CMC and CMS in Textile Printing: Selection, Preparation and Process Control

Match CMC and an FSX CMS commercial grade to its declared textile printing route and...

Use CMC or an FSX CMS candidate only after matching the exact commercial grade to the process. Confirm product identity and powder, flake or liquid form, then control preparation, dose basis, compatibility and final textile performance. A water-viscosity match alone does not approve printing, sizing or coating use.

CMC denotes carboxymethyl cellulose. CMS can denote carboxymethyl starch in technical literature, while FSX CMS is a commercial synthetic printing-thickener family. The family name does not establish every grade’s full composition. Follow the exact product declaration and TDS before applying a chemical identity or structural specification.

If a product is declared as carboxymethyl starch, its starch backbone differs from CMC’s cellulose backbone. Do not extend that description to an unconfirmed FSX CMS compound or synthetic grade. For each candidate, compare the specifications that actually apply, its supplied form and behavior in the complete formulation.

Successful use therefore depends on more than selecting either “CMC” or “CMS” from a supplier catalogue. The commercial grade must be matched to the textile application, prepared using a controlled method and tested in the complete formulation before production approval.

The following best practices apply to textile printing, warp sizing and selected coating or finishing systems. Actual conditions should be adjusted according to the current product TDS, factory equipment and required final textile performance.

Understanding CMC and CMS

What is Carboxymethyl Cellulose?

Карбоксиметилцеллюлоза is a chemically modified cellulose derivative. Textile grades may be evaluated for viscosity control, printing-paste formulation, warp sizing, coating and selected finishing applications.

Commercial CMC grades may differ in degree of substitution, viscosity, purity, moisture, particle size and solution behavior. These differences can influence hydration, electrolyte response, film formation and compatibility with the complete textile formulation.

What Does CMS Identify?

Carboxymethyl starch is a modified starch. That general definition is useful when the supplier identifies that material. For an FSX CMS candidate, first establish the exact commercial grade and declared printing route; a range label or a broad chemical definition is not its full specification.

Review grade-specific parameters and instructions. Degree of substitution is relevant only when an applicable substituted polymer and parameter are declared. Powder moisture or hydration procedures should not be imposed automatically on a liquid or other supplied form. Printing approval does not extend to warp sizing without its own suitability review.

Why they cannot be treated as interchangeable

Two grades can respond differently to salts, alkali, dyes, binders, shear and drying even if their water-viscosity readings match. Product identity and an actual formulation comparison matter more than assumptions drawn from similar abbreviations.

Their dried films may also differ in adhesion, flexibility, strength, moisture response and removability. These properties are particularly important in warp sizing and surface coating.

Quick Comparison of CMC and CMS

Comparison areaCMCFSX CMS candidateBest practice
IdentityКарбоксиметилцеллюлозаCommercial range; confirm exact grade declarationDo not infer full composition from a range name.
Область примененияGrade-specific textile formulationDeclared reactive, disperse or specialty routeConfirm suitability in the actual process.
ВязкостьDefined preparation and measurementGrade-specific preparation and measurementRecord concentration basis and complete method.
Structural parameterDS can be relevantOnly parameters declared for that materialDo not impose a carboxymethyl-starch DS universally.
Supplied formConfirm powder grade and instructionsConfirm powder, flake or liquid formPreparation and dose basis follow the exact product.
Final performanceNeeds full formulation and textile trialNeeds its declared-route trialNo universal 1:1 replacement or cross-process approval.

The table provides general selection guidance. The current product TDS and application trial should determine the final decision.

1. Start with the Textile Application

The first best practice is to define exactly what the material must do. Asking for “textile-grade CMC” or “printing-grade CMS” is often too broad to identify the correct commercial grade.

For textile printing

Define the dye or pigment system, fabric, printing method, required paste viscosity, design detail, fixation process and washing conditions.

A thickener used in reactive printing may face different compatibility requirements from a product used in disperse or pigment printing.

For warp sizing

Define the fibre composition, yarn count, twist, hairiness, loom type, weaving speed, target size pickup and desizing process.

Sizing performance depends on adhesion, film flexibility, abrasion resistance and removability rather than solution viscosity alone.

For coating or finishing

Define the coating method, target pickup, active ingredients, drying or curing process, required handle and downstream compatibility.

Write a short application specification

Before requesting samples, record the main function, current product, current dosage, test method and problem to be solved. This gives the supplier a clearer basis for grade selection.

2. Select the Correct Commercial Grade

Use the exact commercial grade and current TDS. For CMC, relevant parameters can include DS and reference viscosity. For the FSX CMS range, apply only specifications declared for the candidate’s actual material and form. Buying by family name alone is not sufficient qualification.

Review the complete viscosity method

Confirm the concentration, preparation procedure, hydration time, temperature, instrument, spindle and rotational speed used for the reported viscosity.

Values measured under different conditions should not be treated as directly equivalent.

Review degree of substitution

For CMC, or another explicitly identified substituted polymer, review the supplier’s DS definition and method where relevant. For an unconfirmed CMS-range material, first resolve identity and applicable specifications. DS alone does not prove compatibility or finished-textile performance.

Review purity and residual salts

Purity can influence solution appearance, electrolyte load and formulation compatibility. Buyers should use an actual specification rather than an unsupported high-purity description.

Review particle size

Fine particles may hydrate quickly but require controlled addition to avoid lumps. Coarser particles may disperse differently and require more hydration time.

Use a permanent grade code

The tested sample, TDS, quotation, purchase order, package label and COA should refer to the same commercial grade.

3. Standardize Water Quality

Water is the main preparation medium for most CMC and CMS textile formulations. Differences in water hardness, conductivity, dissolved ions, temperature and pH can change dispersion and apparent viscosity.

Use the same water for comparisons

Prepare the reference and candidate using one water source. Comparing one product in deionized laboratory water and another in factory process water can produce a misleading result.

Record basic water information

  • Источник воды
  • Температура
  • pH
  • Hardness where relevant
  • Conductivity where relevant
  • Seasonal or treatment-related variation

Test the actual process water

Deionized water is useful for controlled laboratory comparison, but final production approval should include the water used at the textile factory.

Avoid uncontrolled water correction

Operators should not add extra water only to reach a familiar visual consistency without recording the amount. Uncontrolled dilution changes dosage and makes later troubleshooting difficult.

4. Control Powder Addition and Dispersion

The powder-addition practices below apply when the chosen grade is supplied as a powder and its instructions call for dispersion and hydration. Follow different instructions for a liquid or flake product. During powder preparation, inspect persistent lumps and confirm the actual mixing and addition conditions rather than assuming all CMS forms behave alike.

Create suitable liquid movement first

Start the mixer and establish a stable circulation pattern before adding the powder. The liquid should move sufficiently to distribute the powder without drawing excessive air into the batch.

Add the powder gradually

Introduce the material in a controlled stream rather than dumping the full quantity into one location. Avoid allowing powder to accumulate on the liquid surface or vessel wall.

Do not add too close to the mixer shaft

Addition directly beside the shaft may cause powder to circulate without dispersing or may create a concentrated mass around the impeller.

Control dust and workplace exposure

Follow the current SDS and factory handling procedure. Avoid unnecessary high-speed powder addition that increases airborne dust.

Record the addition time

Powder-addition duration can affect lump formation and final viscosity. It should be included in the preparation record.

5. Allow Sufficient Hydration

Visible dispersion does not always mean that the polymer is fully hydrated. Some grades continue developing viscosity after mixing stops.

Follow the current TDS first

Use the current grade instructions and confirm the required state before incorporation. Do not assume the same hydration or resting period for CMC and every CMS-range grade, or require a powder-hydration step for an as-supplied liquid product.

Measure at defined time points

Useful time points may include immediately after mixing, after the recommended hydration period and after the normal production holding period.

Keep containers covered

Evaporation can increase apparent viscosity and make the product appear to continue hydrating. Use covered containers during controlled comparisons.

Check the complete vessel

Inspect the top, middle and bottom of the batch for undispersed material, settling or nonuniform viscosity.

Do not shorten hydration only to increase production speed

Incomplete hydration may produce unstable results during later storage or printing. Preparation time should be optimized only after controlled testing.

6. Control the Order of Addition

CMC and CMS can behave differently depending on when salts, alkalis, dyes, binders or other auxiliaries are introduced.

Prepare the polymer phase under controlled conditions

Unless the product instructions specify another method, it is generally safer to establish adequate polymer dispersion and hydration before exposing the system to high electrolyte concentrations.

Add sensitive components consistently

Use a fixed addition sequence when testing whether a candidate fits the existing mill SOP. If a grade requires a different documented preparation or addition sequence, evaluate that as a separate application trial. Record the change rather than attributing the result solely to thickener identity.

Watch for immediate viscosity changes

Record whether each addition causes thinning, over-thickening, separation, gel particles or foam.

Do not correct every change immediately

Allow the formulation to reach its defined mixing or resting condition before making corrective additions. Repeated water or powder correction can hide the original incompatibility.

7. Evaluate pH and Electrolyte Tolerance

CMC and CMS are used in formulations that may contain salts, alkalis, acids, dyes and ionic auxiliaries. Their effect should be evaluated in the complete system.

Do not rely on clean-water viscosity

A product that produces high viscosity in water may thin after salts or alkali are added. Another grade may remain more stable despite having a lower initial water viscosity.

Test realistic chemical concentrations

Use the dye, salt, alkali, binder and auxiliary levels found in production. An unrealistically mild laboratory formula may not reveal the relevant compatibility problem.

Measure after the normal holding period

Some viscosity changes develop gradually. Record both immediate and delayed results.

Separate pH effects from temperature effects

Chemical addition can change both pH and temperature. Measure and record both before concluding that one factor caused the viscosity change.

8. Manage Mixing Shear and Temperature

Mixing is necessary for dispersion, but excessive or inconsistent mechanical treatment can make laboratory comparisons unreliable.

Use repeatable mixer conditions

Record mixer type, impeller, speed, batch volume, vessel dimensions and mixing duration.

Avoid unnecessary high-speed mixing after hydration

Once the material is uniformly prepared, continued high shear may increase temperature, introduce air or alter apparent viscosity.

Control measurement temperature

Viscosity normally changes with temperature. Samples should be conditioned to the agreed temperature before comparison.

Do not cool only one sample

When mixing causes temperature rise, condition both the reference and candidate in the same way.

Consider production-scale shear

Laboratory preparation may not reproduce the pumping, circulation or screen shear found in production. Include a machine-relevant trial before final approval.

9. Check Filtration and Residue

A smooth visual appearance does not prove that a CMC or CMS paste is free from gels, lumps or coarse residue.

Use a defined filter

Record filter material, opening size, sample quantity and filtration procedure. Use the same method for all candidates.

Inspect retained material

Determine whether the residue consists of dry powder, hydrated gel, foreign contamination or another formulation component.

Repeat after chemical addition

A stock solution may filter well but develop particles after salts, dyes or binders are added.

Match the test to the equipment

Screen printing, coating and digital pretreatment may require different filtration standards. A coarse laboratory test may not identify a problem relevant to finer equipment.

10. Control Paste Storage and Holding Time

Textile pastes may be stored before use, transferred between vessels or circulated during production. Their condition should remain acceptable throughout the normal operating period.

Define the required holding time

Test the paste for the period actually used by the factory rather than an arbitrary short laboratory interval.

Use clean, closed containers

Contamination and evaporation can change paste appearance and viscosity. Containers should be suitably clean and covered.

Record storage temperature

Seasonal and workshop temperatures can influence viscosity and microbial stability. Compare samples under the same conditions.

Check more than viscosity

  • Разделение
  • Settling
  • Surface skin formation
  • Foam retention
  • Odor or color change
  • Filterability
  • Application behavior after storage

Do not return contaminated paste to the main batch

Material exposed to the machine, screen or open production area can introduce contamination and should be handled according to the factory’s quality procedure.

Best Practices for Textile Printing

CMC and CMS may be evaluated as printing thickeners or components of compound systems, but printing approval should be based on the complete color paste and final fabric.

Use the actual dye or pigment system

Do not approve a printing grade from a polymer-and-water solution alone. Add the actual dyes, pigments, salts, alkalis, binders and auxiliaries.

Use representative fabrics

Fabric weight, construction, fibre composition and absorbency influence spreading and penetration.

Include fine lines, small text, sharp corners, closely spaced elements, solid areas and gradients where relevant.

Evaluate machine behavior

  • Screen passage or coating transfer
  • Paste pickup
  • Spreading and penetration
  • Foam and filtration
  • Consistency during the trial
  • Cleaning requirements

Evaluate after the required post-treatment

Review print definition, color response, levelness, residual paste, fabric handle and relevant fastness or durability after the route-specific fixation or curing and any required washing or desizing. Judge candidates at the same agreed finished-textile endpoint.

Use caution in reactive printing

CMC and CMS grades may interact differently with reactive dyes. When sodium alginate is the current reference, do not assume direct replacement without checking color response, wash-off and handle.

Buyers evaluating reactive printing can also compare the candidate with an appropriate Альгинат натрия reference.

Best Practices for Warp Sizing

Consider sizing only where the exact material’s declaration or a separate technical review supports that application. A commercial CMS printing route is not automatically a sizing approval. Evaluate yarn protection during weaving and removal downstream using the proposed size, actual yarn and controlled add-on.

Evaluate film properties

  • Adhesion to the yarn
  • Film strength
  • Flexibility
  • Brittleness
  • Moisture response
  • Abrasion behavior
  • Removability during desizing

Control size-bath viscosity

Viscosity influences penetration and surface coating of the yarn. A bath that is too thick may produce excessive surface size, while one that is too thin may not provide sufficient protection.

Measure size pickup

Compare yarn pickup under controlled machine settings. Different polymer grades may require different concentrations to reach a similar pickup.

Run a weaving trial

Evaluate yarn breakage, hairiness, abrasion, shedding, loom stops and fabric quality rather than relying only on laboratory film testing.

Confirm desizing

The size must be removed sufficiently for the subsequent dyeing, printing or finishing process. Test the actual desizing method used by the mill.

Best Practices for Coatings and Finishing

CMC and CMS may also be evaluated as rheology modifiers, binders or formulation components in selected textile coatings and finishing systems.

Match viscosity to the application method

Knife coating, padding, screen application, impregnation and spraying impose different flow requirements.

Test compatibility with active ingredients

Pigments, particles, microcapsules, softeners, crosslinkers and other finishing chemicals may change viscosity or destabilize the polymer system.

Evaluate the dried textile

Check coating uniformity, adhesion, flexibility, handle, cracking, blocking and downstream processing.

Do not assume the thickener provides the final function

In functional finishes, antimicrobial, conductive or protective performance normally depends on the complete active system. CMC or CMS may serve as part of the carrier or matrix.

Using CMC and CMS in Blended Formulations

Blending can help formulators balance viscosity, flow, film behavior, chemical tolerance and cost. However, polymer mixtures can also produce unexpected interaction.

Define the purpose of the blend

Decide whether the blend is intended to improve rheology, reduce dosage, modify film properties, improve preparation or adjust cost in use.

Begin with simple ratios

Start with a small number of controlled blend ratios. Changing several polymers and additives simultaneously makes the result difficult to interpret.

Evaluate blend order

Compare pre-blending powders with separately prepared polymer solutions where relevant. The order in which polymers are hydrated may affect the final structure.

Check for delayed instability

Measure the blend immediately and after the required holding time. Watch for thinning, over-thickening, separation or gel formation.

Approve the final blend as a complete formulation

Good performance from the individual CMC and CMS solutions does not prove that their mixture will perform well.

How to Optimize Dosage

Dosage should be optimized by performance and cost in use rather than by nominal viscosity alone.

Start with an equal-concentration comparison

For comparable product forms, an equal as-supplied concentration can provide an initial preparation comparison. A powder and a liquid compound at the same nominal percentage are not automatically equivalent polymer additions. Declare the dose basis and compare the complete application separately.

Adjust one variable at a time

After the initial comparison, adjust the candidate dose in recorded steps while keeping final total mass and non-thickener additions controlled. Account for water introduced with stock paste or liquid product. Treat any additional formulation adjustment as a separate documented trial.

Evaluate actual supplied-product basis

Record as-supplied product mass and the declared dose basis. Powder moisture and a liquid nonvolatile result describe different measurements; neither alone establishes active-polymer mass in a compound grade. Use an active-content correction only when that component and assay are documented.

Record Product Dose, Stock Paste and Final Paste Separately

A stock-paste percentage is not the same as a final-paste product percentage. The following hypothetical mass balance illustrates the distinction; it is not an FSX formulation or recommended dose.

Preparation or additionMass balanceMeaning
Prepare 100 kg stock2 kg as-supplied powder + 98 kg water2% w/w powder in stock
Add stock to a 100 kg final working paste60 kg of that stock1.2 kg powder plus 58.8 kg stock water carried into the final paste
Complete the final pasteOther weighed ingredients and balancing water together total 40 kg100 kg final mass; 1.2% w/w as-supplied powder

The 1.2% figure is not active-polymer content unless an applicable assay establishes that basis. Weigh water and other additions to the final batch total, record any loss or later dilution, and recalculate if stock concentration or stock fraction changes. For a liquid or compound product, use its declared supplied-product basis instead of substituting a powder calculation unchanged.

Do not stop at the viscosity target

Confirm filtration, printing or sizing behavior, final textile quality and storage stability at the optimized dosage.

Measure and Price Cost Drivers

  • Actual product consumption × delivered unit price
  • Время смешивания и гидратации
  • Heating or cooling
  • Фильтрация
  • Machine cleaning
  • Unused paste or size
  • Desizing or wash-off
  • Distinct rejection, rework or disposal charges, without repeating consumed material or operating costs

Convert recorded time and energy to monetary costs using stated rates. Compare the same production boundary and currency per accepted finished-fabric area; keep unpriced operating metrics separate and do not count the same loss twice.

Laboratory-to-Production Scale-Up

A laboratory beaker and a production tank do not create the same mixing, heat transfer and circulation conditions.

Record the laboratory method

Retain the concentration, water, addition time, mixer, speed, hydration, temperature and test settings used for sample approval.

Use an intermediate trial where practical

A pilot or limited production batch can reveal scale-related dispersion, foam, filtration and transfer problems before full conversion.

Do not scale mixer speed directly

Identical revolutions per minute do not produce identical mixing in vessels of different sizes. The technical team should consider impeller design, tank geometry and circulation.

Monitor several tank positions

Sample from appropriate points to check whether the production batch is uniform.

Confirm the normal production holding time

Production batches may remain in storage or circulation longer than laboratory samples. Include the real operating period in the trial.

Batch Quality and Incoming Inspection

Once a commercial CMC or CMS grade is approved, buyers should maintain a consistent incoming-quality procedure.

Check product and batch identity

Confirm the grade code, batch number, package condition, quantity and applicable COA.

Use the approved test method

Repeat the same viscosity and preparation method used during product approval.

Inspect the supplied form

For a powder or flake, check appearance, caking, foreign material and handling behavior as applicable. For a liquid or formulated product, check separation, settling, skin or gel particles and the grade-specific release tests. Use only the applicable moisture or nonvolatile method; follow the current SDS for handling observations.

Retain a reference sample

An approved reference and incoming-batch sample can support later comparison.

Complete application checks for critical batches

A laboratory viscosity result does not replace formulation testing where the application is particularly sensitive.

Buyers can review FSX Chemical’s general production and quality approach on the странице «Производство и качество» .

Troubleshooting Common CMC and CMS Problems

Выявленная проблемаPossible CausesRecommended Checks
Устойчивые узелкиPowder added too quickly, weak circulation, rapid surface hydration or unsuitable addition pointReview addition rate, mixer pattern, temperature and particle profile
Вязкость ниже заданного значенияIncorrect concentration, incomplete hydration, high electrolyte load, method difference or excess waterRecheck weighing, water, hydration time, formulation and test conditions
Вязкость превышает заданное значениеExcess dosage, evaporation, lower measurement temperature or incorrect concentration basisCheck batch calculation, container closure, temperature and dilution records
Viscosity drops after chemical additionSalt, alkali, acid, dye or polymer incompatibilityAdd components separately and measure after each controlled step
Excessive filter residueIncomplete dispersion, coarse particles, gel formation or contaminationInspect residue and repeat preparation with a controlled method
Printing spreads or bleedsUnsuitable rheology, excessive penetration, low structure recovery or high fabric absorbencyReview dosage, rheology, fabric and application conditions
Poor paste transferExcessive viscosity, unsuitable recovery, incomplete screen passage or poor levelingCompare multi-speed behavior and conduct a machine trial
Stiff fabric after processingExcess polymer, poor removal, binder interaction or excessive surface filmReview dosage, wash-off, desizing, drying and complete formulation
Brittle sizing filmUnsuitable grade, excessive drying, low flexibility or incorrect blendEvaluate film properties, auxiliaries and moisture conditions
Batch-to-batch differenceProduct variation, test-method variation, water change, storage or preparation differenceCompare batch numbers, COA, retained samples and complete methods

Avoid changing several formulation variables at once during troubleshooting. Begin by confirming product identity, preparation, water, temperature and measurement method.

Procurement Checklist

Product information to request

  • Постоянный код продукта и марки
  • Актуальный TDS
  • Актуальный SDS
  • Полный метод определения вязкости
  • Degree of substitution specification where relevant
  • Moisture, pH, purity and particle-size data where relevant
  • Рекомендуемый порядок приготовления
  • Recommended applications and known limitations
  • Representative sample
  • Proposed batch COA parameters

Application information to send the supplier

  • Printing, sizing, coating or finishing process
  • Ткань, волокнистый состав или состав пряжи
  • Dye, pigment, ink or auxiliary system
  • Текущий продукт и дозировка
  • Target viscosity and test method
  • Качество воды
  • Mixing and application equipment
  • Holding time and storage conditions
  • Основная производственная проблема
  • Final textile requirements

Коммерческие сведения

  • Предполагаемое количество образцов и оптового материала
  • Предпочтительная упаковка
  • Страна и порт назначения
  • Предпочтительные условия поставки
  • Required technical and export documents

CMC and CMS Best-Practice FAQ

Can CMC and CMS be replaced at the same dosage?

Not as a universal 1:1 replacement. Confirm both commercial grades, identity, supplied form and dose basis. Compare preparation and the complete formulation, optimize the candidate as a recorded trial, and approve only after the required final-textile and production results.

Which thickener is the safer starting point for reactive dye printing?

Sodium alginate is usually the lower-risk reference for reactive printing on cotton and viscose because of its established dye compatibility and wash-off behavior. Selected CMC, CMS or compound systems may be evaluated where cost, rheology or process conditions justify a trial, but performance must be checked with the actual dye, alkali, electrolyte, fabric and fixation route.

How should buyers compare CMC or CMS viscosity?

For repeat-order QC of an approved grade, reproduce its fixed preparation and measurement SOP. For different-grade selection, declare the concentration basis and prepare each product adequately by its documented procedure, then use matched measuring temperature, instrument, spindle, speed and reading protocol. Record preparation differences and assess any unchanged-mill-cycle constraint separately. Equal readings still do not establish equal flow, timed recovery, filtration or printing performance.

What information is needed for CMC or CMS grade matching?

Provide the textile application, fabric and colorant system, current product and dosage, viscosity test method, water quality, mixing procedure, equipment and the problem to be solved. FSX Chemical can use these details for a sample matching review before bulk qualification.

How FSX Chemical Supports Grade Matching

Review the FSX CMC grades or the FSX CMS printing-thickener routes, then use sample matching to provide the current product or TDS, textile process and required result. Confirm a sizing or coating application separately; the printing-range listing does not establish approval for those uses.

Buyers can provide

  • Current TDS or product specification
  • Репрезентативный образец порошка или пасты
  • Fabric, fibre or yarn information
  • Printing, sizing or coating process
  • Current dosage and preparation method
  • Viscosity value with the complete test conditions
  • Main technical or cost-in-use objective

Technical review may include

  • Identification of the appropriate CMC or CMS route
  • Review of the existing product specification
  • Recommendation of a candidate commercial grade
  • Provision of the relevant TDS and SDS
  • Representative samples for laboratory evaluation
  • Guidance for side-by-side preparation and testing
  • Review of laboratory or production-trial feedback
  • Batch documentation for the confirmed commercial grade

A recommended grade is a starting point for controlled evaluation, not a guaranteed direct replacement. Final approval depends on the buyer’s formulation, equipment and textile-quality requirements📧 Электронная почта: Service@fsxchemical.com

Быстрый контакт

Отправьте запрос

или

Бесплатные образцы · Ответ в течение 24 часов

Запросы о продукции и техническая поддержка

Отправьте свои требования к продукции

Сообщите название продукта, область применения, количество, пункт назначения, а также предоставьте техническое описание продукта (TDS), фотографию образца или имеющиеся у вас документы. Компания FSX Chemical рассмотрит эту информацию и порекомендует дальнейшие действия для подготовки коммерческого предложения, подбора образца или выбора продукта.

Информация о продукте Название продукта, марка, модель, фото этикетки или данные о продукте текущего поставщика.
Доступные документы TDS, SDS, COA, фотография образца, перечень продукции или данные испытаний.
Детали заказа Предполагаемый объем, упаковка, страна назначения, порт или условия торговли.
Область применения или проблема Процесс печати на текстиле, требования к составу, текущие проблемы или целевые показатели.