How to Match the Right CMC Grade for Your Textile Projects

Matching the right CMC grade requires more than selecting a viscosity number. This guide explains...

Matching the right CMC grade requires more than selecting a viscosity number. This guide explains how textile buyers can compare application route, degree of substitution, purity, particle size, hydration, rheology, chemical tolerance and sample performance before approving a commercial grade.

Carboxymethyl Cellulose, commonly abbreviated as CMC, is available in many commercial grades. Two products may both be sold as textile-grade CMC while differing in viscosity, degree of substitution, purity, particle size, hydration behavior and chemical tolerance.

These differences matter because textile projects do not all require the same performance. A CMC used to adjust a reactive printing paste may need a different balance from a grade used for warp sizing, textile coating or a compound thickener formulation.

Selecting the highest viscosity or the highest degree of substitution is therefore not a reliable matching method. The correct grade is the one that meets the required function under the buyer’s actual preparation, formulation, equipment and post-treatment conditions.

This guide explains how to move from a general CMC inquiry to a controlled grade-selection process, including specification review, sample testing, production validation and first-batch verification.

Why CMC Grade Matching Matters

CMC is not a single standardized product. It is a family of modified cellulose materials that can be manufactured with different molecular, substitution, purity and particle characteristics.

A grade that develops high viscosity in clean water may lose structure after salts or alkalis are added. Another grade may provide lower initial viscosity but better stability in the complete textile formulation.

Incorrect matching can affect preparation

An unsuitable particle profile or hydration rate may create lumps, undissolved material, excessive mixing time or unstable viscosity.

Incorrect matching can affect production

The CMC may create poor screen passage, unsuitable paste flow, unstable coating pickup, excessive yarn-film buildup or repeated recipe correction.

Incorrect matching can affect the final textile

Depending on the application, the result may include weak print definition, undesirable fabric handle, insufficient yarn protection, difficult removal or nonuniform coating.

Correct matching reduces commercial risk

Connecting the approved sample with a permanent grade, specification and batch document helps the buyer move more safely from laboratory testing to routine commercial supply.

What Defines a CMC Grade?

A commercial CMC grade is defined by more than the chemical name “carboxymethyl cellulose.” Buyers should review several connected parameters.

Степень замещения

Degree of substitution, commonly abbreviated as DS, describes the average level of carboxymethyl substitution on the cellulose structure. It can influence solubility, ionic behavior, chemical compatibility and application performance.

Класс вязкости

CMC is available in low-, medium- and high-viscosity ranges. The result is meaningful only when the concentration, preparation, temperature, instrument and rotational conditions are known.

Purity

Purity and residual salts can affect solution appearance, electrolyte loading and formulation response. The required purity depends on the application rather than on a universal maximum target.

Particle profile

Particle size can influence powder wetting, dusting, hydration rate, lump formation and filtration.

Влажность

Moisture affects powder handling and the amount of dry material delivered at a given as-supplied dose. Record the reported method and basis; a dry-material fraction alone does not establish the CMC polymer fraction, which needs an appropriate content assay.

pH

The pH of a defined CMC solution provides useful quality information, but the complete textile formulation may operate under different pH conditions.

Application behavior

Hydration, flow, stability, film properties and chemical tolerance are not fully described by one TDS number. Representative application testing remains essential.

Overview of FSX Chemical CMC Grade Routes

FSX Chemical organizes its textile CMC selection into three internal product directions. These routes help buyers narrow the starting grade before completing sample tests.

FSX routeWhat the code identifiesWhat still needs comparison
CMC-HDБолее высокая степень замещенияDefined viscosity method and complete application performance
CMC-MDMiddle DS-selection routeHydration, formulation response and required textile result
CMC-LDБолее низкая степень замещенияActual grade compatibility, film or rheology function and removal
Current-grade matchingComparison with an identified reference productSample identity, matched test conditions and production suitability

CMC-HD, CMC-MD and CMC-LD identify FSX DS-selection routes, not high-, medium- and low-viscosity rankings or a performance league table. Verify the current TDS for the exact quoted grade. A higher DS does not automatically mean higher viscosity or a better finished textile.

Buyers can review the current grade routes on the FSX Chemical CMC product page .

1. Define the Textile Project

Grade selection should begin with the textile process rather than with a target price or a general request for high-viscosity CMC.

Textile printing

Identify the dye or pigment system, fabric, printing method, complete formulation, target paste behavior, fixation process and final print requirements.

Warp sizing

Identify the fibre, yarn count, twist, hairiness, loom type, weaving speed, required size pickup and desizing process.

Textile coating

Identify the coating method, target viscosity, pickup, active components, drying or curing conditions, adhesion and required fabric handle.

Compound thickener formulation

Define whether CMC will provide primary viscosity, flow adjustment, stability, water retention, film modification or support for another polymer.

Supplier replacement

State whether the objective is lower cost, stronger consistency, clearer specification, improved solubility or correction of a particular production problem.

2. Identify the Required Function

One CMC grade can perform several functions, but the selection priority should be clear.

Primary thickener

When CMC provides most of the formulation viscosity, chemical tolerance, flow and stability become critical.

Secondary rheology modifier

In a compound system, a smaller amount of CMC may be used to adjust paste body, flow, water retention or structural recovery.

Film-forming sizing component

In warp sizing, the grade must be evaluated for yarn adhesion, film strength, flexibility, abrasion behavior and desizing.

Coating formulation component

In coatings, CMC may support viscosity, suspension, water retention or film development. Compatibility with binders and active materials must be checked.

Cost-adjustment component

CMC should not be added to reduce formulation cost unless the modified formula still meets all preparation, production and final textile requirements.

3. Confirm the Viscosity Test Method

Viscosity is often the first specification buyers compare, but an isolated number is not sufficient to match a grade.

A complete viscosity method should include

  • CMC concentration and calculation basis
  • Water source and quality
  • Powder-addition procedure
  • Mixer type, speed and preparation time
  • Время для питья или отдыха
  • Температура измерения
  • Viscometer model or measurement principle
  • Шпиндель, ротор или геометрия
  • Rotational speed or shear condition
  • Unit and reading procedure

Do not compare unlike methods

A viscosity measured at one concentration cannot be compared directly with a result measured at another concentration. Temperature and rotational speed can also change the reported value.

Use one method for reference and candidate

First define the comparison. A common factory SOP tests whether each grade works within the existing water, equipment, mixing and hydration schedule. Report a candidate that is not ready by that deadline as an operational limitation under that SOP. Separately, qualify application performance after each grade has been prepared by its documented procedure to an agreed endpoint, then condition to the same measurement temperature and use comparable measurement settings. Record preparation differences. Nouryon’s CMC preparation guidance explains why grade and mixing conditions matter; it is background, not an FSX grade instruction.

Keep the method after approval

Retain the agreed incoming-QC method for comparison with the approved reference and first commercial lot. Keep that release test distinct from the documented preparation and application trial used to qualify the grade.

4. Evaluate Degree of Substitution

DS is an important CMC selection parameter, but it should not be treated as a simple quality ranking.

Use DS as a Selection Parameter, Not a Performance Guarantee

A higher-DS grade is a candidate when that structural parameter is relevant to the formulation. Verify the full grade in the required chemistry; differences in polymer characteristics, substitution distribution and residual salts prevent DS alone from proving compatibility.

Medium DS may provide a balanced route

A medium-DS grade can be a practical starting point when the buyer needs a balance of viscosity, solubility, application performance and commercial cost.

Lower DS may suit selected adjustment functions

A lower-DS route may be considered in selected compound formulations, flow-adjustment projects or applications where its specific interaction provides a benefit.

Average DS does not describe everything

Two products with similar average DS can differ in substitution distribution, purity, polymer characteristics and textile performance.

Compare the Whole CMC Grade, Not a DS Label

Use this proposed sequence to locate where the candidate differs from the reference. Define whether samples follow the common-SOP challenge or grade-appropriate application preparation. Use independent preparations, a declared concentration basis and the same final measurement temperature; record preparation history and readiness criteria. A plateau in one viscosity reading alone does not prove complete dissolution, so also inspect undissolved material and defined filtration behavior. Match or adjust the recipe only as a separately documented comparison.

Test pointKeep controlledЧто необходимо фиксировать
Hydrated CMC stockPowder concentration, dispersion, hydration and measurement settingsUndissolved material, viscosity development and filtration result
After the relevant chemical additionIdentity, dose, addition order and elapsed timeImmediate change and the result after the chosen holding interval
Complete working formulationFinal total mass, water balance and representative processing conditionsMulti-speed flow, handling, transfer or film behavior as relevant
Finished textileFabric or yarn, deposited amount and post-treatmentPrint quality or yarn protection, removal and required final properties

If grades differ at one addition stage, investigate the complete grade–chemical interaction. That observation does not establish DS as the sole cause. Approve the actual commercial grade and process, not the HD, MD or LD label in isolation.

Reactive printing requires special caution

In reactive systems, remaining hydroxyl groups and the structure of the CMC may influence dye interaction, wash-off and fabric handle. These properties require actual printing tests.

5. Review Purity and Residual Salts

Purity can affect solution appearance, ionic load and formulation behavior. However, the highest available purity is not automatically required for every textile project.

Printing formulations

Residual salts may influence viscosity and the response of the complete dye or pigment paste. Use representative chemical concentrations during testing.

Sizing formulations

Purity and residual material may influence film consistency, bath stability and later removal.

Coating formulations

Sensitive binders, dispersions or active ingredients may require closer control of ionic content.

Request an application-relevant specification

Buyers should ask which purity-related parameters are controlled for the proposed grade and which values can be reported on the batch COA.

6. Check Particle Size and Solubility

Particle profile affects how CMC enters the water and develops a uniform solution.

Fine particles

Fine material may hydrate rapidly, but rapid surface hydration can create lumps when the powder is added too quickly.

Coarser particles

Coarser material may wet differently and require a longer hydration period. It may be easier to disperse under some mixing conditions.

Powder addition matters

Establish stable liquid circulation before adding CMC. Introduce the powder gradually rather than dumping it into one point.

Check the complete vessel

Inspect the top, middle and bottom for dry material, gels, settling or nonuniform viscosity.

Filtration supports diagnosis

A defined filtration test can locate retained material and compare preparations. Record the filter, loading and conditions, then inspect the residue and use suitable follow-up checks before assigning it to incomplete hydration, gel, coarse material or contamination; filtration alone does not establish its identity.

7. Evaluate Water, pH and Electrolyte Conditions

A grade that performs well in laboratory water may behave differently in the factory’s process water and complete formulation.

Жесткость воды

Dissolved minerals can affect polymer behavior and interactions with other formulation components.

Conductivity and salts

Electrolytes may reduce or otherwise change the apparent viscosity of an anionic polymer system.

pH conditions

Textile printing, coating and sizing formulations may operate under different pH ranges. Test the grade under the actual process condition.

Порядок сложения

Adding a large amount of salt or alkali before adequate CMC hydration may produce a different result from adding it after the polymer phase has been prepared.

Record immediate and delayed changes

Measure the formulation after preparation and after the normal holding period. Some compatibility problems develop gradually.

8. Compare Rheology, Not Only Viscosity

CMC solutions and textile pastes may change their flow behavior when exposed to mixing, pumping, screen pressure or coating shear.

Flow under shear

A printing or coating paste should move sufficiently through the selected equipment without creating excessive resistance.

Recovery after shear

After application, the formulation may need to recover enough structure to control spreading, penetration or coating levelness.

Multi-speed viscosity testing

Measuring at more than one rotational speed can compare rate-dependent flow under a defined instrument setup. It does not by itself measure recovery with time. Where recovery matters, specify the prior shear, interval, final measurement setting and observation times, then compare independent preparations. Do not treat mixer RPM as a universal shear rate or an instrument recovery result as a direct screen-transfer prediction.

Application testing remains necessary

Rheometer or multi-speed data can support grade selection, but machine and fabric trials are still required.

The target depends on the project

A CMC suitable for a high-viscosity sizing bath may not provide the same balance required for fine textile printing or a smooth coating.

9. Check Film and Removal Properties

Film behavior is especially important in warp sizing, coating and applications where CMC remains temporarily on the textile surface.

Yarn adhesion

A sizing grade should attach sufficiently to the yarn and help protect it during weaving.

Film flexibility

An excessively brittle film may crack, shed or fail to protect the yarn. An excessively soft or tacky film may also create production problems.

Abrasion resistance

Laboratory film tests should be supported by a representative weaving trial that checks yarn breaks, shedding and loom performance.

Desizing or wash-off

The CMC-containing film must be sufficiently removable under the mill’s normal downstream process.

Готовая тканевая ручка

Printing or coating formulations should be evaluated after the complete washing, drying or curing process to identify residual stiffness or surface buildup.

10. Evaluate Holding Stability and Filtration

Textile formulations may remain in tanks for several hours before or during production. The CMC grade should remain sufficiently stable for the required operating period.

Measure at defined time points

Check the material after preparation, after complete hydration and after the normal holding time.

Inspect physical stability

  • Изменение вязкости
  • Разделение
  • Settling
  • Surface skin formation
  • Foam retention
  • Gel development
  • Filterability after storage

Use closed comparison containers

Evaporation can increase concentration and create an artificial viscosity difference.

Test the stock solution and final formulation

A CMC solution may remain stable alone but change after dyes, salts, binders or other polymers are added.

CMC Selection Guide by Textile Project

Textile ProjectPractical CMC DirectionCritical Tests
Reactive printing-paste adjustmentHigher-DS or balanced route as the initial candidateDye interaction, viscosity stability, rheology, definition, wash-off and handle
Reactive compound thickenerHD, MD or a selected blend depending on the complete formulaBlend stability, electrolyte response, print quality and dosage
Selected disperse formulationBalanced or compatibility-adjustment CMC routePaste stability, screen passage, fixation and final textile result
Warp sizingGrade selected by viscosity, film behavior and desizingAdhesion, flexibility, abrasion, size pickup, weaving and removal
Textile coatingGrade matched to coating viscosity and binder systemFlow, suspension, pickup, adhesion, handle and curing stability
Formulation viscosity adjustmentMD or LD route depending on compatibility and flow targetAddition response, holding stability, rheology and total dosage
Current supplier replacementClosest HD, MD or LD candidate after TDS reviewSame-method comparison, complete application and first-batch check

This table identifies possible starting directions. It does not establish automatic suitability or a one-to-one replacement.

How to Choose Between FSX CMC-HD, CMC-MD and CMC-LD

Consider CMC-HD when

  • A higher-DS route is required for comparison
  • The formulation has demanding chemical-compatibility requirements
  • The project involves reactive printing or a specialized blend
  • The current high-performance CMC grade needs a backup source

Consider CMC-MD when

  • A balanced CMC route is required
  • The project is a routine printing-paste or viscosity-control trial
  • The buyer wants to compare performance and cost together
  • The current TDS indicates a medium-DS commercial direction

Consider CMC-LD when

  • The project requires compatibility or flow adjustment
  • CMC will be one part of a compound thickener system
  • A selected reactive or disperse formulation is being developed
  • The lower-DS route matches the existing supplier specification

Do not choose from the model name alone

The final candidate should be confirmed through the current TDS, target viscosity, DS, sample preparation and actual textile application.

How to Match an Existing Supplier Grade

Buyers replacing an existing CMC supplier should begin with the current product rather than requesting an unrelated standard sample.

Collect available product information

  • Current product and grade name
  • Актуальные TDS и SDS
  • Recent batch COA
  • Package-label photograph
  • Viscosity result and complete method
  • DS and purity information where available

Provide a representative sample

A physical powder or solution sample can help compare appearance, hydration, viscosity and filtration.

Describe the actual formulation

Product specifications should be connected with the fabric, colorant, additives, dosage and production process.

State the reason for replacement

Common objectives include price review, improved consistency, clearer DS information, better solubility or qualification of a backup supplier.

Approve a commercial route

The matched candidate should be linked to a permanent FSX grade code, specification and bulk-supply route.

Current product information can be submitted through Образцы и подбор продукции FSX Chemical .

Step 1: Define the reference

Use a representative sample of the current approved CMC grade.

Step 2: Confirm the test plan

Record the properties that will determine approval, including viscosity, hydration, chemical tolerance, application behavior and final textile quality.

Step 3: Standardize preparation

  • Define the water and concentration basis for both comparisons; record any grade-specific preparation requirements
  • Use the same concentration basis
  • Use identical containers and mixers for a common-SOP challenge; document any preparation changes for the application comparison
  • Control powder-addition time
  • Record mixing speed, geometry and duration for the stated comparison
  • Use the fixed hydration deadline for the common-SOP challenge; verify each grade’s documented readiness endpoint before its application trial
  • Condition samples to the same temperature

Step 4: Record powder and solution behavior

  • Powder wetting
  • Lump formation
  • Время гидратации
  • Пена
  • Solution clarity or uniformity
  • Top-to-bottom consistency

Step 5: Measure viscosity

Use the same instrument, spindle, speed, temperature and reading procedure. Include more than one speed where rheology is important.

Step 6: Test filtration

Use a defined filter method and inspect the retained material.

Step 7: Prepare the complete formulation

Add the actual dyes, salts, alkalis, binders, other polymers or auxiliaries in the normal production order.

Step 8: Check holding stability

Measure and inspect the formulation immediately and after the required holding period.

Step 9: Complete the textile application

Conduct a printing, sizing or coating test using representative material and processing conditions.

Step 10: Evaluate the finished textile

Complete fixation, curing, washing or desizing before making the final comparison.

How to Scale from Laboratory to Production

A production vessel does not reproduce the same mixing and circulation conditions as a small laboratory beaker.

Record the approved laboratory method

Keep concentration, water, addition time, mixer, hydration, temperature and measurement settings.

Use a limited production batch

A pilot or controlled first run can identify mixing, filtration, foam and application problems before full conversion.

Do not copy RPM directly

The same mixer speed does not create the same circulation in vessels of different size and geometry.

Check batch uniformity

Where appropriate, compare samples from different vessel positions before production use.

Monitor the full operating period

Record viscosity, temperature, application behavior and textile quality throughout the production trial.

Verify the first commercial shipment

Repeat the approved incoming test and conduct a controlled application check before routine release.

How to Review TDS, SDS and COA

Технический паспорт

The TDS should identify the product, grade route, intended application, relevant properties and recommended preparation method.

Паспорт безопасности

The SDS supports handling, storage, transport and workplace-safety review. It should apply to the actual supplied product.

Сертификат анализа

The COA reports selected results for a confirmed production batch. Buyers should clarify which parameters will be listed before ordering.

Typical data and acceptance ranges

A typical value on a TDS is not always the same as an order-specific acceptance limit. Confirm which properties form part of the commercial specification.

Идентификационные данные документа

The product name and grade on the sample, TDS, quotation, label and COA should remain consistent.

Available document categories can be reviewed on the FSX Chemical Certificates & Technical Documents page .

How to Compare Total Cost in Use

The lowest CMC price per kilogram does not automatically provide the lowest cost for the textile project.

Дозировка материала

Compare the actual optimized quantity required to meet the same technical target.

Стоимость подготовки

Include powder addition, mixing, hydration, heating, cooling, labor and filtration.

Production cost

Include machine speed, correction work, cleaning, interruptions and unused formulation.

Затраты, связанные с конечным качеством

Include rejected printing, weak sizing performance, coating defects, reprocessing and customer claims.

Removal cost

Where relevant, include washing, desizing and additional downstream processing.

Затраты на снабжение

Include packaging, freight, import charges, inventory and batch-quality verification.

Cost comparisons should only include candidates that meet the required production and final textile standards. Use the same currency, accounting boundary and accepted output unit. Convert time, energy and losses to monetary costs where included, and avoid counting consumed or rejected material twice. Report preparation differences and accepted yield beside the unit cost.

Troubleshooting Common CMC Matching Problems

Выявленная проблемаPossible CausesRecommended Checks
CMC forms persistent lumpsPowder added too quickly, poor circulation, rapid surface hydration or unsuitable particle profileReview addition rate, mixer pattern, water temperature and hydration procedure
Viscosity is below targetIncorrect concentration, incomplete hydration, method difference, high electrolyte load or excess waterCheck weighing, water, hydration, chemicals and measurement method
Viscosity is above targetExcess dosage, evaporation, temperature difference or unsuitable gradeReview concentration, container closure, temperature and grade direction
Viscosity drops after salt or alkali additionElectrolyte sensitivity, addition-order issue or grade mismatchTest each chemical addition separately and compare HD, MD or LD routes
Excessive filtration residueIncomplete hydration, gel particles, coarse material or contaminationInspect residue and repeat preparation using a controlled method
Print spreads or loses definitionUnsuitable rheology, slow recovery, excessive penetration or fabric absorbencyReview dosage, multi-speed behavior, fabric and printing conditions
Fabric feels stiff after printingDye interaction, excessive dosage, incomplete wash-off or unsuitable CMC structureReview DS route, complete formula, fixation and washing
Sizing film is brittleUnsuitable grade, excessive drying, weak flexibility or poor blend balanceTest film properties, moisture conditions and alternative grades
Coating is unevenIncorrect rheology, poor dispersion, foam or binder incompatibilityReview mixing, flow behavior, coating pickup and complete formula
Bulk batch differs from sampleGrade identity, test-method difference, storage, water or batch variationCompare product codes, COA, retained samples and complete methods

Information to Include in Your Inquiry

Product information

  • Current CMC product and grade
  • Current TDS, SDS or COA
  • Target viscosity and complete test method
  • DS, purity, pH or particle requirement where available
  • Representative powder or solution sample

Сведения о применении

  • Textile printing, warp sizing, coating or formulation adjustment
  • Ткань, волокнистый состав или состав пряжи
  • Dye, pigment, binder or other chemical system
  • Current dosage and preparation process
  • Качество воды
  • Equipment and production conditions
  • Normal holding time
  • Процесс закрепления, термофиксации, промывки или расшлихтовки
  • Main technical problem or performance target

Коммерческие сведения

  • Предполагаемое количество образцов и оптового материала
  • Ожидаемое годовое потребление при наличии данных
  • Предпочтительная упаковка
  • Страна и порт назначения
  • Предпочтительные условия поставки
  • Required technical and export documents

Common CMC Selection Mistakes

Choosing only by viscosity

Similar viscosity does not confirm similar DS, purity, chemical tolerance, rheology or textile performance.

Assuming higher DS is always better

Higher DS may be useful in selected applications, but it may not provide the best performance-to-cost balance for every project.

Comparing different test methods

Viscosity numbers obtained under different concentrations, temperatures or speeds should not be compared directly.

Testing only in clean water

The actual dyes, salts, alkalis, binders and other polymers may change the result.

Ignoring film properties

Warp sizing and coating applications require more than solution viscosity.

Assuming direct replacement

A candidate CMC grade should be treated as a trial route rather than an automatically approved one-to-one replacement.

Утверждение образца без указания названия

The sample should be connected to a repeatable commercial grade, specification and batch-control route.

Пропуск проверки первой партии

The first commercial shipment should be tested against the approved reference before routine use.

How FSX Chemical Supports CMC Grade Matching

FSX Chemical supplies CMC for textile printing paste, compound thickener adjustment, viscosity control and selected textile projects. Buyers can begin with an FSX grade route or submit an existing supplier product for comparison.

Current-grade review

FSX Chemical can review the current TDS, viscosity method, DS, application, sample condition and bulk-order requirements.

HD, MD or LD starting direction

The available information can be used to determine whether a higher-DS, balanced or compatibility-adjustment route is the most practical starting point.

Laboratory sample comparison

Candidate samples can be evaluated for hydration, viscosity, solution uniformity, filtration and complete formulation performance.

Поддержка технической документацией

Relevant TDS and SDS information can support product review. Batch-level COA information can be connected with the confirmed commercial grade and shipment.

Factory-direct commercial supply

After the grade route is approved, quantity, packaging, destination, private label, shipping marks and export documents can be reviewed.

A recommended FSX grade remains a candidate for controlled laboratory and production testing. Final suitability depends on the customer’s complete textile process.

FSX Chemical’s general production and quality approach is available on the странице «Производство и качество» 📧 Электронная почта: Service@fsxchemical.com

Быстрый контакт

Отправьте запрос

или

Бесплатные образцы · Ответ в течение 24 часов

Запросы о продукции и техническая поддержка

Отправьте свои требования к продукции

Сообщите название продукта, область применения, количество, пункт назначения, а также предоставьте техническое описание продукта (TDS), фотографию образца или имеющиеся у вас документы. Компания FSX Chemical рассмотрит эту информацию и порекомендует дальнейшие действия для подготовки коммерческого предложения, подбора образца или выбора продукта.

Информация о продукте Название продукта, марка, модель, фото этикетки или данные о продукте текущего поставщика.
Доступные документы TDS, SDS, COA, фотография образца, перечень продукции или данные испытаний.
Детали заказа Предполагаемый объем, упаковка, страна назначения, порт или условия торговли.
Область применения или проблема Процесс печати на текстиле, требования к составу, текущие проблемы или целевые показатели.