Define the exact grade before comparing pigment-printing thickeners. Distinguish acrylic, CMC and documented carboxymethyl-starch chemistry...

Define the product identity before comparing pigment-printing thickeners. The chemical-route comparison below distinguishes acrylic rheology modifiers, CMC and documented carboxymethyl-starch candidates. FSX CMS is a commercial synthetic printing-thickener family, so its trade name is not a third, mutually exclusive chemistry category and does not place a grade in the starch column. Confirm the exact grade and intended pigment-printing use, then compare complete-paste rheology, binder interaction, dose and cured-fabric results. Water viscosity or the family name alone cannot approve the candidate.

Which Thickener Route Is Best for Pigment Printing?

There is no universal winner.

For many conventional pigment-printing systems, synthetic acrylic or polyacrylate thickeners are a common starting route because they can deliver strong thickening efficiency at relatively low dosage and can be designed for useful shear-thinning and recovery behavior.

CMC and CMS can still be evaluated in selected pigment systems, especially when the mill is exploring:

  • Different rheological profiles
  • Higher water retention
  • Compound-thickener systems
  • Cost optimization
  • Specific binder / pigment combinations

The correct selection sequence is:

Complete Paste Compatibility → Rheology → Screen Transfer → Curing → Fastness → Post-Cure Residue / Washability → Fabric Hand → Total Cost in Use

Do not select by viscosity, raw-material name or price per kilogram alone.

Important Comparison Boundary: Pigment Printing Is Binder-Film Printing

Pigment printing differs fundamentally from reactive printing.

Pigment particles do not chemically react with the fiber in the same way reactive dyes do.

The binder forms a film that holds pigment on the textile surface after drying and curing.

Therefore, the thickener should be evaluated as a rheology-control component inside the binder system.

This changes how “wash-off” should be interpreted.

In conventional pigment printing:

  • Пленка-связующее вещество должна остаться на месте.
  • The process may not include the same intensive wash-off used after reactive printing.
  • Residual thickener, surface cleanliness and hand still matter.
  • If a post-cure wash is used, the thickener’s removability and interaction with the binder film should be checked.

Do not apply reactive-printing wash-off rules directly to pigment printing.

The Three Thickener Routes at a Glance

МаршрутTypical StrengthMain Risk to Check
Synthetic acrylic / polyacrylateHigh thickening efficiency, tunable rheology, low dosage potentialElectrolyte / pH / binder sensitivity
CMCPseudoplastic flow, water retention, broad availabilityHigher dosage, binder interaction, residue / hand
Confirmed carboxymethyl starch (CMS)Pseudoplastic flow, cost potential, compound-system flexibilityGrade variability, hydration, binder compatibility

These are route-level tendencies, not product guarantees.

Commercial grades can behave very differently inside each category.

Synthetic Acrylic / Polyacrylate Thickener

Synthetic acrylic thickeners are widely used in pigment-printing systems because the chemistry can be designed for:

  • Высокая эффективность загущения
  • Low addition level
  • Сильное сдвиговое разжижение
  • Controlled recovery
  • Easy liquid dosing

Many grades are pH-responsive and may require correct neutralization.

Their most important technical checks are:

  • Activation pH
  • Совместимость связующих веществ
  • Толерантность к электролитам
  • Стабильность при выдержке
  • Complete-paste rheology

A synthetic grade that gives very high water viscosity can still fail in the real pigment formula if binder or pigment salts collapse the polymer structure.

CMC for Selected Pigment-Printing Systems

CMC is an anionic cellulose derivative with well-known pseudoplastic behavior.

Its performance depends strongly on:

  • Степень замещения
  • Молекулярная масса
  • Purity
  • Концентрация
  • Salt / binder environment

CMC can be worth evaluating when the mill wants:

  • A polysaccharide-based rheology route
  • Strong water retention
  • A different low-shear / high-shear balance
  • A compound-thickener component

However, CMC should not be assumed to be a direct one-for-one substitute for a synthetic pigment-printing thickener.

It may require a different dosage and can create different:

  • Paste solids
  • Эластичность
  • Перенос изображения на экран
  • Post-cure residue
  • Тканевая ручка

Grade selection should be based on the complete binder-containing formula.

Confirmed Carboxymethyl Starch (CMS) for Pigment Systems

In the generic chemistry comparison, CMS means confirmed carboxymethyl starch, a starch derivative. Apply starch-backbone and substitution statements only to a candidate whose grade documentation establishes that identity. The FSX CMS commercial synthetic printing-thickener family is a separate naming context: obtain its current grade-specific TDS, composition information and application recommendation rather than importing starch or CMC specifications. Classify the identified material before choosing the relevant comparison column.

Selected CMS grades can be evaluated as:

  • Primary rheology-control components in specific pigment systems
  • Compound-thickener components
  • Cost-optimization routes

For a proposed carboxymethyl-starch versus CMC trial, record the exact grades and compare the same pigment, binder, complete-paste conditions, deposit and curing route. The results qualify those identified formulations; they do not establish the performance of an unrelated FSX commercial grade.

This is important because CMS should not be treated as “cheap CMC.”

Its:

  • Substitution
  • Starch structure
  • Молекулярная масса
  • Purity
  • Гидратация

can produce a distinctly different rheological profile.

Rheology Comparison: Shear Thinning, Recovery and Elasticity

All three routes can show pseudoplastic behavior, but the degree and recovery profile can differ.

Synthetic Acrylic

Often provides strong, designable shear thinning and can be formulated for rapid recovery.

CMC

Typically shows non-Newtonian pseudoplastic behavior, with flow strongly influenced by DS, molecular weight and concentration.

Confirmed Carboxymethyl-Starch Candidate

Also commonly shows pseudoplastic behavior, but the exact profile depends on starch source, substitution and modification route.

For screen printing, the key comparison is:

Low-Shear Body → High-Shear Flow → Recovery → Elasticity

not:

Which sample has the highest Brookfield number?

Why the Same Viscosity Does Not Mean the Same Printing Behavior

Two pastes can both measure 30,000 mPa·s under one viscometer condition and still differ in:

  • Flow through the screen
  • Squeegee pressure requirement
  • Проникновение
  • Восстановление конструкции
  • Stringiness
  • Прокачка

One-point viscosity should therefore be treated as a QC value, not a complete rheological description.

When possible, compare:

  • Multi-speed viscosity
  • Recovery after controlled shear
  • Machine screenability

Совместимость с связующими веществами

Binder compatibility is critical in pigment printing.

Binder can change:

  • pH
  • Electrolyte level
  • Баланс поверхностно-активных веществ
  • Общее содержание твердых веществ
  • Viscoelasticity

Синтетический загуститель

Can be highly efficient but may be sensitive to the specific binder chemistry or ionic load.

CMC

Can respond to binder salts and ionic conditions and should be checked for viscosity drift or flocculation.

Confirmed Carboxymethyl-Starch Candidate

Can also interact with binder / auxiliaries and should be evaluated for delayed thickening, thinning, separation or foam.

Use the same binder and pigment package for all three comparisons.

Electrolyte and pH Sensitivity

All three routes can respond to ionic conditions, but not in the same way.

Synthetic Polyacrylate

Often sensitive to charge screening, especially in conventional highly ionic systems, although hydrophobically modified grades can show improved tolerance.

CMC

Salt tolerance depends strongly on DS, molecular weight and substitution uniformity.

Confirmed Carboxymethyl-Starch Candidate

Salt / alkali response depends on substitution, starch backbone and grade design.

Therefore, compare:

Water Viscosity

and:

Complete Pigment-Paste Viscosity

for every route.

Dosage and Polymer Solids

Compare each candidate at the dose needed to reach the agreed complete-paste printing window. Record as-supplied dose in g/kg of final paste first; equal dose is not necessarily a useful performance comparison.

QuantityHow to report itWhat not to assume
As-supplied product doseWeighed commercial product per final paste mass, including formulation water corrections.Liquid and powder dosages contain equal functional polymer.
Measured nonvolatile contributionProduct dose × nonvolatile mass fraction from an agreed test; state time, temperature and sample handling.Dry residue is automatically active acrylic polymer, CMC or starch.
Functional polymer contributionCalculate only from confirmed grade composition or an applicable validated assay.Moisture correction alone establishes purity, or SDS identification supplies an active-content assay.
Retained printed-system depositCompare measured deposit and finished-fabric performance under matched printing and curing.Calculated bath solids alone predict residue, softness or fastness.

If active polymer content is undisclosed, mark it as unknown and compare documented as-supplied dose, measured nonvolatile contribution and finished performance. Nonvolatile testing, such as the applicable approach described in ASTM D2369, is a method-dependent residue measurement; confirm suitability for the particular product rather than imposing one drying method on every grade.

Hypothetical comparison: 10 g/kg of a liquid product with 30% measured nonvolatile content contributes 3 g/kg measured residue. This does not establish 3 g/kg active thickener. A powder containing moisture and salts requires its own composition evidence. Keep binder and pigment contributions separate when assessing fabric hand.

Screen Transfer and Print Definition

Good print definition requires:

  • Clean screen passage
  • Controlled paste deposit
  • Ограниченное боковое распространение
  • Appropriate structural recovery

Synthetic thickener can offer a strong balance where high-shear flow and rapid recovery are required.

CMC or CMS can also provide useful definition when the grade and dosage create the right pseudoplastic profile.

Do not compare print sharpness at unmatched viscosity or unmatched paste deposit.

Penetration and Surface Color

Thickener route changes how the pigment-binder paste moves into the textile.

Too much penetration can reduce:

  • Концентрация цвета поверхности
  • Чёткость краёв

Too little penetration can create:

  • Surface-heavy deposits
  • Uneven coverage in some constructions

Compare penetration on the same:

  • Ткань
  • Экран
  • Скребок
  • Уровень наполнения папки

Otherwise, process variation can be mistaken for thickener behavior.

Wash-Off, Residue and Post-Cure Cleanliness

Conventional pigment printing normally ends with drying and binder curing, without the reactive-dye process of removing unfixed dye and thickener after steaming. The useful endpoint is an intact, durable pigment–binder print with acceptable hand. Cotton Incorporated explains this process distinction.

A specified finishing wash and an end-use laundering test are separate operations. Record which is being evaluated, including detergent or bath chemistry, temperature, time, mechanical action and drying. If your approved production route has no post-cure wash, compare candidates in that route first.

Observed after washingVerify before interpreting it
Softer fabricDid surface friction or bending change while shade, rubbing and film integrity remain acceptable? Softness alone does not prove selective thickener removal.
Lower specimen mass or visible residue in the bathWere conditioning, fabric controls and test handling matched? The lost material may include additives, loose pigment or damaged binder; mass loss alone does not identify it.
Shade loss, staining or crackingCheck pigment retention, binder cure and film damage, rather than calling the outcome good wash-off.

Water solubility of an uncured CMC or confirmed carboxymethyl-starch solution does not establish removal from a cured pigment print. Polymer may remain associated with or trapped by the film. Selective removal claims require appropriate analytical evidence; until then report only the measured wash response.

Fabric Hand

Fabric hand is often where the thickener routes become commercially different.

Hand depends on:

  • Binder film
  • Thickener solids
  • Paste deposit
  • Отверждение
  • Состав ткани

A lower-dose synthetic thickener can reduce added polymer solids and may help support a softer hand if binder and curing are also optimized.

CMC or CMS may require higher solids depending on the grade, which can increase the risk of a heavier or stiffer surface.

But this is not universal.

A well-optimized CMC or CMS compound system can still produce acceptable hand, while an over-bindered synthetic-thickener system can become very stiff.

The final comparison must be made after curing.

Rubbing Fastness and Curing

Rubbing fastness is primarily controlled by the pigment binder and curing process.

The thickener contributes indirectly by affecting:

  • Pigment distribution
  • Распределение связующих веществ
  • Paste deposit
  • Проникновение

Higher binder concentration can improve rubbing fastness but may also increase stiffness.

Therefore, do not select a thickener route only because it produces a deeper wet print.

Сравните:

  • Сухое втирание
  • Влажное протирание
  • Wash fastness where relevant
  • Тканевая ручка

after identical curing.

Holding Stability

Compare fresh paste with held paste.

Запись:

  • Вязкость
  • pH
  • Температура
  • Пена
  • Разделение
  • Гель / флок

Synthetic

Watch for pH or electrolyte-related viscosity drift.

CMC

Watch for hydration completion, salt response and delayed viscosity change.

Confirmed Carboxymethyl-Starch Candidate

Watch for hydration, formulation interaction and storage stability.

A paste that is stable only when fresh is not suitable for a long production holding window.

Flat Screen vs. Rotary Screen

The thickener route should be evaluated on the intended machine.

Плоскошаблонная печать

Important factors include:

  • Low-shear hold
  • Pause / restart behavior
  • Recovery after squeegee stroke

Ротационный трафарет

Important factors include:

  • Pumpability
  • Continuous shear
  • Circulation stability
  • Mid-run and end-run viscosity

A route that works in flat screen may need dosage or grade adjustment in rotary screen.

Can Synthetic Thickener Be Blended with CMC or CMS?

Yes, compound-thickener systems can be evaluated.

The purpose of blending is not simply to reduce cost.

A blend can be designed to change:

  • Тело с низким сдвигом
  • Shear-thinning profile
  • Восстановление
  • Водоудерживающая способность
  • Реакция электролитов
  • Polymer solids

A published mixed-thickener study examined modified polyacrylic acid and CMS in reactive-dye printing on viscose, with dye-dependent results. It provides a reason to study mixture rheology, not proof that the same blend is compatible with a pigment binder or meets pigment-printing fastness requirements. Read the original study and its application scope.

However, there is no universal synthetic/CMC or synthetic/CMS ratio.

Compound systems must be tested for:

  • Совместимость
  • Стабильность при выдержке
  • Перенос изображения на экран
  • Отверждение
  • Рука

Practical Selection Matrix

Область выбораSynthetic AcrylicCMCConfirmed Carboxymethyl Starch
Typical thickening efficiencyOften highGrade-dependentGrade-dependent
Shear-thinning design flexibilityВысокаяModerate / grade-dependentModerate / grade-dependent
pH activation requirementCommon in some gradesNormally no acrylic-style activationNormally no acrylic-style activation
Electrolyte sensitivityCan be significantDepends on DS / gradeDepends on substitution / grade
Typical dosage levelOften lowerOften higherOften higher
Совместимость связующих веществMust verifyMust verifyMust verify
Post-cure residue / handOften benefits from low solids if optimizedDepends on dosage / binder trappingDepends on dosage / binder trapping
Compound-thickener potentialВысокаяPossiblePossible

This table is a route-selection aid, not a product specification.

How to Compare the Three Routes in the Laboratory

Use the same:

  • Пигмент
  • Связующее вещество
  • Ремонтник
  • Вспомогательные средства
  • Ткань
  • Отверждение

Then:

Step 1: Build Each Grade to a Useful Rheology Window

Do not force equal dosage.

Step 2: Measure Fresh Complete-Paste Viscosity

Use the same instrument and method.

Step 3: Run Multi-Speed / Recovery Comparison

Compare screen-relevant rheology.

Step 4: Hold the Paste

Check end-of-shift stability.

Step 5: Print the Same Fabric

Keep screen and squeegee conditions constant.

Step 6: Cure Identically

Затем сравните:

  • K/S / оттенок
  • Определение термина «печать»
  • Проникновение
  • Сухое / влажное протирание
  • Post-cure residue or wash response
  • Рука

For a controlled grade comparison, FSX Chemical can review current products or TDS through Образцы и подбор продукции.

Утверждение пробного производства

Only the best laboratory candidates should move to production.

Запись:

  • Thickener route and grade
  • Дозировка
  • Complete formula
  • Вязкость в начале, в середине и в конце пробега
  • Скорость работы станка
  • Поведение экрана
  • Beginning-to-end shade
  • Curing result
  • Стойкость окраски к трению
  • Тканевая ручка

Approve a route only if it remains stable across the intended production window.

When Does Synthetic Thickener Usually Make More Sense?

Synthetic acrylic thickener is often worth prioritizing when the mill needs:

  • Высокая эффективность загущения
  • Низкая доза
  • Tailored shear thinning
  • Fast liquid incorporation
  • Low added polymer solids

It is especially attractive when the binder / pigment system has already been optimized for synthetic rheology modifiers.

But electrolyte tolerance and pH activation must be checked.

When Can CMC Be Worth Evaluating?

CMC may be worth testing when the mill wants:

  • A polysaccharide rheology route
  • Strong water retention
  • A different screen-transfer profile
  • A compound formulation
  • An alternative supply route

Selection should focus on:

  • DS
  • Молекулярная масса
  • Purity
  • Совместимость связующих веществ
  • Required dosage

Do not assume one generic CMC grade represents all textile CMC products.

When Can CMS Be Worth Evaluating?

CMS may be worth evaluating when the mill wants:

  • Cost optimization
  • Compound-thickener flexibility
  • Pseudoplastic flow
  • Alternative rheology

Selection should focus on:

  • Substitution
  • Purity
  • Гидратация
  • Совместимость связующих веществ
  • Стабильность при выдержке

Selected CMS grades can be technically useful, but the result is formulation-specific.

Common Comparison Mistakes

1. Comparing Equal Dosage Only

Different grades have different thickening efficiency.

2. Comparing Water Viscosity Only

Pigment and binder can change the complete paste substantially.

3. Assuming Synthetic Always Gives Softer Hand

Binder solids, dosage and curing can dominate hand.

4. Assuming CMC / CMS Must Wash Out Completely

In pigment printing, binder film can retain or trap part of the hydrophilic thickener.

5. Treating CMS as Cheap CMC

The polymer backbone and rheology are different.

6. Using Reactive-Printing Wash-Off Logic

Pigment printing is binder-film printing and must be evaluated differently.

7. Selecting by Price per Kilogram

Working dosage and finished-fabric result determine real cost.

Таблица устранения неисправностей

Observed DifferenceПервые переменные, которые следует проверитьНе делайте поспешных выводов
Synthetic paste is thinner after binderpH, electrolytes, binder compatibilitySynthetic route is unsuitable
CMC needs higher dosageGrade, DS, molecular weight, target rheologyHigher dosage means worse overall cost
CMS gives different screen feelShear thinning, recovery, hydrationSame viscosity means same rheology
Synthetic gives softer handPolymer solids, binder film, paste depositAll synthetic grades will do the same
CMC/CMS leaves more residueDosage, curing, post-cure wash, binder trappingPolysaccharide route is automatically poor
Rubbing fastness differsBinder distribution, curing, paste depositThickener chemistry alone controls fastness
Lab result good, rotary run driftsContinuous shear, holding time, temperatureLab viscosity predicts long-run stability
Compound system outperforms single polymerBlend rheology and compatibilityOne polymer must always be best

Общая стоимость эксплуатации

Compare the three routes using:

Cost per Saleable Unit = Total Attributable Production Cost ÷ Accepted Printed Output

Choose one denominator before comparing trials: accepted printed area in m² or accepted fabric mass in kg. Use the same fabric, design, quality criteria and costing boundary. Linear meters are comparable only when fabric width is also matched.

Cost componentCalculate in currency for the same trial or production run
MaterialsSum actual consumed quantity × unit price for pigment, binder, thickener and other auxiliaries. For a recipe estimate, thickener g/kg paste ÷ 1,000 × paste kg × supplied-product price/kg gives thickener cost. Reconcile actual use with returned or reusable paste.
Preparation and machine timeRecorded preparation, printing, cleaning and occupied equipment hours × the applicable cost rate. Lower speed or downtime changes these costs; efficiency is not a currency amount that can be added directly.
Energy, water and curingRecorded consumption × unit tariff, including the relevant drying, curing and any approved washing route.
Additional rework or disposalInclude extra material, time, energy and documented disposal costs attributable to the failed output.
Accepted outputUse only printed area or fabric mass meeting the agreed color, fastness, definition and hand criteria as the denominator.

Dosage is an input to material cost, not an additional cost term. Avoid double counting: if an equipment rate already includes labor or energy, do not add them again. Material and processing spent on rejected output are already included in the run’s numerator and its lower accepted-output denominator; add only separate losses not yet counted. This is a proposed comparison worksheet, not an FSX measured cost-saving result.

A synthetic thickener can have a higher price per kilogram but lower working dosage.

CMC or CMS can have a lower raw-material cost but require more solids or different preparation.

A compound system may reduce cost only if it also maintains:

  • Стабильность пасты
  • Производительность экрана
  • Fastness
  • Рука

Compare cost per acceptable printed meter—not cost per kilogram of thickener.

Какую информацию следует предоставить поставщику загустителей?

For a useful synthetic-vs-CMC-vs-CMS comparison, provide:

  • Current thickener product / TDS
  • Текущая дозировка
  • Вязкость и полная методика испытаний
  • Пигментная дисперсия
  • Связующее вещество и дозировка
  • Фиксаторы / вспомогательные элементы
  • Конечный уровень pH пасты
  • Ткань
  • Плоское или ротационное сито
  • Сетка экрана / гравировка
  • Время удержания
  • Условия отверждения
  • Main target: rheology, hand, residue, fastness or cost

FSX Chemical can review the exact current product and TDS through Образцы и подбор продукции to identify a candidate and the relevant trial route. Establish the identity of any proposed FSX CMS grade before applying a generic starch comparison or selecting blend components.

Обзор CMC, the FSX CMS commercial printing-thickener family и Области применения загустителей в текстильной печати for route-specific product information. A commercial-family link does not confirm a carboxymethyl-starch composition.

How Should a Mill Compare Synthetic Thickener, CMC and CMS for Pigment Printing?

Практическая последовательность действий выглядит следующим образом:

Match Complete-Paste Rheology → Compare Dosage & Solids → Hold → Screen Print → Cure → Check Fastness → Check Residue / Wash Response → Check Hand → Calculate Total Cost in Use

Основные принципы заключаются в следующем:

  1. Synthetic thickener, CMC and CMS should not be compared at equal dosage alone.
  2. Same viscosity does not mean same shear thinning, recovery or print definition.
  3. Binder compatibility must be checked for all three routes.
  4. Wash-off in pigment printing means post-cure residue and cleanliness, not reactive-style removal of the printed film.
  5. Fabric hand depends on binder film, thickener solids, paste deposit and curing together.
  6. The best route is the one that delivers the required production window at the lowest Total Cost in Use.

Часто задаваемые вопросы

1. Is synthetic thickener better than CMC or CMS for pigment printing?

Not universally. Synthetic acrylic thickeners are a common starting route because of high efficiency and tailored rheology, while selected CMC, CMS or compound systems can be useful in specific formulations.

2. Why do synthetic thickeners often use lower dosage?

Many acrylic/polyacrylate products are designed for high thickening efficiency, but actual dosage still depends on solids, pH, electrolyte load and formula.

3. Can CMC be used in pigment printing?

Selected CMC grades can be evaluated, especially where a polysaccharide rheology route or compound system is desired. Binder compatibility and dosage must be verified.

4. Can CMS be used in pigment printing?

Selected, identified carboxymethyl-starch grades can be evaluated in pigment-printing systems, with results dependent on the binder, pigment, dose and process. For an FSX CMS commercial grade, request its intended-use information and run a separate complete-paste and cured-fabric trial; the acronym alone does not transfer a generic starch result.

5. Which route gives the best shear thinning?

It depends on the commercial grade. Synthetic acrylic systems often offer more rheology-design flexibility, but CMC and CMS are also pseudoplastic and can provide useful screen behavior.

6. Which route gives the softest fabric hand?

There is no universal answer. Lower polymer solids can help, but binder dosage, curing and paste deposit often dominate final hand.

7. Does CMC wash off better than synthetic thickener?

Not automatically in pigment printing. CMC is water-soluble before curing, but part of it can be retained in or under the cured binder film. Test the real post-cure process.

8. Does CMS leave more residue?

Residue depends on grade, dosage, hydration, binder film and post-treatment. Do not assume residue from polymer family alone.

9. Can synthetic thickener be blended with CMC or CMS?

Yes. Compound systems can be evaluated to tune rheology, solids, water retention or cost, but the blend must be tested for compatibility and curing performance.

10. Should the three routes be compared at the same viscosity?

Compare them inside the same useful complete-paste rheology window, then evaluate screen transfer, definition, curing, hand and cost.

11. Which route is cheapest?

Compare Total Cost in Use. A lower raw-material price can be offset by higher dosage, longer preparation, lower machine efficiency or poorer hand.

12. What should I send FSX Chemical for comparison testing?

Send your current thickener or TDS, dosage, viscosity method, pigment, binder, fabric, machine route, curing conditions and main target so the most relevant route can be selected for trial.

Compare Synthetic Thickener, CMC and CMS Under the Same Pigment Formula

If your mill is deciding between synthetic acrylic thickener, CMC, CMS or a compound-thickener route, FSX Chemical can help structure a controlled comparison based on complete-paste rheology and finished-fabric performance rather than water viscosity alone.

Чтобы получить полезный технический обзор, отправьте:

  • Your current thickener sample, TDS or COA
  • Текущая дозировка
  • Вязкость и полная методика испытаний
  • Пигментная дисперсия
  • Система связующего и закрепителя
  • Конечный уровень pH пасты
  • Fabric and screen route
  • Время удержания
  • Условия отверждения
  • Current rheology, wash/residue, hand or cost target

Начните с Образцы и подбор продукции для проведения контролируемого исследования по сравнению «текущий кандидат против другого кандидата».

Обзор CMC, the FSX CMS commercial printing-thickener family и Области применения загустителей в текстильной печати for route-specific selection. A commercial-family link does not confirm a carboxymethyl-starch composition.

Вы также можете Запросить предложение напрямую от производителя after the suitable thickener route and working dosage are confirmed or Связаться с компанией FSX Chemical для обсуждения технических вопросов📧 Электронная почта: Service@fsxchemical.com

The best pigment-printing thickener is not determined by polymer family alone. It is the route that gives the required rheology, binder compatibility, cured fastness, acceptable residue and hand, and the lowest practical Total Cost in Use.

Быстрые ссылки

Быстрый контакт

Отправьте запрос

или

Бесплатные образцы · Ответ в течение 24 часов

Запросы о продукции и техническая поддержка

Отправьте свои требования к продукции

Сообщите название продукта, область применения, количество, пункт назначения, а также предоставьте техническое описание продукта (TDS), фотографию образца или имеющиеся у вас документы. Компания FSX Chemical рассмотрит эту информацию и порекомендует дальнейшие действия для подготовки коммерческого предложения, подбора образца или выбора продукта.

Информация о продукте Название продукта, марка, модель, фото этикетки или данные о продукте текущего поставщика.
Доступные документы TDS, SDS, COA, фотография образца, перечень продукции или данные испытаний.
Детали заказа Предполагаемый объем, упаковка, страна назначения, порт или условия торговли.
Область применения или проблема Процесс печати на текстиле, требования к составу, текущие проблемы или целевые показатели.