Pretreatment Solids Content in Reactive Digital Printing: How It Affects Color Yield, Bleeding and Fabric Hand

Pretreatment solids affect ink localization, fixation chemistry, drying and wash-off, but bath concentration alone is...

Specify reactive pretreatment solids as a method-defined residue or a documented formulation contribution, then connect it to measured fabric add-on. Total dry residue is not automatically active polymer: urea, alkali, salts and other ingredients can contribute. The useful target is a process-specific formulation and add-on window that meets post-wash color, edge definition and fabric-hand requirements, with the required drying, fixation and washing retained.

How Does Pretreatment Solids Content Affect Reactive Digital Printing?

Pretreatment solids influence how much chemistry remains on and inside the fabric after pretreatment water is removed.

That chemistry affects:

  • Ink droplet spreading
  • Ink penetration
  • Surface color concentration
  • Alkali available for reactive dye fixation
  • Moisture behavior during steaming
  • Drying load
  • Wash-off demand
  • Final fabric hand if residues remain

The useful relationship is not:

More Solids → Better Printing.

Instead, mills should find:

Minimum Stable Pretreatment Add-On That Delivers the Required Color Yield, Boundary Clarity, Fixation and Post-Wash Hand.

This requires controlling both pretreatment concentration and fabric pick-up.

What Does “Pretreatment Solids Content” Mean?

In reactive digital printing, “pretreatment solids” should be defined before data is compared.

It can refer to the combined nonvolatile or dry-forming components in the pretreatment liquor, such as:

  • Thickener or migration-control polymer
  • Urea or another moisture-management component
  • Alcalin
  • Sels
  • Other nonvolatile auxiliaries

This is different from:

Commercial Thickener Product Solids.

A liquid pretreatment thickener may itself contain water, while a powder product may be mostly dry material.

Therefore, always distinguish:

  • Product dosage
  • Method-defined dry residue contributed by the product, distinct from any documented active-polymer content
  • Total pretreatment-liquor solids
  • Actual dry chemical add-on on fabric

Bath Solids vs. Dry Chemical Add-On

Pretreatment bath solids alone do not tell the mill how much chemistry reaches the textile.

A simplified relationship is:

Estimated dry add-on (%) ≈ net wet pick-up (%) × bath nonvolatile mass fraction. State the fabric reference basis and the bath-solids method. This retained-liquor estimate assumes a uniform bath and does not establish the amount of each active ingredient.

For controlled comparison, the exact calculation basis should be defined by the mill.

Two fabrics running through the same bath can receive different dry add-on if their wet pick-up differs.

Likewise, two pretreatment baths can deliver similar dry add-on if one has higher solids but lower pick-up and the other has lower solids but higher pick-up.

This is why pretreatment solids and fabric pick-up should be evaluated together.

Why Pretreatment Solids Matter

Conventional reactive inkjet pretreatment commonly uses polymer, alkali and moisture-management chemistry on the fabric before printing.

The polymer helps control droplet spreading and penetration. The alkali supports reactive dye fixation during steaming. Moisture-management components help maintain the water environment needed for dye dissolution and diffusion.

Changing total solids therefore changes several process functions at once unless the formula is carefully redesigned.

A useful test must distinguish:

Total Solids Effect

Source :

Individual Ingredient Effect.

What Happens When Pretreatment Solids Are Too Low?

When dry chemical add-on falls below the useful window, possible symptoms include:

  • More lateral ink spreading
  • More face-to-back penetration
  • Lower surface color yield
  • Weaker edge definition
  • Insufficient fixation chemistry
  • Uneven shade if pretreatment becomes less uniform

The exact symptom depends on which part of the formula was reduced.

Too little migration-control polymer can increase spreading; too little alkali can reduce fixation; and too little moisture-management chemistry can change steaming behavior.

Therefore, “low solids” should not be diagnosed without knowing which component changed.

What Happens When Pretreatment Solids Are Too High?

Excess dry add-on can create a different set of problems.

Possible effects include:

  • Heavy surface film build
  • Longer drying demand
  • More difficult wash-off
  • More residual salts or polymer if washing is insufficient
  • Potential hand deterioration
  • Higher chemical cost

Very strong surface localization can also alter ink penetration, droplet coalescence and surface concentration and does not guarantee a proportional increase in color yield.

The useful pretreatment window often shows diminishing returns beyond a certain chemical add-on.

How Pretreatment Solids Affect Color Yield

Pretreatment can increase apparent color yield by keeping more reactive ink near the visible fabric surface and by supplying the chemistry needed for fixation.

Published reactive inkjet studies show that changing pretreatment-agent concentration can materially change K/S and fixation.

However, the relationship is not universally linear.

Color yield can reach a plateau or fall if ink penetration becomes poor or nonuniform, excess chemistry changes wetting, alkali becomes excessive, or drying and steaming are no longer matched to the add-on.

The correct target is not the maximum pretreatment-solids concentration.

It is the lowest stable add-on that reaches the required post-wash color and fixation.

How Pretreatment Solids Affect Bleeding and Edge Definition

Polymer pretreatment can form a surface-controlling layer that limits uncontrolled droplet spreading.

If polymer add-on is too low:

  • Droplets can move laterally through fiber / yarn pathways.
  • Fine lines can widen.
  • Color-to-color boundaries can become less clear.

Increasing pretreatment polymer can improve boundary control up to a useful range.

But excessive polymer film can create different surface wetting, slower liquid absorption and more residue to remove.

Evaluate bleeding together with color yield and wash-off.

Surface Localization vs. Excess Penetration

Reactive ink must contact cellulose and fix during steaming, but excessive depth is not always useful for visual color.

Too much penetration can reduce surface color concentration and make the face appear weaker even when total ink usage is unchanged.

Pretreatment solids can help control droplet residence near the surface, lateral spreading and through-thickness movement.

For every solids level, compare:

  • Face-side K/S or approved shade
  • Reverse-side show-through
  • Définition des traits fins

Do not optimize color without observing penetration.

How Pretreatment Solids Affect Fabric Hand

Fabric hand requires careful interpretation in reactive digital printing because pretreatment is followed by steaming and washing.

Many conventional water-soluble pretreatment components are intended to be removed during wash-off.

Therefore:

High Pretreatment Solids ≠ Automatically Permanent Hard Hand.

The final hand depends on:

  • Polymer chemistry
  • Pretreatment add-on
  • Dye fixation
  • Wash-off efficiency
  • Residual polymer / salts / unfixed dye
  • Fabric structure

Some pretreatment polymers wash out more readily than others.

Polymer coatings that remain more strongly on the textile can contribute to harder post-wash hand.

Therefore, judge hand only after the complete production wash-off and conditioning step.

Wash-Off Efficiency and Residual Solids

Reactive printing wash-off removes hydrolyzed or unfixed dye, residual alkali, urea or other water-soluble components, and water-soluble pretreatment residue.

If pretreatment add-on is increased, wash-off demand can also increase.

Insufficient washing can leave:

  • Harsh hand
  • Residual surface polymer
  • Sels
  • Color contamination in white areas

When comparing solids levels, use one standardized washing sequence first.

If a high-solids sample only becomes acceptable after much more intensive washing, include that water, energy and time in the commercial decision.

Why Polymer Chemistry Matters as Much as Solids

Two pretreatment polymers at the same dry add-on can behave differently.

Important differences include:

  • Hydratation
  • Formation d'un film
  • Ink-drop confinement
  • Reactive-dye compatibility
  • Washability

Sodium alginate is widely used in reactive printing because of its dye compatibility and good wash-out behavior.

Other cellulose derivatives and synthetic polymers can also improve inkjet definition, but their post-wash behavior must be verified.

Therefore:

Same Solids Add-On ≠ Same Printing Result or Hand.

Thickener / Migration-Control Polymer

The thickener component is usually the most direct solids variable affecting ink migration.

Changing thickener dosage can change bath rheology, fabric surface film, droplet spreading, penetration and wash-off load.

Research on reactive cotton inkjet pretreatment has shown that thickener concentration can have an optimum range rather than a simple “more is better” relationship.

For practical development, build a dosage ladder around the current commercial level.

Keep alkali, urea, pick-up, drying and steaming constant in the first test.

Urea and Moisture-Management Solids

Urea can represent a large part of the dry chemical load in conventional reactive pretreatment.

Its function is different from thickener.

It primarily supports moisture and dye-solubility conditions during fixation.

Changing urea level can alter total solids, drying demand, moisture behavior during steaming and wash-off load.

Modern urea-reduced and urea-free approaches also exist, showing that the required moisture-management route is process-specific.

Therefore, do not reduce total solids by cutting urea unless fixation and color are revalidated.

Alkali Add-On and Fixation Chemistry

Alkali is required for reactive dye fixation, but excessive alkali is not an advantage.

Pretreatment-solids optimization should keep track of:

  • Alkali concentration
  • Wet pick-up
  • Actual alkali add-on
  • Final fabric / pretreatment pH where controlled

If the whole pretreatment formula is diluted to reduce solids, alkali add-on can also fall.

The resulting lower K/S may then be caused by fixation loss rather than poor migration control.

Separate thickener solids from fixation chemistry during troubleshooting.

Salts and Other Nonvolatile Auxiliaries

Some pretreatment systems also contain salts, anti-reducing agents, cationic components or other auxiliaries.

These materials contribute to total dry add-on even if they do not contribute to bath viscosity.

They can affect conductivity or ionic environment, polymer behavior, drying and wash-off.

Do not use bath viscosity as a proxy for total solids.

A low-viscosity pretreatment can still contain a high level of dissolved solids.

Wet Pick-Up Multiplies the Effect of Bath Solids

Pick-up is the bridge between pretreatment concentration and fabric chemical load.

Pour un contrôle gravimétrique simple :

Absorption d'eau (%) = (poids du tissu humide − poids du tissu sec) ÷ poids du tissu sec × 100

If bath solids remain constant:

Higher Pick-Up → Higher Chemical Add-On

and vice versa.

This is why solids optimization cannot be separated from padding pressure, nip condition, fabric absorbency and application route.

For broader process logic, see Textile Printing Thickener Testing Parameters.

Drying Load and Solids Migration

Higher pretreatment add-on usually means more water and/or more dissolved or dispersed material must be managed during drying.

Drying can change the final pretreatment distribution through water migration, surface concentration, polymer film formation and salt redistribution.

As solids and pick-up change, the current dryer setting may no longer produce the same residual moisture, surface chemistry or fabric dimensional condition.

Therefore, after a solids change is selected, drying should be revalidated.

Residual Moisture Before Printing

Pretreatment solids and residual moisture are related but different variables.

A fabric can have high solids / low residual moisture, high solids / high residual moisture, low solids / low residual moisture, or low solids / high residual moisture.

These conditions can give different ink spreading and fixation behavior.

Do not use “dry to touch” as the only production control.

Where residual moisture is important, measure or standardize it separately.

Fabric Structure and Absorbency

The same pretreatment solids can behave differently on lightweight knit, dense woven, mercerized cotton, viscose or lyocell because fabric structure changes wet pick-up, penetration, surface area and drying.

A high-solids formula that gives excellent surface localization on one fabric may create excessive surface film on another.

Approve solids by fabric family and construction where necessary.

Cotton vs. Viscose vs. Lyocell

Cotton, viscose and lyocell all support reactive dye chemistry but differ in swelling and liquid transport.

Therefore, the same bath solids can create different actual results because pick-up, penetration, drying and residual moisture differ.

Do not define one universal “cellulosic pretreatment solids” specification.

Use one controlled liquor first, measure actual add-on, and then create substrate-specific working windows.

Light vs. Dark Reactive Ink Loads

A pretreatment solids level that works for light shades may not be the best stress condition.

Dark or high-ink-load areas challenge droplet coalescence, bleeding control, surface localization, fixation chemistry and wash-off.

For qualification, include fine lines / small text, medium-tone blocks and high-ink-load dark areas.

This reveals whether the pretreatment window remains stable across the real design range.

Steaming and Fixation

Pretreatment solids should never be optimized independently from steaming.

During steaming, reactive dye fixation depends on available alkali, moisture, heat, time and dye / cellulose accessibility.

If solids are reduced by cutting alkali or moisture-management chemistry, the print can lose fixation even if bleeding improves.

If solids are increased substantially, the established steaming condition may also need review.

Keep steaming fixed during the first solids trial, then optimize only if needed.

Do Not Change Solids, Pick-Up and Drying at the Same Time

One common development mistake is to change pretreatment concentration, padding pressure and drying temperature in one trial.

If the result improves, the mill cannot identify why.

Use a staged method:

Stage 1: Solids Concentration

Stage 2: Pick-Up

Stage 3: Drying / Residual Moisture

Stage 4: Steaming

This produces a much more reliable production specification.

Reconcile a Solids Result with the Formulation Ledger

Record the final bath mass and the commercial mass of each ingredient added. Where the supplier provides a relevant nonvolatile or polymer-content value, retain its basis and test method. Keep unknown composition explicit; a total-solids result cannot resolve an undisclosed formulation.

Result or recordUseful interpretationDo not infer
Commercial-product doseMass of the supplied product per final bath mass.The same mass of active polymer in a powder, solution and compound product.
Bath residue under a stated methodMaterial remaining after that preparation, drying and weighing procedure.Pure thickener content, or all original solids if the method causes component loss or reaction.
Component ledgerKnown polymer, alkali, moisture-management and other contributions kept distinct.That equal total residue gives equal ionic balance, fixation conditions or ink control.
Treated-fabric dry-mass incrementAn application check using comparable specimen basis and a suitable blank.Distribution through the fabric, the amount of each active component or final washability.

When testing a polymer change, keep the remaining final-bath composition defined and balance water deliberately. If a commercial candidate carries other unknown ingredients, label it a complete-product comparison rather than an isolated polymer experiment. Verify that the residue method is suitable for the ingredients, including materials that may volatilise, decompose or react during heating; do not invent one universal oven condition for every formulation.

Build a Pretreatment-Solids Ladder

Prepare several controlled pretreatment levels around the current production condition.

A useful test design can include lower solids, current reference, moderately higher solids and a high stress point where technically justified.

Keep fabric, pick-up, drying, ink, steaming and washing constant first.

For every sample, record:

  • Bath solids
  • Wet pick-up
  • Calculated dry add-on
  • K/S or shade
  • Bleeding / boundary clarity
  • Pénétration
  • Post-wash hand

Do not assume the highest-solids point is the best.

Build a Solids × Pick-Up Matrix

Pretreatment ConditionLower Pick-UpReference Pick-UpHigher Pick-Up
Lower solidsTestTestOptional
Reference solidsTestReferenceTest
Higher solidsOptionalTestStress point

This matrix reveals whether a problem comes from bath concentration, fabric pick-up or total dry add-on rather than treating all three as one variable.

Calculate Dry Chemical Add-On

For process comparison, define one internal calculation method.

A simplified estimate is:

Estimated dry add-on (% on the stated fabric basis) ≈ net wet-pick-up fraction × bath nonvolatile mass fraction × 100. Do not multiply two percentage numbers as though both were fractions. Check the estimate against a suitable treated-fabric/blank method where needed.

Example calculations should use the mill’s actual concentration basis and measured pick-up.

Do not mix % w/w of bath, g/L and % on weight of fabric without conversion.

Dry add-on is often the most useful bridge between laboratory formula and production fabric.

Build a Color / Bleeding / Hand Response Map

Dry Add-OnRendement en couleurBleeding / DefinitionPénétrationPost-Wash Hand
LowRecordRecordRecordRecord
ReferenceRecordRecordRecordRecord
HigherRecordRecordRecordRecord

The optimum is where all required outputs pass.

It may not be the condition with the absolute highest K/S.

A small K/S gain can be commercially unattractive if it requires much more pretreatment, longer drying, more wash-off or worse hand.

  1. Define the current pretreatment formula and concentration basis.
  2. Measure or calculate total pretreatment solids.
  3. Use one fabric lot and one controlled application method.
  4. Build a pretreatment-solids ladder.
  5. Measure wet pick-up for every sample.
  6. Calculate dry chemical add-on.
  7. Dry under identical conditions first.
  8. Print fine details, medium tones and a high-ink-load area.
  9. Steam under one controlled condition.
  10. Wash / soap identically.
  11. Compare K/S, bleeding, penetration, fixation where available and post-wash hand.
  12. Then optimize pick-up, drying or steaming only where the response map shows a need.

For grade matching, review Digital Textile Printing Pretreatment et Échantillons et correspondances.

Production Trial Approval

After the laboratory working window is identified, run the best condition on the actual pretreatment line.

Record:

  • Fabric composition / construction
  • Pretreatment product / batch
  • Total bath solids
  • Bath pH
  • Wet pick-up
  • Calculated / measured dry add-on
  • Drying temperature / speed
  • Residual moisture if monitored
  • Ink / print mode
  • Conditions de cuisson à la vapeur
  • Conditions de lavage
  • Color / K/S
  • Bleeding / edge definition
  • Pénétration
  • Post-wash hand

Approve a solids / add-on working window, not one isolated bath concentration.

Common Pretreatment-Solids Mistakes

1. Calling Thickener Dosage “Total Solids”

Alkali, urea, salts and other auxiliaries can contribute significant dry add-on.

2. Comparing Bath Concentration Without Measuring Pick-Up

The same bath can deliver different chemical loading to different fabrics or padder settings.

3. Assuming More Solids Always Give Higher Color Yield

Color can plateau or fall if wetting, penetration, drying or fixation becomes unbalanced.

4. Assuming High Solids Always Cause Permanent Hard Hand

Final hand depends strongly on polymer chemistry and wash-off efficiency.

5. Reducing Total Solids by Cutting Alkali

Lower fixation can be mistaken for a migration-control problem.

6. Reducing Urea Without Rechecking Steaming

Moisture-management demand must be validated rather than assumed.

7. Changing Solids and Pick-Up Together

The true cause of the result becomes difficult to identify.

8. Judging Hand Before Washing

Reactive pretreatment should be assessed after the complete wash-off and conditioning route.

Troubleshooting Table

Problème constatéFirst Variables to CheckDo Not Assume
Low color and heavy bleedingPolymer add-on, pick-up, drying, ink loadMore alkali is the first fix
Color improves but hand worsensTotal dry add-on, polymer chemistry, wash-offAll extra solids remain permanently
High solids give no further K/S gainFixation, penetration, saturation / plateauMore pretreatment will continue improving color
Same bath gives different results by fabricWet pick-up, absorbency, GSM, constructionThe bath formula defines actual add-on
Lower-solids trial loses fixationAlkali / moisture-management add-onThickener reduction alone caused the loss
Post-wash fabric feels harshPolymer washability, wash-off, residual salts / dyeHigh pre-print viscosity is the cause
Edges are sharp but surface feels heavily coatedPolymer add-on, pick-up, solids concentrationMaximum localization is always best
Lab result works but production bleedsPick-up drift, bath solids drift, drying / moistureThe pretreatment grade changed

Coût total d'utilisation

Pretreatment-solids optimization should include more than chemical price.

A useful model is:

Cost per accepted m² = total non-overlapping in-scope run cost ÷ accepted finished-fabric area. Convert actual chemical, ink, energy, labour, post-treatment and additional disposal expenses into one currency. Pick-up and add-on determine consumption; they are not separate monetary cost lines. Include resources used in rejected fabric and rework without counting their underlying materials twice.

A lower-solids pretreatment can be economically better if it maintains color, controls bleeding, reduces drying load and reduces wash-off demand.

But it can become more expensive if color yield falls, ink consumption must rise, bleeding increases or fixation falls.

Compare cost per acceptable printed meter rather than pretreatment cost per kilogram.

What Information Should You Send to a Supplier?

For useful pretreatment-solids matching, provide:

  • Reactive ink / dye system
  • Composition et fabrication du tissu
  • Current pretreatment product / TDS
  • Thickener or migration-control dosage
  • Alkali type / dosage
  • Urea or moisture-management component
  • Other salts / auxiliaries
  • Total pretreatment concentration basis
  • Wet pick-up
  • Conditions de séchage
  • Residual moisture if available
  • Conditions de cuisson à la vapeur
  • Washing route
  • Main issue: color, bleeding, penetration, wash-off or hand

FSX Chemical can use this information through Échantillons et correspondances to define a controlled solids / add-on comparison.

Critique Digital Textile Printing Pretreatment, Textile Printing Applications et Épaississants pour l'impression textile, classés par procédé for broader route selection.

How Should a Mill Set Pretreatment Solids for Reactive Digital Printing?

A practical control chain is:

Define Total Bath Solids → Measure Wet Pick-Up → Calculate Dry Add-On → Print / Steam / Wash → Compare Color / Bleeding / Penetration / Hand → Adjust One Variable at a Time → Lock Solids + Pick-Up Working Window

Les principes fondamentaux sont les suivants :

  1. Pretreatment solids means more than thickener dosage; all nonvolatile or dry-forming pretreatment components should be considered.
  2. Bath concentration does not define fabric chemical load unless wet pick-up is also controlled.
  3. Low solids can reduce surface control or fixation chemistry, while excessive solids can increase drying, wash-off and residual-hand risk.
  4. Color yield can improve with pretreatment add-on but does not increase indefinitely; penetration, wetting, alkali and steaming must remain balanced.
  5. Final hand should be judged after reactive wash-off because polymer chemistry and residue removal determine what remains on the fabric.
  6. The best pretreatment is the lowest dry-add-on window that delivers the required color yield, bleeding control, fixation and post-wash hand at the lowest practical Total Cost in Use.

Foire aux questions

1. What does pretreatment solids content mean in reactive digital printing?

It refers to the dry or nonvolatile components in the pretreatment liquor, such as migration-control polymer, alkali, urea or other moisture-management chemicals, salts and other auxiliaries.

2. Is pretreatment solids the same as thickener solids?

No. Thickener is only one contributor. Total pretreatment solids can include several nonvolatile ingredients.

3. Why does higher pretreatment solids sometimes increase color yield?

More polymer can localize ink near the surface and more fixation chemistry may be carried by the fabric, but the response is not universally linear.

4. Can too much pretreatment solids reduce color performance?

Yes. Excessive surface film, wetting changes, unbalanced alkali, drying or steaming can create diminishing returns or poorer print behavior.

5. How does pretreatment solids affect bleeding?

Insufficient migration-control polymer can allow more lateral spreading. Increasing polymer add-on can improve edge definition until other surface or wash-off effects become limiting.

6. Does high pretreatment solids always make the fabric hard?

No. Reactive printing is followed by washing, so final hand depends on polymer washability, residual salts, unfixed dye and wash-off efficiency—not solids alone.

7. Why should wet pick-up be measured?

Because the same pretreatment bath delivers different chemical add-on when the fabric retains different amounts of liquor.

8. What is dry chemical add-on?

It is a method-defined dry-mass increment or a retained-liquor estimate on a stated fabric basis. It is not automatically the amount of active polymer. Record the bath composition, pick-up basis, drying method and any assumptions or losses.

9. Should I reduce urea to lower pretreatment solids?

Only after validating moisture management, color yield and fixation under the actual steaming conditions. Urea serves a different function from thickener.

10. Should I optimize solids before pick-up?

For clean diagnosis, first build a controlled solids ladder at one pick-up, then optimize pick-up around the best chemical condition.

11. Why can the same solids level behave differently on cotton and viscose?

Fabric absorbency, swelling, pick-up and penetration differ, so the actual distribution of pretreatment and ink is not identical.

12. What should I send FSX Chemical for pretreatment-solids matching?

Send the fabric, ink, pretreatment formula or TDS, thickener, alkali, urea/auxiliaries, concentration basis, wet pick-up, drying, steaming, washing and the specific color, bleeding or hand problem.

Optimize Pretreatment Solids by Dry Add-On, Not Bath Concentration Alone

If your reactive digital prints show weak color, bleeding, excessive penetration, high drying demand or post-wash hand changes after a pretreatment adjustment, FSX Chemical can help structure a controlled solids / pick-up comparison.

For a useful technical review, send:

  • Your reactive ink / dye system
  • Composition et fabrication du tissu
  • Current pretreatment product / TDS
  • Thickener or migration-control dosage
  • Alkali and moisture-management system
  • Total pretreatment concentration basis
  • Wet pick-up
  • Drying / residual-moisture data
  • Conditions de cuisson à la vapeur
  • Washing route
  • Current color, bleeding, penetration or hand target

Commencez par Échantillons et correspondances for a controlled current-vs-candidate evaluation.

Critique Digital Textile Printing Pretreatment for the current FSX reactive inkjet pretreatment route.

You can also Demander un devis directement auprès du fabricant after the suitable pretreatment grade and dry-add-on window are confirmed or Contacter FSX Chemical for technical discussion📧 E-mail: Service@fsxchemical.com

The most useful pretreatment-solids specification is not one bath concentration. It is a controlled dry chemical add-on window that combines solids concentration with fabric pick-up and is validated after drying, printing, steaming and washing for color yield, bleeding, fixation and post-wash fabric hand.

Contact rapide

Envoyez-nous votre demande

ou

Échantillons gratuits · Réponse sous 24 heures

Renseignements sur les produits et assistance

Envoyez-nous vos spécifications produit

Veuillez nous communiquer le nom du produit, son application, la quantité, la destination, ainsi que toute fiche technique (TDS), photo ou document dont vous disposez déjà. FSX Chemical examinera ces informations et vous recommandera la marche à suivre pour obtenir un devis, trouver un échantillon correspondant ou choisir un produit.

Informations sur le produit Nom du produit, référence, modèle, photo de l'étiquette ou référence du fournisseur.
Documents disponibles Fiche technique (TDS), fiche de données de sécurité (SDS), certificat d'analyse (COA), photo d'exemple, liste des produits ou données d'essai.
Détails de la commande Quantité estimée, conditionnement, pays de destination, port ou conditions commerciales.
Demande ou problème Procédé d'impression textile, besoins en matière de formulation, problème actuel ou performances visées.