fixer system
  • Time
  • Température
  • Actual fabric temperature
  • Vitesse de la machine

A formula with moderate binder and correct cure can outperform a higher-binder formula that is poorly cured.

Therefore, optimize binder level only after the curing process is controlled.

Use the binder supplier’s validated cure range as the starting point.

Why Under-Curing Can Make a Low-Solids Formula Fail

If curing is incomplete:

  • Binder film formation may be incomplete.
  • Pigment can release more easily during rubbing.
  • Wet rubbing can be especially weak.

The operator may respond by increasing binder concentration.

This can improve fastness but make the hand harder—without solving the real thermal-process problem.

Before increasing binder, confirm:

  • Actual oven temperature
  • Temps de séjour
  • Température du tissu
  • Binder cure requirement

Why Over-Curing Can Also Hurt Hand

More heat is not automatically better.

Excessive curing can:

  • Increase polymer film hardness
  • Change fabric hand
  • Consume unnecessary energy
  • Stress heat-sensitive substrates or finishes

The correct target is:

Complete Enough Cure for Required Fastness Without Unnecessary Thermal Severity.

Do not publish or use one universal curing temperature for all binder systems.

Dark Shades and High Pigment Loading

Dark shades are a demanding test of low-solids formulation.

They often contain more:

  • Pigment solids
  • Dispersant / surfactant
  • Binder demand

At the same time, color defects are visually obvious.

Vérifier :

  • Viscosity retention
  • Solid-area coverage
  • Pénétration
  • Mousse
  • Rubbing
  • Hand

Do not apply a light-shade low-solids formula directly to black or navy without a separate trial.

Fabric Structure and Hand Sensitivity

The same polymer deposit can feel different on different fabrics.

A lightweight knit can be highly sensitive to a stiff printed film.

A dense woven fabric can tolerate a different deposit before the hand becomes unacceptable.

Important variables include:

  • GSM
  • Thickness
  • Knit / woven construction
  • Étirement
  • Surface hairiness

Hand should therefore be assessed on the actual commercial substrate.

Cotton, Polyester and Blends

Pigment printing can be used across cotton, polyester and blends because binder provides the main fixation mechanism.

But the substrate still changes:

  • Wetting
  • Pénétration
  • Surface adhesion
  • Perceived hand

A low-solids formula optimized on cotton should therefore be rechecked on polyester or CVC before commercial use.

Keep the low-solids strategy, but validate the fabric-specific working window.

Screen Mesh, Engraving and Deposit Control

Screen geometry directly influences paste add-on.

If hand is too hard, the first chemical response should not always be lower binder.

Also check whether:

  • Screen opening is too large.
  • Engraving is too deep.
  • The design receives excessive deposit.

Reducing unnecessary paste add-on can improve hand while preserving binder concentration and fastness chemistry.

Thickener and screen settings should be optimized together.

Squeegee Pressure, Speed and Stroke Count

Machine settings change how much paste reaches the fabric.

Higher pressure or multiple strokes can increase:

  • Paste transfer
  • Pénétration
  • Total deposited solids

If a low-solids formula still feels hard, record:

  • Squeegee pressure
  • Speed
  • Angle
  • Stroke count

before changing binder chemistry.

A lower-deposit printing setup can preserve both color and hand more effectively than simply reducing binder.

Foam, Defoamer and Hidden Add-On Problems

Entrained air can make paste density and transfer less consistent.

Foam can also create:

  • Pinholes
  • Uneven deposit
  • Variable coverage

The operator may then compensate with more paste or stronger machine settings.

This can increase solids deposit unintentionally.

Control foam before finalizing a low-solids working window.

Also recheck viscosity after defoamer optimization because some defoamers can change associative acrylic rheology.

How Should Soft Hand Be Evaluated?

Hand can be assessed subjectively or instrumentally.

For routine laboratory work, use a controlled panel or internal rating method.

Keep constant:

  • Fabric lot
  • Printed area
  • Conditioning
  • Durcissement
  • Comparison direction

Compare hand only after:

  • Color target is acceptable.
  • Rubbing passes.
  • Paste add-on is known or controlled.

A softer but under-bindered print is not a successful low-solids result.

How Should Rubbing Fastness Be Evaluated?

Use the customer-required standard or the mill’s validated internal method.

At minimum, compare:

  • Dry rubbing
  • Wet rubbing

after the defined cure and conditioning. Use the customer-agreed dry and wet rubbing method, such as ISO 105-X12:2016, and record the method edition, specimen direction, test location, wet-cloth preparation and rating conditions. Check the actual standard and customer protocol before claiming compliance; a method name does not itself establish a passing grade.

If a lower-binder sample feels softer but fails wet rubbing, that tested combination is unacceptable. The result alone does not establish a minimum binder threshold or prove binder dosage is the only cause. Check delivered binder and pigment mass, coverage, substrate, actual cure, conditioning and the rubbing method against the passing reference.

Retain the approved reference while investigating. Use a controlled, repeated binder ladder to bracket a passing range, and evaluate cure sensitivity separately when needed. A laboratory pass permits only the next authorized trial stage; confirm the finished-fabric requirements in production before adopting a reduced level.

Should Pigment Prints Be “Washed Off” Like Reactive Prints?

No universal reactive-style wash-off step should be assumed for conventional pigment printing.

The binder film is intentionally designed to remain on the fabric and hold the pigment.

If the process includes post-cure washing, evaluate it for:

  • Surface residue removal
  • Hand
  • Loose pigment removal
  • Final customer requirements

Do not treat aggressive wash-off as a substitute for optimizing binder, thickener solids or curing.

  1. Document the current commercial formula and paste add-on.
  2. Record current viscosity, pH, pigment, binder and thickener dosage.
  3. Print and retain a current-reference fabric.
  4. Build a thickener dosage curve first.
  5. Choose the lowest stable thickener point that prints cleanly.
  6. Build a small binder-level curve at that thickener point.
  7. Keep curing constant and validated.
  8. Measure color, penetration, dry/wet rubbing and hand.
  9. Repeat with a dark shade if commercially relevant.
  10. Confirm on the real fabric construction and machine.

For a broader thickener qualification framework, review Textile Printing Thickener Testing Parameters.

Use GO / CONDITIONAL / FAIL Decision Gates

DecisionMeaningPermitted next step
GOAll agreed critical criteria pass for the tested stage and recorded cure window.Proceed only to the next documented approval stage; a laboratory pass is not automatically a commercial release.
CONDITIONALEvidence is incomplete or a process restriction still needs validation.Only a specifically authorized controlled trial, with an owner, scope and stop criteria. Do not release routine production while a critical requirement remains unmet.
FAILA critical print, fastness or process requirement fails.Hold the candidate; investigate and retest before any release decision.

A low-solids target should never override the finished-fabric requirement.

Production Trial Approval

After laboratory optimization, run a representative production trial.

Record:

  • Fabric composition / construction
  • Thickener grade / batch
  • Dosage de l'épaississant
  • Binder grade / dosage
  • Pigment product / dosage
  • Fixer / auxiliary package
  • Final pH
  • Méthode d'essai de viscosité
  • Screen mesh / engraving
  • Squeegee settings
  • Paste add-on
  • Vitesse de la machine
  • Curing conditions
  • Color / K/S or approved shade
  • Dry / wet rubbing
  • Tissu à la main

Approve a complete production window rather than a formula percentage alone.

Common Low-Solids Formulation Mistakes

1. Reducing Binder First

Binder is the main fixation component. Reduce unnecessary thickener and deposit before sacrificing fastness.

2. Assuming Less Thickener Always Means Softer Hand

If rheology becomes poor and paste add-on rises, total deposited solids can increase.

3. Comparing Product Solids Instead of Deposited Solids

Working dosage and paste add-on determine the real polymer load.

4. Ignoring Curing

Under-cured low-binder prints can fail rubbing even when the chemistry is otherwise suitable.

5. Optimizing Hand Before Fastness

A soft print that fails wet rubbing is not a successful formulation.

6. Using One Formula for Every Shade

Dark shades can require a different binder/thickener working window.

7. Ignoring Screen Deposit

Excess add-on can create hard hand even with an efficient thickener.

8. Calling “Low Solids” a Sustainability Claim Without Data

Measure actual chemical dosage, add-on, energy and rejects before making broader environmental claims.

Troubleshooting Table

Problème constatéFirst Variables to CheckDo Not Assume
Hand is hard but rubbing is excellentBinder level, thickener solids, paste add-on, curingBinder reduction is the only solution
Hand improves but wet rubbing failsDelivered binder and pigment mass, coverage, actual cure, substrate and test methodThe thickener caused the fastness loss
Lower thickener gives weak surface colorPenetration, transfer, add-onMore pigment is the first correction
Low-solids lab print works but production feels hardScreen deposit, squeegee pressure, stroke countThe formula changed
Dark shade is much harder than light shadePigment/binder solids, thickener dosage, add-onOne formula fits every shade
Fastness improves only at very high binderBinder chemistry, curing efficiency, fabric surfaceHigh binder is always the best route
Low-thickener paste spreadsRheology / recovery / screen settingsLow solids requires low viscosity
High-efficiency thickener costs more/kgWorking dosage and total depositHigher price/kg means higher print cost

Coût total d'utilisation

Low-solids optimization should reduce total process cost—not simply chemical grams.

A useful model is:

Cost per accepted output unit = Total allocated trial or production cost (currency) ÷ Accepted finished output in the agreed unit. Include actual consumed chemical cost, cure energy, processing time and consistently allocated rework, waste and quality loss. Paste add-on determines consumption; machine efficiency affects time and output. Neither is an extra currency amount to add directly. Avoid counting the same waste or rework twice.

A higher-efficiency acrylic thickener can justify a higher price per kilogram if it allows:

  • Lower working dosage
  • Lower residual polymer deposit
  • Stable screen transfer
  • Softer hand
  • Less formula correction

A higher-performance binder can also justify a higher unit price if it reaches the required rubbing fastness at a lower practical film build.

Use a consistent output basis:

Compare cost per accepted m², or per accepted linear meter only at the same finished width, quality specification and design coverage. Record both chemical use and accepted yield; a cheaper paste is not a lower-cost print if it needs more deposit or creates more rejected fabric.

Raw-material price alone is not the decision criterion.

What Information Should You Send to a Supplier?

For useful low-solids / soft-hand matching, provide:

  • Current acrylic thickener / TDS
  • Dosage de l'épaississant
  • Binder grade / dosage / solids if available
  • Pigment product / dosage
  • Fixer / auxiliary package
  • Final paste pH
  • Viscosity and complete test method
  • Fabric composition / construction
  • Screen mesh / engraving
  • Squeegee settings
  • Paste add-on if measured
  • Curing conditions
  • Current dry / wet rubbing
  • Current hand problem

FSX Chemical can use this information through Échantillons et correspondances to define a controlled low-solids trial.

Critique Synthetic Printing Thickeners, CMC for Pigment Printing: Binder Compatibility, Rheology and Fabric Hand Feel et Textile Printing Thickener Applications for related selection logic.

How Should a Mill Build a Low-Solids Pigment Printing Formula?

A practical control chain is:

Measure Current Deposit → Reduce Unnecessary Thickener Solids → Keep Rheology Stable → Find Minimum Passing Binder Level → Control Screen Add-On → Validate Cure → Compare Color / Rubbing / Hand → Confirm on Production Machine

Les principes fondamentaux sont les suivants :

  1. Low-solids pigment printing means reducing unnecessary deposited solids, not simply reducing every ingredient.
  2. Binder remains the main pigment-fixation component and should not be reduced below the fastness requirement.
  3. High-efficiency acrylic thickener can improve hand by controlling rheology at lower polymer dosage.
  4. Paste add-on can affect hand as strongly as formula solids, so screen and squeegee settings must be controlled.
  5. Curing efficiency determines whether a lower-binder formula can still achieve acceptable rubbing fastness.
  6. The best low-solids route is the formulation and application window that produces the required color, rubbing and hand at the lowest practical Total Cost in Use.

Foire aux questions

1. What does low-solids pigment printing mean?

It means minimizing unnecessary nonvolatile material deposited in the printed area while maintaining the pigment, binder and rheology needed for acceptable print quality and fastness.

2. Does low-solids printing mean using less binder?

Not automatically. Binder provides the main pigment fixation. A reduced level must repeatedly pass the required fastness and hand criteria within the tested fabric, deposited binder/pigment and actual cure window. One passing or failing point does not establish a universal minimum.

3. Why can lower thickener dosage improve fabric hand?

Less nonvolatile thickener polymer remains in the printed area, provided the lower dosage still gives stable rheology and does not increase paste add-on or penetration.

4. Can synthetic acrylic thickener help produce a softer print?

Yes, if its high thickening efficiency allows the required rheology at a low working dosage. Final hand still depends strongly on binder, pigment, deposit and curing.

5. Why does reducing binder improve hand but reduce rubbing fastness?

Binder forms the film that holds pigment to the fabric. Too little binder reduces film integrity and pigment fixation.

6. Can better curing allow lower binder dosage?

Potentially, if the original process was under-curing the binder. The new level must be validated through rubbing and other required tests; do not assume every formula can reduce binder.

7. Why can a low-solids formula still feel hard?

Paste add-on may still be high, the binder film may be stiff, pigment loading may be high, or curing may be too severe.

8. Should dark shades use the same low-solids formula as light shades?

Not automatically. Dark shades usually have higher pigment loading and may need a different binder/thickener working window.

9. What should be optimized first: thickener or binder?

First establish the lowest stable thickener dosage that gives clean printing. Then optimize binder only within the fastness requirement.

10. Does lower Brookfield viscosity mean lower solids?

No. Viscosity is a rheological result, while solids describe composition. A low-viscosity paste can still contain high binder and pigment solids.

11. Should pigment prints be washed aggressively to improve hand?

Not as a universal strategy. Pigment binder film is intended to remain. Post-cure washing should be process-specific and should not replace proper control of binder, thickener and add-on.

12. What should I send FSX Chemical for low-solids matching?

Send the current thickener, binder, pigment and auxiliary dosages, viscosity method, fabric, screen, paste add-on if known, curing conditions, rubbing results and hand target.

Reduce Unnecessary Solids Without Sacrificing Pigment Fastness

If your pigment print has acceptable color and rubbing fastness but the printed area feels too stiff, FSX Chemical can help structure a controlled low-solids trial focused on thickener efficiency, binder minimum, paste add-on and curing.

For a useful technical review, send:

  • Your current acrylic thickener sample, TDS or COA
  • Dosage de l'épaississant
  • Binder grade / dosage / solids if available
  • Pigment product and dosage
  • Fixer / auxiliary package
  • Final pH and viscosity test method
  • Fabric composition / structure
  • Screen mesh / engraving
  • Squeegee settings
  • Paste add-on if available
  • Curing conditions
  • Dry / wet rubbing results
  • Current fabric-hand target

Commencez par Échantillons et correspondances for a controlled current-vs-candidate evaluation.

Critique Synthetic Printing Thickeners for the current FSX pigment-printing thickener range.

You can also Demander un devis directement auprès du fabricant after the suitable low-solids working window is confirmed or Contacter FSX Chemical for technical discussion📧 E-mail: Service@fsxchemical.com

The best low-solids pigment-printing formula is not the one with the least chemistry. It is the one that removes unnecessary polymer and deposit while preserving the binder film, rheology and curing needed for stable color, rubbing fastness and an acceptably soft hand.

Contact rapide

Envoyez-nous votre demande

ou

Échantillons gratuits · Réponse sous 24 heures

Renseignements sur les produits et assistance

Envoyez-nous vos spécifications produit

Veuillez nous communiquer le nom du produit, son application, la quantité, la destination, ainsi que toute fiche technique (TDS), photo ou document dont vous disposez déjà. FSX Chemical examinera ces informations et vous recommandera la marche à suivre pour obtenir un devis, trouver un échantillon correspondant ou choisir un produit.

Informations sur le produit Nom du produit, référence, modèle, photo de l'étiquette ou référence du fournisseur.
Documents disponibles Fiche technique (TDS), fiche de données de sécurité (SDS), certificat d'analyse (COA), photo d'exemple, liste des produits ou données d'essai.
Détails de la commande Quantité estimée, conditionnement, pays de destination, port ou conditions commerciales.
Demande ou problème Procédé d'impression textile, besoins en matière de formulation, problème actuel ou performances visées.